Conservation oils protective ability

Kravchenko N.G., Shchekin V.K., Efimova E.A., Zherdev D.V.
Kravchenko N.G., Shchekin V.K., Efimova E.A., Zherdev D.V. Conservation oils protective ability // Proceedings of VIAM. 2023. No. 4. DOI: 10.18577/2307-6046-2023-0-4-90-98. URL: https://www.viam-works.ru/en/journal/2023/4/9
Keywords
temporary anticorrosive protection, preservation oil, full-scale climatic tests, protective ability, oil-soluble corrosion inhibitor
Abstract

Comparative experiments were carried out to determine the protective properties of promising conservation oils in comparison with standard K-17 oil. The most effective conservation oils that can be used in the development of recommendations for the protection of aircraft parts and the revision of current regulatory documentation have been determined. Based on the analysis of the oil-soluble corrosion inhibitors contained in the tested oils and the mechanism of their action, an assumption was made to explain the effectiveness of a particular oil.

Reference list
  1. Krymskaya R.S., Trusov V.I., Altsybeeva A.I. Corrosion inhibitor N-M-1. Korroziya: materialy, zashchita, 2011, no. 9, pp. 32–35.
  2. Shekhter Yu.N., Shkolnikov V.M., Bogdanova T.I., Milovanov V.D. Working-preservation lubricants. Moscow: Khimiya, 1979, 256 p.
  3. Shekhter Yu.N., Krein S.E., Teterina L.N. Oil-soluble surfactants. Moscow: Khimiya, 1978, 304 p.
  4. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Report of XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
  5. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  6. Vetrova E.Yu., Shchekin V.K., Kurs M.G. Comparative evaluation of methods for the determination of corrosion aggressivity of the atmosphere. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 74–81. DOI: 10.18577/2071-9140-2019-0-1-74-81.
  7. Kurs M.G., Nikolayev E.V., Abramov D.V. Full-scale and accelerated tests of metallic and nonmetallic materials: key factors and specialized stands. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 66–73. DOI: 10.18577/2071-9140-2019-0-1-66-73.
  8. Abramova M.G. Full-scale accelerated tests of aluminum alloys at continental and marine type stations. Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 57–65. DOI: 10.18577/2071-9140-2020-0-3-57-65.
  9. Abramova M.G., Lutsenko A.N., Varchenko E.A. Concerning the aspects of validation of climate resistance of airborne materials at all life cycle stages (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 86–94. DOI: 10.18577/2071-9140-2020-0-1-86-94.
  10. Startsev V.O., Slavin A.V., Nikolaev E.V. Study of the content of aggressive ions in the at-mosphere and sea water of the Gelendzhik bay. Trudy VIAM, 2020, no. 10 (92), paper no. 12. Available at: http://www.viam-works.ru (accessed: November 07, 2022). DOI: 10.18577/2307-6046-2020-0-10-106-115.
  11. Kablov E.N., Startsev O.V., Medvedev I.M., Panin S.V. Corrosive aggressiveness of the coastal atmosphere. Part 1. Factors of influence (review). Corrosion: materials, protection. 2013, no. 12, рр. 6–18.
  12. Shkolnikov V.M. Fuel. Lubricants. Technical liquids. Range and application. Moscow: Tekhinform, 1999, 596 p.
  13. Conservation oil "Rosoil-700": pat. 2232794С1 Rus. Federation; filed 26.12.02; publ. 20.07.04.
  14. Washing-preservation liquid concentrate: pat. 2024605 Rus. Federation; filed 14.04.92; publ. 15.12.94.
  15. Washing-preservation liquid concentrate: pat. 2218385 Rus. Federation; filed 29.08.02; publ. 10.12.03.
  16. Washing-preservation liquid concentrate: pat. 2215777 Rus. Federation; filed 22.04.02; publ. 10.11.03.
  17. Gaidar S.M., Nizamov R.K., Golubev M.I., Golubev I.G. Protective efficiency of water-soluble corrosion inhibitors. Vestnik Mordovskogo universiteta, 2018, vol. 28, no. 3, pp. 429–444.
  18. Gaidar S.M., Petrovsky D.I., Posunko I.A. Boric derivatives of amines as water-soluble corrosion inhibitors. Korroziya: materialy, zashchita, 2017, no. 12, pp. 27–35.
  19. Levashova V.I., Yangirova I.V., Kazakova E.V. Review of corrosion inhibitors based on organoboron compounds. Sovremennye problemy nauki i obrazovaniya, 2014, no. 6, pp. 10–17.
  20. Kuznetsov Yu.I. Progress in the science of corrosion inhibitors. Korroziya: materialy, zashchita, 2015, no. 3, pp. 12–23.
  21. Kuznetsov Yu.I. Triazoles are a class of multifunctional corrosion inhibitors. Review. Part I-1. 1, 2, 3-benzotriazole, its derivatives, copper, zinc and their alloys. Korroziya: materialy, zashchita, 2019, no. 1, pp. 1–14.