Influence of operational factors on the properties of fabric-film material for low-pressure air ducts of the air conditioning system of aircraft

Ivanov M.S., Pavlukovich N.G., Donskih I.N., Morozova V.S.
Ivanov M.S., Pavlukovich N.G., Donskih I.N., Morozova V.S. Influence of operational factors on the properties of fabric-film material for low-pressure air ducts of the air conditioning system of aircraft // Proceedings of VIAM. 2023. No. 4. DOI: 10.18577/2307-6046-2023-0-4-118-127. URL: https://www.viam-works.ru/en/journal/2023/4/11
Keywords
low pressure air ducts, air conditioning system, coated textile material, resource tests, material aging, climatic factors, operational factors
Abstract

Within the framework of the general qualification of the VRT-12 brand coated textile material developed by the «Kurchatov Institute» ‒ VIAM for the manufacture of a sealed shell of flexible air ducts of the air conditioning system of aircraft, studies of fire safety characteristics and the influence of operational factors on the properties of the material were carried out. Compliance of the material with aviation regulations on flammability, smoke formation and release of toxic gases has been established. Resistance to temperatures from ‒60 to +80 °C, high humidity, mold fungi and aggressive liquids has been confirmed.

Reference list
  1. Voronin G.I. Air conditioning systems on aircraft. Moscow: Mashinostroenie., 1973, 443 p.
  2. Kablov E.N. Materials and chemical technologies for aviation equipment. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, pp. 520–530.
  3. Kravchenko A.G., Shilova A.K., Tamba-Tamba V.P., Ozersky A.I. Overview of the main units of air conditioning systems for aircraft. Tekhnika. Tekhnologii. Inzheneriya, 2017, no. 3, pp. 24–27. Available at: https://moluch.ru/th/8/archive/62/2532/ (accessed: December 01, 2022).
  4. Savin S.P. The use of modern polymeric composite materials in airframe construction. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2012, vol. 14, no. 4 (2), pp. 686–693.
  5. Platonov M.M., Nazarov I.A., Nesterova T.A. Tissue-film materials for inflatable air rescue equipment. Novosti materialovedeniya. Nauka i tekhnika, 2013, no. 2, art. 6. Available at: http://www.materialsnews.ru (accessed: December 01, 2022).
  6. Levant M.G., Ponomarev P.A. Creation of domestic materials for the manufacture of shells for aeronautical complexes. Polet, 2008, no. 12, pp. 57–60.
  7. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: December 01, 2022). DOI: 10.18577/2071-9140-2021-0-4-70-80.
  8. Ivanov M.S., Veshkin E.A., Satdinov R.A., Donskikh I.N. New domestic coated textile material for flexible air conditioning ducts of flight vehicles. Trudy VIAM, 2019, no. 4 (76), paper no. 07. Available at: http://www.viam-works.ru (accessed: December 01, 2022). DOI: 10.18577/2307-6046-2019-0-4-57-66.
  9. Aviation regulations. Airworthiness standards for transport category aircraft: AP-25. 5th ed., rev. 1–8. Moscow: Aviaizdat, 2015, 278 p.
  10. Barbotko S.L. Development of the fire safety test methods for aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.
  11. Kablov E.N., Startsev V.O., Inozemtsev A.A. The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  12. Kablov E.N. The key problem is materials. Trends and guidelines for Russia's innovative development. Moscow: VIAM, 2015, pp. 458–464.
  13. Kablov E.N. Creation of a national network of climatic stations is a necessary condition for the reliability and resource of aviation equipment. Krylya Rodiny, 2010, no. 8, pp. 3–6.
  14. Laptev A.B., Pavlov M.R., Novikov A.A., Slavin A.V. Current trends in the development of testing materials for resistance to climate factors (review). Part 1. Testing of new materials. Trudy VIAM, 2021, no. 1 (95), paper no. 12. Available at: http://www.viam-works.ru (accessed: December 01, 2022). DOI: 10.18577 / 2307-6046-2021-0-1-114-122.
  15. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  16. Kurs M.G., Nikolayev E.V., Abramov D.V. Full-scale and accelerated tests of metallic and nonmetallic materials: key factors and specialized stands. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 66–73. DOI: 10.18577/2071-9140-2019-0-1-66-73.
  17. Aviation regulations. Airworthiness standards for civil light aircraft: AP-23. 4th ed., rev. 1–5. Moscow: Aviaizdat, 2014, 207 p.
  18. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.