Evaluation of the effect of antiadhesion composition on the free surface energy of carbon fiber-reinforced plastics

Savitsky R.S., Sudyin Yu.I.
Savitsky R.S., Sudyin Yu.I. Evaluation of the effect of antiadhesion composition on the free surface energy of carbon fiber-reinforced plastics // Proceedings of VIAM. 2023. No. 3. DOI: 10.18577/2307-6046-2023-0-3-39-47. URL: https://www.viam-works.ru/en/journal/2023/3/4
Keywords
boundary wetting angle, PCM molding, free surface energy (FSE), OWRK method, anti-adhesion fluid
Abstract

At present, the share of polymer composite materials (PCM) in the aviation industry is increasing year by year, which is why there is a growing interest in composite molding tooling. This interest can be explained by the fact that due to affinity of materials, a formed part and rigging have similar coefficients of thermal expansion, by means of which problems of warping and occurrence of residual stresses are eliminated. In article some factors of influence on service properties of tooling for PCM manufacturing are considered, the technique of control of tooling technological properties is offered, influence of antiadhesion liquids on free surface energy of PCM is shown.

Reference list
  1. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  2. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Prospects for the use of carbon-containing nanoparticles in binders for polymer composite materials. Rossiyskiye nanotekhnologii, 2013, vol. 8, no. 3–4, pp. 24–42.
  3. Gunyaev G.M., Kablov E.N., Aleksashin V.M. Modification of structural carbon fiber plastics with carbon nanoparticles. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 5–11.
  4. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Postnova M.V., Postnov V.I. Development experience out-of-autoclave methods of formation PCM Trudy VIAM, 2014, no. 4, paper no. 06. Available at: http://www.viam-works.ru (accessed: April 23, 2022). DOI 10.18577/2307-6046-2014-0-4-6-6.
  6. Veshkin E.A. Features of out-of-autoclave forming of poor-porous PCM. Trudy VIAM, 2016, no. 2 (38), paper no. 07. Available at: http://www.viam-works.ru (accessed: April 25, 2022). DOI: 10.1857/2307-6046-2016-0-2-7-7.
  7. Kolpachkov E.D., Petrova A.P., Kurnosov A.O., Sokolov I.I. Methods of molding aviation products from PCM (review). Trudy VIAM, 2019, no. 11 (83), paper no. 03. Available at: http://www.viam-works.ru (accessed: April 25, 2022). DOI: 10.18577/2307-6046-2019-0-11-22-36.
  8. Lopatin A.N., Zverkov I.D. Shaping molding tools production for composite parts by means of additive technologies. Aviacionnye materialy i tehnologii, 2019, no. 2 (55). pp. 53–59. DOI: 10.18577/2071-9140-2019-0-2-53-59.
  9. Malyugin A.S., Smirnov M.M. Development of large-sized non-metallic tooling for molding parts based on polyurethanes and hybrid plastics. Trudy MAI, 2010, no. 38, pp. 22–24.
  10. Tkachuk A.I., Terekhov I.V., Gurevich Ya.M., Kudryavtseva A.N. Application of bismaleimide VST-57 binder for obtaining heat-resistant dimensionally stable molds from polymer composite materials. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 32–40. DOI: 10.18577/2071-9140-2020-0-2-32-40.
  11. Equipment for molding products from polymer composite materials and method of its manufacture: pat. 2630798 Rus. Federation, no. 2016134245; filed 22.08.16; publ. 13.09.17.
  12. Ruppel V. Latest developments in the field of anti-adhesive compounds and coatings for master models and tooling in the production of composite products. Kompozitnyy mir, 2016, no. 5 (68), pp. 32–35.
  13. Postnov V.I., Petukhov V.I., Makrushin K.V., Yudin A.A. Investigation of anti-adhesive coatings during the molding of interior panels with a gelcoat layer. Aviacionnye materialy i tehnologii, 2009, no. 3 (12), pp. 23–25.
  14. Barannikov A.A., Satdinov R.A., Veshkin E.A., Kurshev E.V. The effect of atmospheric pressure plasma on the strength of an adhesive bond based on CFPR. Trudy VIAM, 2021, no. 12 (106), paper no. 06. Available at: http://www.viam-works.ru (accessed: April 25, 2022). DOI: 10.18577/2307-6046-2021-0-12-47-54.
  15. Barannikov A.A., Postnov V.I., Veshkin E.A., Satdinov R.A. The use of atmospheric pressure plasma as a method of preparing the surface of polymer composite materials for gluing. Reports of V All-Rus. sci.-tech. conf. "Polymer composite materials and production technologies of a new generation". Moscow: NRC "Kurchatov Institute" – VIAM, 2021, pp. 177–195.
  16. Babayan A.L. Surface energy of polymers (elastomer compositions): comparative analysis of surface energy values with polymer defectiveness parameters. Nauchnyy zhurnal KubGAU, 2017, no. 131, pp. 300–309.
  17. Langer M., Otto D. Methods for studying the surface characteristics of polymers after plasma treatment. Comparative analysis. Analitika, 2018, no. 2, pp. 68–74. DOI: 10.22184/2227-572X.2018.39.2.68.74.
  18. Missol V. Surface energy of phase separation in metals. Moscow: Metallurgiya, 1978. 176 p.