Precipitation of η-phase during heat treatment in Ni–Fe–Co–Nb–Ti alloy

Ovsepyan S.V., Akhmedzyanov M.V., Filonova E.V., Zaysev D.V.
Ovsepyan S.V., Akhmedzyanov M.V., Filonova E.V., Zaysev D.V. Precipitation of η-phase during heat treatment in Ni–Fe–Co–Nb–Ti alloy // Proceedings of VIAM. 2023. No. 4. DOI: 10.18577/2307-6046-2023-0-4-3-13. URL: https://www.viam-works.ru/en/journal/2023/4/1
Keywords
nickel-iron superalloy, heat treatment, microstructure, phase, lamellar particle, temperature–time–precipitation diagram
Abstract

The effect of annealing at the temperature of 800–1040 °С on the η-phase formation in the weldable wrought VZh176 alloy of the Ni–Fe–Co–Nb–Ti system, intended for use in gas turbine engines, has been investigated. It is shown that annealing leads to the precipitation of η-phase particles and change the shape and distribution: from short plates at the grain boundaries to the Widmanstatten structure. The dependence of the quantity of the phase on the duration of processing is established. The composition and crystallographic structure of the η-plates are determined by the methods of transmission electron and scanning microscopy, using the methods of backscattered electron diffraction and х-ray microanalysis. A diagram of the change of the η-phase from temperature and duration of treatment was built.

Reference list
  1. Sims Ch.T., Stoloff N.S., Hagel U.K. Superplanes II: heat-resistant materials for aerospace and industrial power plants. Moscow: Metallurgy, 1995, 384 p.
  2. Reed R.C. The Superalloys: Fundamentals and Applications. N.Y.: Cambridge University Press, 2008, 392 р.
  3. Kablov E.N., Evgenov A.G., Mazalov I.S., Shurtakov S.V., Zaitsev D.V., Prager S.M. The evolution of the structure and properties of a high-resistant heat-resistant alloy VZh159 obtained by the method of selective laser fusion. Part I. Materialovedenie, 2019, no. 3, pp. 9–17.
  4. Kablov E.N., Letnikov M.N., Ospennikova O.G., Bakradze M.M., Shestakova A.A. Particulars of the precipitation strengthening γʹ-phase during aging of heat-resistant wrought nickel superalloy VZh175-ID. Trudy VIAM, 2019, no. 9 (81), paper no. 01. Available at: http://www.viam-works.ru (accessed: November 11, 2022). DOI: 10.18577/2307-6046-2019-0-9-3-14.
  5. Lomberg B.S., Shestakova A.A., Bakradze M.M., Karachevtsev F.N. The investigation of the stability of γ′-phase with size below 100 nm in Ni-base superalloy VZh175-ID. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 3–10. DOI: 10.18577/2071-9140-2018-0-4-3-10.
  6. Shestakova A.A., Karachevtsev F.N., Zhebelev N.M. The investigation of the influence of ageing temperature on structural and phase transformations in VZh177. Trudy VIAM, 2018, no. 5, papers no. 01. Available at: http://www.viam-works.ru (accessed: November 11, 2022). DOI: 10.18577/2307-6046-2018-0-5-3-11.
  7. Lomberg B.S., Shestakova A.A., Letnikov M.N., Bakradze M.M. The influence of temperature and stresses on nature of nanosize γʹ-phase in Ni-base superalloy VZh175-ID. Trudy VIAM, 2019, no. 12 (84), paper no. 01. Available at: http://www.viam-works.ru (accessed: November 11, 2022). DOI: 10.18577/2307-6046-2019-0-12-3-10.
  8. Sun F. Achieving High Tensile Strength of Heat-Resistant Ni-Fe-Based Alloy by Controlling Microstructure Stability for Power Plant Application. Crystals, 2022, vol. 12, is. 10 (1433), pp. 1–11. DOI: 10.3390/cryst12101433.
  9. Kappmeyer G., Hubig C., Hardy M. et al. Modern Machining of Advanced Aerospace Alloys – Enabler for Quality and Performance. Procedia CIRP, 2012, no. 1, pp. 28–43. DOI: 10.1016/j.procir.2012.04.005.
  10. Ducki K.J. Analysis of the Precipitation and Growth Processes of the Intermatallic Phases in an Fe–Ni Superalloy. Superalloy. Intech open Science, 2015, pp. 111–137.
  11. Nickel-Iron alloys market report: Global Forecast from 2022 to 2030. Available at: www.dataintelo.com/report/nickel-iron-alloys-market (accessed: November 11, 2022).
  12. Kobayashi S., Otsuka T., Watanabe R. et al. Alloying Effects on the Competition Between Discontinuous Precipitation Versus Continuous Precipitation of δ/η Phases in Model Ni-Based Superalloys. Superalloys 2020: Proceedings of the 14th International Symposium on Superalloys. Springer Cham, 2020, pp. 163–170. DOI: 10.1007/978-3-030-51834-9_16.
  13. Tang L. Precipitation sequences in rapidly solidified Allvac 718 Plus alloy during solution treatment. Journal of Materials Science & Technology, 2022, vol. 128, pp. 180–194. DOI: 10.1016/j.jmst.2022.03.031.
  14. Guo X., Kusabiraki K., Saji S. Intragranular precipitates in Incoloy Alloy 909. Scripta Materialia, 2001, vol. 44, is. 1, pp. 55–60. DOI: 10.1016/S1359-6462(00)00576-5.
  15. Lagow D.W. Materials Selection in Gas Turbine Engine Design and the Role of Low Thermal Expansion Materials. JOM, 2016, no. 68, pp. 2770–2775.
  16. Incoloy 903. Available at: www.specialmetals.com/documents/technical-bulletins/incoloy/incoloy-alloy-903.pdf (accessed: November 11, 2022).
  17. Incoloy 907. Available at: www.specialmetals.com/documents/technical-bulletins/incoloy/incoloy-alloy-907.pdf (accessed: November 11, 2022).
  18. Incoloy 909. Available at: www.specialmetals.com/documents/technical-bulletins/incoloy/incoloy-alloy-909.pdf (accessed: November 11, 2022).
  19. A heat-resistant deformable alloy based on a nickel with a low temperature coefficient of linear expansion and the product made from it: pat. 2721261 Rus. Federation; filed 11.12.19; publ. 18.05.20.
  20. Xiong U., Zhao L., Zhipeng W. et al. Effect of Long-term Aging on Properties of Low Expansion Superalloy GH2909. Chinese Journal of Materials Research, 2021, vol. 35, is. 5, pp. 330–338. DOI: 10.11901/1005.3093.2020.314.
  21. Wong M.J. Design of an Eta-Phase Precipitation-Hardenable Nickel-Based Alloy with the Potential for Improved Creep Strength Above 1023 K (750 °C). Metallurgical and Materials Transactions, 2015, no. 46. DOI: 10.1007/s11661-015-2898-0.
  22. Mohale N. Role of Eta Phase Evolution on Creep Properties of Nickel Base Superalloys Used In Advanced Electric Power Generation Plants. Open Access Dissertation. Michigan Technological University, 2021. DOI: 10.37099/mtu.dc.etdr/1295.
  23. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  24. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Priority directions for the development of technologies for the production of heat-resistant materials for aviation engineering. Problemy chernoy metallurgii i materialovedeniya, 2013, no. 3, pp. 47–54.
  25. Antonov S., Detrois M., Helmink R.C., Tin S. Precipitate phase stability and compositional dependence on alloying additions in γ–γ′–δ–η Ni-base superalloys. Journal of Alloys and Compounds, 2015, vol. 626, pp. 76–86.
  26. Rath M., Povoden-Karadeniz E., Kozeschnik Е. Precipitation Kinetic Modeling of the New Eta-Phase Ni6AlNb in Ni-Base Superalloys. Superalloys. Ed. M. Hardy et al. TMS, 2016, pp. 97–105.