Influence of external influences on the coefficient of linear thermal expansion of carbon fiber plastics

Part 3. Climatic aging of nanomodified cyanester carbon plastic
Startsev V.O., Vardanyan A.M.
Startsev V.O., Vardanyan A.M. Influence of external influences on the coefficient of linear thermal expansion of carbon fiber plastics. Part 3. Climatic aging of nanomodified cyanester carbon plastic // Proceedings of VIAM. 2023. No. 4. DOI: 10.18577/2307-6046-2023-0-4-99-117. URL: https://www.viam-works.ru/en/journal/2023/4/10
Keywords
carbon fiber, cyanoether binder, carbon plastics, multilayer nanotubes, coefficient of linear thermal expansion, strength, glass transition temperature, thermal cycles, post-curing, degradation, microcracks, aging
Abstract

In the third part of the article, the influence of additives of multilayer carbon nanotubes (astralene) on the change in the coefficient of linear thermal expansion (CLTE) of CFRP based on a cyanoether binder, exposed for 24 months in a temperate climate and laboratory simulation conditions, is considered. It is shown that the presence of 0.5 and 3.0 wt. % astralene significantly changes the CLTE in the glassy and highly elastic states of the binder carbon fiber in the initial state and at the stages of 24 months of climatic testing in the modes of standard exposure on an open atmospheric stand and exposure with weekly thermal cycles simulating the mode of takeoff and landing of an aircraft. The mechanism of the stabilizing effect of the nanomodifier was revealed when comparing the CLTE, compressive and bending strengths, and the glass transition temperature of the binder during the aging of carbon fiber in natural and simulated laboratory conditions.

Reference list
  1. Gunyaev G.M., Chursova L.V., Komarova O.A., Gunyaeva A.G. Constructional carbon the plastics modified by nanoparticles. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 277–286.
  2. Gunyaev G.M., Chursova L.V., Raskutin A.E., Gunyaeva A.G. Lightning firmness of modern polymeric composites. Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 20–22.
  3. Liew K.M., Lei Z.X., Zhang L.W. Mechanical analysis of functionally graded carbon nanotube reinforced composites: A review. Composite Structures, 2015, vol. 120, pp. 90–97.
  4. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Prospects for the use of carbon-containing nanoparticles in binders for polymer composite materials. Rossiyskie nanotekhnologii, 2012, no. 3–4, pp. 28–46.
  5. Sharma H., Kumar A., Rana S., Guadagno L. An Overview on Carbon Fiber-Reinforced Epoxy Composites: Effect of Graphene Oxide Incorporation on Composites Performance. Polymers, 2022, vol. 14, art. 1548.
  6. Cha J., Kim J., Ryu S., Hong S.H. Comparison to mechanical properties of epoxy nanocomposites reinforced by functionalized carbon nanotubes and graphene nanoplatelets. Composites. Part B: Engineering, 2019, vol. 162, pp. 283–288.
  7. Chhetri S., Adak N.C., Samanta P. et al. Functionalized reduced graphene oxide/epoxy composites with enhanced mechanical properties and thermal stability. Polymer Testing, 2017, vol. 63, pp. 1–11.
  8. Shivakumar H., Renukappa N.M., Shivakumar K.N., Suresha B. The Reinforcing Effect of Graphene on the Mechanical Properties of Carbon-Epoxy Composites. Open Journal of Composite Materials, 2020, vol. 10, pp. 27–44.
  9. Bolshakov V.A., Kondrashov S.V., Merkulova Y.I., Dyachkova T.P., Yurkov G.Y., Ilyichyov F.V. Research of nanomodified carbon composites before and after hydrothermal aging. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 61–66. DOI: 10.18577/2071-9140-2015-0-2-61-66.
  10. Raimondo M., Catauro M., Guadagno L. Strategic Role of Carbon Nanotube Functionalization on the Multifunctional Properties of Structural Epoxy Nanocomposites. Macromolecular Symposia, 2022, vol. 404, аrt. 2100275.
  11. Liang X., Dai F. Epoxy Nanocomposites with Reduced Graphene Oxide-Constructed Three-Dimensional Networks of Single Wall Carbon Nanotube for Enhanced Thermal Management Capability with Low Filler Loading. ACS Applied Materials and Interfaces, 2020, vol. 12, pp. 3051–3058.
  12. Huh S.H., Choi S.H., Ju H.M., Kim D.H. Properties of interlayer thermal expansion of 6-layered reduced graphene oxide. Journal of the Korean Physical Society, 2014, vol. 64, pp. 615–618.
  13. Dong C. Coefficient of thermal expansion of single-wall carbon nanotube reinforced nanocomposites. Journal of Composites Science, 2021, vol. 5, art. 26.
  14. Fasanella N., Sundararaghavan V. Atomistic modeling of thermomechanical properties of SWNT/Epoxy nanocomposites. Modelling and Simulation in Materials Science and Engineering, 2015, vol. 23, аrt. 065003.
  15. Ackermann A.C., Fischer M., Wick A. et al. Mechanical, Thermal and Electrical Properties of Epoxy Nanocomposites with Amine-Functionalized Reduced Graphene Oxide via Plasma Treatment. Journal of Composites Science, 2022, vol. 6, art. 153.
  16. Wang S., Tambraparni M., Qiu J. et al. Thermal expansion of graphene composites. Macromolecules, 2009, vol. 42, pp. 5251–5255.
  17. Wang S., Liang Z., Gonnet P. et al. Effect of nanotube functionalization on the coefficient of thermal expansion of nanocomposites. Advanced Functional Materials, 2007, vol. 17, no. 1, pp. 87–92.
  18. Seong M., Kim D.S. Effects of facile amine-functionalization on the physical properties of epoxy/graphene nanoplatelets nanocomposites. Journal of Applied Polymer Science, 2015, vol. 132, аrt. 42269.
  19. Schapery R.A. Thermal Expansion Coefficients of Composite Materials Based on Energy Principles. Journal of Composite Materials, 1968, vol. 2, no. 3, pp. 380–404.
  20. Kamarian S., Bodaghi M., Isfahani R.B. et al. Influence of carbon nanotubes on thermal expansion coefficient and thermal buckling of polymer composite plates: experimental and numerical investigations. Mechanics Based Design of Structures and Machines, 2021, vol. 49, no. 2, pp. 217–232.
  21. Startsev V.O., Nikolaev E.V., Vardanyan A.M., Nechaev A.A. The influence of climatic fac-tors on residual stresses in nanomodified cyanate ester-based CFRP. Trudy VIAM, 2021, no. 8 (102), paper no. 12. Available at: http://www.viam-works.ru (accessed: December 05, 2022). DOI: 10.18577/2307-6046-2021-0-8-104-112.
  22. Awad S.A., Fellows C.M., Mahini S.S. Effects of accelerated weathering on the chemical, mechanical, thermal and morphological properties of an epoxy/multi-walled carbon nanotube composite. Polymer Testing, 2018, vol. 66, pp. 70–77.
  23. Awad S.A., Fellows C.M., Mahini S.S. Evaluation of bisphenol A-based epoxy resin containing multiwalled carbon nanotubes to improve resistance to degradation. Journal of Composite Materials, 2019, vol. 53, pp. 2981–2991.
  24. Chiang C.-L., Chou H.-Y., Shen M.-Y. Effect of environmental aging on mechanical properties of graphene nanoplatelet/nanocarbon aerogel hybrid-reinforced epoxy/carbon fiber composite laminates. Composites. Part A: Applied Science and Manufacturing, 2020, vol. 130, art. 105718.
  25. Aslan A., Salur E., Düzcükoğlu H. et al. The effects of harsh aging environments on the properties of neat and MWCNT reinforced epoxy resins. Construction and Building Materials, 2021, vol. 272, art. 121929.
  26. Jojibabu P., Ram G.D.J., Deshpande A.P., Bakshi S.R. Effect of carbon nano-filler addition on the degradation of epoxy adhesive joints subjected to hygrothermal aging. Polymer Degradation and Stability, 2017, vol. 140, pp. 84–94.
  27. Arribas C., Prolongo M.G., Sánchez-Cabezudo M. et al. Hydrothermal ageing of graphene/carbon nanotubes/epoxy hybrid nanocomposites. Polymer Degradation and Stability, 2019, vol. 170, art. 109003.
  28. Kara M., Ak S., Uyaner M. et al. The Effect of Hydrothermal Aging on the Low-Velocity Impact Behavior of Multi-Walled Carbon Nanotubes Reinforced Carbon Fiber/Epoxy Composite Pipes. Applied Composite Materials, 2021, vol. 28, no. 5, pp. 1567–1587.
  29. Sánchez-Romate X.F., Terán P., Prolongo S.G. et al. Hydrothermal ageing on self-sensing bonded joints with novel carbon nanomaterial reinforced adhesive films. Polymer Degradation and Stability, 2020, vol. 177, art. 109170.
  30. Yang T., Lu S., Song D. et al. Effect of Nanofiller on the Mechanical Properties of Carbon Fiber/Epoxy Composites under Different Aging Conditions. Materials, 2021, vol. 14, art. 7810.
  31. Wang J., Guan L., Ge J. Research on Aging Resistance of Three Phase Composites for Anti-collision Intelligent Control of Bridge Engineering. Journal of Physics: Conference Series, 2021, vol. 2095, аrt. 012041.
  32. Mach P., Geczy A., Polanský R., Bušek D. Glass transition temperature of nanoparticle-enhanced and environmentally stressed conductive adhesive materials for electronics assembly. Journal of Materials Science: Materials in Electronics, 2019, vol. 30, pp. 4895–4907.
  33. Glaskova-Kuzmina T., Aniskevich A., Zarrelli M. et al. Effect of filler on the creep characteristics of epoxy and epoxy-based CFRPs containing multi-walled carbon nanotubes. Composites Science and Technology, 2014, vol. 100, pp. 198–203.
  34. Glaskova-Kuzmina T., Aniskevich A., Martone A. et al. Effect of moisture on elastic and viscoelastic properties of epoxy and epoxy-based carbon fibre reinforced plastic filled with multiwall carbon nanotubes. Composites. Part A: Applied Science and Manufacturing, 2016, vol. 90, pp. 522–527.
  35. Glaskova-Kuzmina T., Aniskevich A., Papanicolaou G. et al. Hydrothermal aging of an epoxy resin filled with carbon nanofillers. Polymers, 2020, vol. 12, art. 1153.
  36. Kondrashov S.V., Merkulova Yu I., Marakhovskii P. S. et al. Degradation of physicomechanical properties of epoxy nanocomposites with carbon nanotubes upon heat and humidity aging. Russian Journal of Applied Chemistry, 2017, vol. 90, no. 5, pp. 788–796.
  37. Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples’ temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577/2071-9140-2020-0-4-47-58.
  38. Perov N.S., Startsev V.O., Chutskova E.Yu. et al. Properties of carbon plastic based on polycyanurate binder after exposure to various natural and artificial environments. Materialovedenie, 2017, no. 2, pp. 3–9.
  39. Slavin A.V., Startsev O.V. Properties of aircraft glass- and carbonfibers reinforced plastics at the early stage of natural weathering. Trudy VIAM, 2018, no. 9 (69), paper no. 08. Available at: http://www.viam-works.ru (accessed: December 5, 2022). DOI: 10.18577/2307-6046-2018-0-9-71-82.
  40. Startsev V.O., Slavin A.V. Carbon and glass reinforced polymer based on solvent-free binders resistance to the impact of a moderate cold and moderate warm climate. Trudy VIAM, 2021, no. 5 (99), paper no. 12. Available at: http://www.viam-works.ru (accessed: December 5, 2022). DOI: 10.18577/2307-6046-2021-0-5-114-126.
  41. Startsev V.O., Plotnikov V.I., Antipov Yu.V. Reversible influence of moisture on the mechanical properties of PCM after weathering. Trudy VIAM, 2018, no. 5 (65), paper no. 12. Available at: http://www.viam-works.ru (accessed: December 5, 2022). DOI: 10.18577/2307-6046-2018-0-5-110-118.
  42. Startsev O.V., Kurs I.S., Deev I.S., Nikishin E.F. Thermal expansion of KMU-4L carbon fiber after 12 years of exposure in outer space. Voprosy materialovedeniya, 2013, no. 4 (76), pp. 77–85.
  43. Startsev V.O., Molokov M.V., Grebeneva T.A., Tkachuk A.I. Dynamic mechanical and thermomechanical analysis of reversible plasticization of epoxy-diane resin-diaminodiphenylsulfon system by moisture. Polymer Science. Series A, 2017, vol. 59, no. 5, pp. 640–648.
  44. Startsev O.V., Vapirov Y.M., Lebedev M.P., Kychkin A.K. Comparison of Glass-Transition Temperatures for Epoxy Polymers Obtained by Methods of Thermal Analysis. Mechanics of Composite Materials, 2020, vol. 56, no. 2, pp. 227–240.
  45. Odegard G.M., Bandyopadhyay A. Physical aging of epoxy polymers and their composites. Journal of Polymer Science. Part B: Polymer Physics, 2011, vol. 49, no. 24, pp. 1695–1716.
  46. Kong E.S.-W. Physical aging in epoxy matrices and composites. Epoxy Resins and Composites. Berlin, 1986, pp. 125–171.
  47. Startsev O.V., Krotov A.S., Golub P.D. Effect of climatic and radiation ageing on properties of VPS-7 glass fibre reinforced epoxy composite. Polymer Degradation and Stability, 1999, vol. 63, no. 3, pp. 353–358.
  48. Di Ludovico M., Piscitelli F., Prota A. et al. Improved mechanical properties of CFRP laminates at elevated temperatures and freeze-thaw cycling. Construction and Building Materials, 2012, vol. 31, pp. 273–283.
  49. Park S.Y., Choi W.J., Choi C.H., Choi H.S. An experimental study into aging unidirectional carbon fiber epoxy composite under thermal cycling and moisture absorption. Composite Structures, 2019, vol. 207, pp. 81–92.
  50. Herakovich C.T., Hyer M.W. Damage-induced property changes in composites subjected to cyclic thermal loading. Engineering Fracture Mechanics, 1986, vol. 25, no. 5, pp. 779–791.
  51. Kato A., Goto K., Kogo Y., Inoue R. Changes in thermal expansion coefficient of CFRP laminate due to thermal cycle. ICCM International Conferences on Composite Materials, 2017, vol. 2017, art. 138793.
  52. Startsev O.V., Perepechko I.I. Molecular mobility and relaxation in an epoxy matrix. 1. Influence of the reinforcing filler. Mechanics of Composite Materials, 1984, vol. 20, no. 3, pp. 271–274.
  53. Startsev O.V., Mashinskaya G.P., Yartsev V.A. Molecular mobility and relaxation processes in an epoxy matrix. 2. Effects of weathering in humid subtropical climate. Mechanics of Composite Materials, 1985, vol. 20, no. 4, pp. 406–409.
  54. Kablov E.N., Startsev O.V., Panin S.V. Moisture transfer in carbon-fiber-reinforced plastic with degraded surface. Doklady Physical Chemistry, 2015, vol. 461, no. 2, pp. 80–83.
  55. Salnikov V.G., Startsev O.V., Lebedev M.P. et al. Influence of daily and seasonal changes in relative humidity and temperature on moisture saturation of carbon fiber in open climatic conditions. Vse materialy. Entsiklopedicheskiy spravochnik, 2022, no. 5, pp. 2–10.
  56. Startsev V.O., Nechaev A.A. Moisture transfer in cyanoether carbon plastic during accelerated and full-scale climatic tests. Physical and mechanical tests, strength and reliability of modern structural and functional materials: materials of XIV All-Russia. conf. for testing and research of the properties of materials "TestMat". Moscow, 2022, pp. 214–226.
  57. Panin S.V., Startsev O.V., Krotov A.S., Medvedev I.M., Frolov A.S. Corrosion and aging of structural materials surface studied by 3D microscopy. Trudy VIAM, 2014, no. 12, paper no. 12. Available at: http://www.viam-works.ru (accessed: December 5, 2022). DOI: 10.18577/2307-6046-2014-0-12-12-12.
  58. Startsev VO, Valevin EO, Gulyaev AI. The influence of polymer composite materials’ surface weathering on its mechanical properties. Trudy VIAM, 2020, no. 8 (90), paper no. 07. Available at: http://www.viam-works.ru (accessed: December 5, 2022). DOI: 10.18577/2307-6046-2020-0-8-64-76.
  59. Startsev O.V., Medvedev I.M., Kurs M.G. Hardness as the indicator of corrosion of aluminum alloys in sea conditions. Aviacionnye materialy i tehnologii, 2012, no. 3, pp. 16–19.