Ultrasonic testing of CFRP monolith structures radius zones by radius phased array and special device

Boychuk A.S., Dikov I.A., Chertishchev V.Yu., Generalov A.S., Gorbovets M.A.
Boychuk A.S., Dikov I.A., Chertishchev V.Yu., Generalov A.S., Gorbovets M.A. Ultrasonic testing of CFRP monolith structures radius zones by radius phased array and special device // Proceedings of VIAM. 2023. No. 5. DOI: 10.18577/2307-6046-2023-0-5-111-123. URL: https://www.viam-works.ru/en/journal/2023/5/10
Keywords
fiber reinforced plastics (FRP), carbon fiber-reinforced plastics (CFRP), radius zone, non-destructive testing, ultrasonic pulse-echo method, phased array
Abstract

The paper is devoted to nondestructive testing of CFRP monolithic structures radius zones. Manual ultrasonic testing technique by radius phased array and special device is proposed by the authors. Technique allows non-destructive testing of such zones with different radii and bending angles of structures from the inside without testing object immersing in a water container. Technique makes it possible to detect flat defects in radius zones such as extraneous inclusions and voids with diameter from 3 mm and a signal-to-noise ratio of more than 10 dB.

Reference list
  1. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  2. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
  3. Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2022, no. 1 (66), paper no. 04. Available at: http://www.journal.viam.ru (accessed: December 05, 2022). DOI: 10.18577/2071-9140-2022-0-1-41-50.
  4. Sidorina A.I. Multiaxial carbon fabrics in the products of aviation technology (review). Aviation materials and technologies, 2021, no. 3 (64), paper no. 10. Available at: http://www.journal.viam.ru (accessed: December 01, 2022). DOI: 10.18577/2713-0193-2021-0-3-105-116.
  5. Slavin А.V., Silkin A.N., Grinevich D.V., Yakov-lev N.O. Composite materials with a 3D-reinforced structure (review). Trudy VIAM, 2022, no. 8 (114), paper no. 09. Available at: http://www.viam-works.ru (accessed: December 01, 2022). DOI: 10.18577/2307-6046-2022-0-8-113-122.
  6. Goncharov V.A., Timoshkov P.N., Usacheva M.N. Prospects of the production of large-sized aircraft parts from polymer composite materials (review). Trudy VIAM, 2021, no. 12 (106). paper no. 07. Available at: http://www.viam-works.ru (accessed: December 01, 2022). DOI: 10.18577/2307-6046-2018-0-8-55-62.
  7. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 1. Automated Tape Laying (ATL). Aviation materials and technologies, 2021, no. 2 (63), paper no. 06. Available at: http://www.journal.viam.ru (accessed: December 02, 2022). DOI: 10.18577/2713-0193-2021-0-2-51-61.
  8. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 2. Automated Fiber Placement (AFP). Aviation materials and technologies, 2021, no. 3 (64), paper no. 11. Available at: http://www.journal.viam.ru (accessed: December 02, 2022). DOI: 10.18577/2713-0193-2021-0-3-117-127.
  9. Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes. II. Development of methods for studying the early stages of aging. Deformatsiya i razrushenie materialov, 2020, no. 1, pp. 15–21.
  10. Barinov D.Ya. About selection of optimal thickness of the carbon sample for thermal conductivity measurements using laser flash method. Aviation materials and technologies, 2022, no. 2 (67), paper no. 12. Available at: http://www.journal.viam.ru (accessed: December 05, 2022). DOI: 10.18577/2713-0193-2022-0-2-131-140.
  11. Gulyaev A.I., Medvedev P.N., Sbitneva S.V., Petrov A.A. Experimental research of «fiber–matrix» adhesion strength in carbon fiber epoxy/polysulphone composite. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 80–86. DOI: 10.18577/2071-9140-2019-0-4-80-86.
  12. Veligodskiy I.M., Koval T.V., Kurnosov A.O., Marakhovskiy P.S. Study of resistance of glass fiber reinforced plastic to natural weathering in different climatic conditions. Trudy VIAM, 2022, no. 11 (117), paper no. 12. Available at: http://www.viam-works.ru (accessed: December 06, 2022). DOI: 10.18577/2307-6046-2022-0-11-134-148.
  13. Boychuk A.S., Dikov I.A., Generalov A.S., Slavin A.V. FRP structures radius zones ultrasonic testing (review). Trudy VIAM, 2021, no. 8 (102), paper no. 11. Available at: http://www.viam-works.ru (accessed: December 06, 2022). DOI: 10.18577/2307-6046-2021-0-8-92-103.
  14. Introduction to Phased Array Ultrasonic Technology Applications: R/D Tech Guideline. Quebec: R/D Tech inc., 2004, 368 p.
  15. Boychuk A.S., Generalov A.S., Dalin M.A., Dikov I.A. Inspection of monolithic parts and structures of aviation equipment made from PCM by ultrasonic non-destructive testing using phased arrays. Proceedings of the X All-Rus. conf. "The main trends, directions and prospects for the development of non-destructive testing methods in the aerospace industry" (TestMat). Moscow: VIAM, 2018, pp. 18–31. Available at: https://conf.viam.ru/sites/default/files/uploads/proceedings/1063.pdf (accessed: December 06, 2022).
  16. Hopkins D., Neau G., Le Ber L. Advanced phased-array technologies for ultrasonic inspection of complex composite parts. Smart Materials, Structures & NDT in Aerospace. Montreal; Quebec, 2011. Available at: https://www.ndt.net/article/ndtcanada2011/papers/109_Hopkins.pdf (accessed: December 07, 2022).
  17. Lamarre A. Ultrasonic phased-array for aircraft maintenance. Amsterdam, 2009. Available at: https://ndt.aero/images/docs/UTPAfor%20maintenance.pdf (accessed: December 07, 2022).
  18. Brotherhood C.J., Drinkwater B.W., Freemantle R.J. An ultrasonic wheel-array sensor and its application to aerospace structures. Insight, 2003, vol. 45, no. 11, pp. 729–734. Available at: http://https://www.researchgate.net/publication/239411267_An_ultrasonic_wheel-array_sensor_and_its_application_to_aerospace_structures (accessed: December 07, 2022).
  19. Nageswaran C., Bird C.R. Phased array scanning of artificial and impact damage in carbon fibre reinforced plastic (CFRP). Insight, 2006, vol. 48, no. 3, pp. 155–159. Available at: https://www.ndt.net/article/insight/papers/insi_48_3_155.pdf (accessed: December 07, 2022).
  20. Boychuk A.S. Development of technologies for non-destructive testing of monolithic structures made of carbon fiber using ultrasonic antenna arrays: thesis, Cand. Sc. (Tech.). Moscow, 2016, 203 p.
  21. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  22. Boychuk A.S., Dikov I.A., Generalov A.S. Features of ultrasonic structures made of carbon fiber with a convex surface using phased arrays and Waterbox mandrels. Kontrol. Diagnostika, 2019, no. 3, pp. 14–21.
  23. Rau E., Grauvogl E., Manzke H., Cyr P. Ultrasonic Phased Array Testing of Complex Aircraft Structures. Available at: https://www.ndt.net/article/ecndt2006/doc/Tu.1.1.2.pdf (accessed: December 07, 2022).
  24. Moles M. Portable Phased Array Applications. 3rd MENDT – Middle East Nondestructive Testing Conference & Exhibition. Bahrain, Manama, 2005. Available at: https://www.ndt.net/article/mendt2005/pdf/20.pdf (accessed: December 08, 2022).
  25. Kass D., Nelligan T., Henjes E. The Evolution and Benefits of Phased Array Technology for the Every Day Inspector. 9th European Conference on NDT. Berlin, 2006, pp. 1–6. Available at: https://www.ndt.net/article/ecndt2006/doc/P198.pdf (accessed: December 08, 2022).