Properties and features of protective coatings based on polyvinylidene fluoride and its copolymers (review)

Losev A.V.
Losev A.V. Properties and features of protective coatings based on polyvinylidene fluoride and its copolymers (review) // Proceedings of VIAM. 2023. No. 4. DOI: 10.18577/2307-6046-2023-0-4-81-89. URL: https://www.viam-works.ru/en/journal/2023/4/8
Keywords
polyvinylidene fluoride (PVDF) coatings, polymer coating, fluoropolymers, paint coatings, adhesion, chemical resistance, fluoroolefins
Abstract

A review of developments and scientific publications in the field of protective coatings based on polyvinylidene fluoride and vinylidene fluoride copolymers is presented. Chemical properties of the polymer, its polymorphic modifications, peculiarities of dissolution and properties of obtained dispersions in the environment of organic solvents are described. Advantages and disadvantages of obtained protective coatings are given. A review of research results on modification of polyvinylidene fluoride dispersions with inorganic fillers and preparation of superhydrophobic coatings is presented.

Reference list
  1. Kablov E.N. Materials of the new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  2. Kablov E.N. What is the future to be made of? Materials of a new generation, technologies for their creation and processing – the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  3. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, p. 24.
  4. Huang X., Tepylo N., Pommier-Budinger V. et al. A survey of acephobic coatings and their potential use in a hybrid coating/active ice protection system for aerospace applications. Progress in Aerospace Sciences, 2019, vol. 105, pp. 74–97.
  5. Shuldeshov E.M., Nazarov I.A., Ivanov M.S., Donskih I.N. Decoratively finishing materials for wall panels of passenger cab and the crew cockpit of air vehicles (review). Trudy VIAM, 2022, no. 11 (117), paper no. 05. Available at: http://www.viam-works.ru (accessed: August 03, 2022). DOI: 10.18577/2307-6046-2020-0-11-38-47.
  6. Zhivulin B.E., Zherebtsov D.A., Lebedeva S.M. Synthesis and properties of products of high-temperature heat treatment of polyvinylidene fluoride. Fizika tverdogo tela, 2017, vol. 59, no. 2, pp. 394–398.
  7. Leivo E., Wilenius T., Kinos T. et al. Properties of thermally sprayed fluoropolymer PVDF, ECTFE, PFA and FEP coatings. Progress in Organic Coatings, 2004, vol. 49, pp. 69–73.
  8. Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), paper no. 07. Available at: http://www.viam-works.ru (accessed: August 03, 2022). DOI: 10.18577/2307-6046-2019-0-5-62-67.
  9. Pavlov A.V., Andreeva N.P., Pavlov M.R., Merkulova Yu.I. Climatic tests of paint coating based on fluoroplastic and features of its destruction. Trudy VIAM, 2019, no. 5, paper no. 12. Available at: http://www.viam-works.ru (accessed: August 03, 2022). DOI: 10.18577/2307-6046-2019-0-5-103-110.
  10. Beider E.Ya., Donskoy A.A., Zhelezina G.F. and others. Experience in the use of fluoropolymer materials in aviation technology. Rossiyskiy khimicheskiy zhurnal, 2008, vol. LII, no. 3, pp. 30–44.
  11. Kuznetsova V.A., Marchenko S.A., Emelyanov V.V., Zheleznyak V.G. Study of the influence of molecular mass of epoxy oligomers and hardeners on the operational properties of paint coatings. Aviation materials and technology, 2021, no. 1 (62), paper no. 07. Available at: http://www.journal.viam.ru (accessed: August 03, 2022). DOI: 10.18577/2713-0193-2021-0-1-71-79.
  12. Yun H.K., Yong S.K., Min Y.S., Myung J.M. Corrosion Protection Performance of PVDF/PMMA-Blended Coatings by Electrochemical Impedance Method. Journal Electrochemical Science and Technology, 2018, vol. 9, no. 1, pp. 1–8.
  13. Wood K.A., Tanaka A., Zheng M., Garcia D. 70 % PVDF Coatings for Highly Weatherable Architectural Coatings. Available at: https://www.researchgate.net/publication/238712168_70_PVDF_Coatings_for_Highly_Weatherable_Architectural_Coatings (accessed: August 03, 2022).
  14. Sonnendecker A., Crouse P.L. PVDF coatings: Solvent compatibility and the effect of plasticisers on the morphology, physical and mechanical properties of high molecular-weight PVDF. Fluoropolymers: research, production problems, new applications: coll. abstracts of the Intern. conf. Kirov: Publishing House of Vyatsk State Univ., 2020, pp. 55–59.
  15. Kostitsyn A.V., Golikov I.V., Kulikova O.A. Influence of the concentration of the network-forming component on the properties of polymer mixtures based on polyvinylidene fluoride. Khimiya i khimicheskaya tekhnologiya, 2009, vol. 52, no. 8, pp. 82–84.
  16. Kostitsyn A.V., Golikov I.V., Sakharov L.A. Influence of polymethyl methacrylate on the rheological properties of polyvinylidene fluoride dispersions in organic solvents of various nature. Khimiya i khimicheskaya tekhnologiya, 2008, vol. 51, no. 4, pp. 77–78.
  17. Fluoropolymer organodispersion: pat. 2047625 Rus. Federation; filed 02.07.82; publ. 10.11.95.
  18. McKeen L.W. Fluorinated coatings and finishes handbook: the definitive user’s guide and databook. William Andrew Inc., 2006, 367 p.
  19. Screening polymer film and method for its production: pat. 2705967 Rus. Federation; filed 23.05.18; publ. 12.11.19.
  20. Mohamdi S., Sharifi-Sanjani N., Foyouhi A. Evaluation of graphene nanosheets influence on the physical properties of PVDF/PMMA blend. Journal of Polymer Research, 2013, vol. 20, no. 46, pp. 1–10.
  21. Kondrashov E.K., Malovа N.E. Paint coatings based on copolymers of trifluorochloroethylene. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 39–44. DOI: 10.18577/2071-9140-2015-0-2-39-44.
  22. hotocatalytic coating of protective rubber-fabric material: pat. RU 2622439C2; filed 13.10.15; publ. 15.06.17.
  23. Chernyavsky G.G., Baranets I.V., Purtseladze V.I., Emelyanov G.A. Mixed compositions based on low molecular weight fluoro(co)polymers of vinylidene fluoride with hexafluoropropylene and determination of the physical and mechanical properties of their vulcanizates. Molodoy ucheniy, 2014, no. 14.1 (73.1), pp. 48–50.
  24. Low molecular weight ternary copolymers of vinylidene fluoride and a monomer containing a fluorosulfate group: pat. RU 2432366C1; filed 09.04.10; publ. 27.10.11.
  25. Buznik V.M. Superwaterproof materials on the basis of fluoropolymers. Aviacionnye materialy i tehnologii, 2013, no. 1, pp. 29–34.
  26. Nam K.L., Young H.K., Tae G.I. et al. Analysis of PVDF Coating Properties with Addition of Hydrophobically Modified Fumed Silica. Corrosion science and technology, 2019, vol. 18, no. 6, pp. 232–242.
  27. Kovrizhkina N.A., Kuznetsova V.A., Silaeva A.A., Marchenko S.A. Ways to improve the properties of paint coatings by adding different fillers (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 41–48. DOI: 10.18577/2071-9140-2019-0-4-41-48.
  28. Liling Y., Ke W., Lin Y. Super hydrophobic property of PVDF/CaCO3 nanocomposite coatings. Journal of Material Science Letters, 2003, vol. 22, pp. 1713–1717.
  29. Method for obtaining an anticorrosive wear-resistant coating on magnesium alloys: pat. 2617088 Rus. Federation; filed 18.02.16; publ. 19.04.17.
  30. Method for obtaining protective superhydrophobic coatings on aluminum alloys: pat. 2617088 Rus. Federation; filed 29.06.21; publ. 13.05.22.
  31. Chaoyi P., Suli X., Zhiqing Y. et al. Preparation and anti-icing of superhydrophobic PVDF coating on a wind turbine blade. Applied Surface Science, 2012, vol. 259, pp. 764–768.
  32. Cai X., Lei T., Sun D., Lin L. A critical analysis of the α, β and γ phases in poly(vinilidene fluoride) using FTIR. RSC Advances, 2017, vol. 7, no. 25, pp. 15382–15389.
  33. Kochervinsky V.V. Structure and properties of block polyvinylidene fluoride and systems based on it. Uspekhi khimii, 1996, vol. 65, no. 10, pp. 936–987.
  34. Kochervinsky V.V. Structure formation in crystallizing ferroelectric polymers. Fizika tverdogo tela, 2006, vol. 48, no. 6, pp. 1016–1018.