Influence of external influences on the coefficient of linear thermal expansion of carbon fiber plastics

Part 2. Comparison of the results of full-scale and laboratory climatic tests
Startsev V.O., Vardanyan A.M.
Startsev V.O., Vardanyan A.M. Influence of external influences on the coefficient of linear thermal expansion of carbon fiber plastics. Part 2. Comparison of the results of full-scale and laboratory climatic tests // Proceedings of VIAM. 2023. No. 3. DOI: 10.18577/2307-6046-2023-0-3-132-144. URL: https://www.viam-works.ru/en/journal/2023/3/12
Keywords
carbon fiber, cyanoether binder, carbon plastic, coefficient of linear thermal expansion, strength, climatic aging, thermal cycles, post-curing, destruction, microcracks
Abstract

The second section of the article presents the results of studies of the coefficient of linear thermal expansion (CLTE) of carbon fiber reinforced plastic based on the cyanoether binder VSC-14, exposed for 24 months in a moderately cold climate and laboratory simulation conditions. Two variants of full-scale climatic tests were studied: standard exposure on an open atmospheric stand and exposure with a combination of thermal cycles simulating the mode of takeoff and landing of an aircraft. To find out the reasons for the change in the CLTE, the results of measurements of the compressive and tensile strengths, as well as the glass transition temperature of the binder VSC-14, are analyzed.

Reference list
  1. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  2. Irving P., Soutis C. Polymer composites in the aerospace industry. Polymer Composites in the Aerospace Industry. 2nd ed. Woodhead Publishing, 2019, 688 p.
  3. Charitidis P.J. Criteria for the selection of carbon fiber composite materials for fighter aircraft. Advances in Materials Science and Engineering: An International Journal (MSEJ), 2018, vol. 5, no. 2/3/4, pp. 1–13.
  4. Shetty K., Bojja R., Srihari S. Effect of hygrothermal aging on the mechanical properties of IMA/M21E aircraft-grade CFRP composite. Advanced Composites Letters, 2020, vol. 29, рр. 1–9.
  5. Iijima N., Katogi H., Takemura K. Effect of Thermal Cycling after Water Absorption on Flexural Property of CFRP. Advanced Materials Research, 2015, vol. 1110, pp. 19–22.
  6. Cinquin J., Medda B. Influence of laminate thickness on composite durability for long term utilisation at intermediate temperature (100–150 °C). Composites Science and Technology, 2009, vol. 69, no. 9, pp. 1432–1436.
  7. Jedidi J., Jacquemin F., Vautrin A. Accelerated hydrothermal cyclical tests for carbon/epoxy laminates. Composites. Part A, 2006, vol. 37, pp. 636–645.
  8. Kumar B.G., Singh R.P., Nakamura T. Degradation of Carbon Fiber-Reinforced Epoxy Composites by Ultraviolet Radiation and Condensation. Journal of Composite Materials, 2002, vol. 36, no. 24, pp. 2713–2733.
  9. Kablov E.N., Startsev O.V., Deev I.S., Nikishin E.F. Properties of polymer composite materials after exposure to open space in near-Earth orbits. Vse materialy. Entsiklopedicheskiy spravochnik, 2012, no. 10, рр. 2–9.
  10. Startsev O.V., Nikishin E.F. Aging of polymer composite materials in open space. Mekhanika kompozitnykh materialov, 1993, no. 4, pp. 457–467.
  11. Dexter H.B. Long-term environmental effects and flight service evaluation of composite materials. NASA Technical Report TM-89067, 1987, 188 p.
  12. Startsev O.V., Mashinskaya G.P., Yartsev V.A. Molecular mobility and relaxation processes in an epoxy matrix. 2. Effects of weathering in humid subtropical climate. Mechanics of Composite Materials, 1985, vol. 20, no. 4, pp. 406–409.
  13. Tian W., Hodgkin J. Long-term aging in a commercial aerospace composite sample: Chemical and physical changes. Journal of Applied Polymer Science, 2010, vol. 115, no. 5, pp. 2981–2985.
  14. Kirillov V.N., Efimov V.A., Shvedkova A.K. Influence of climatic factors and mechanical loading on the properties of carbon fiber reinforced plastic with epoxy binder. Plasticheskiye massy, 2012, no. 2, pp. 3–7.
  15. Kafodya I., Xian G., Li H. Durability study of pultruded CFRP plates immersed in water and seawater under sustained bending: Water uptake and effects on the mechanical properties. Composites. Part B: Engineering, 2015, vol. 70, pp. 138–148.
  16. Startsev O.V., Lebedev M.P., Blaznov A.N. Aging of polymer composite materials in a loaded state (end). Vse materialy. Entsiklopedicheskiy spravochnik, 2020, no. 11, pp. 2–12.
  17. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite aviation materials: 3. Significant aging factors. Russian Metallurgy (Metally), 2012, no. 4, pp. 323–329.
  18. Startsev O.V., Medvedev I.M., Kurs M.G. Hardness as the indicator of corrosion of aluminum alloys in sea conditions. Aviacionnye materialy i tehnologii, 2012, no. 3, pp. 16–19.
  19. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymeric composite materials. Moscow: VIAM, 2021, 528 p.
  20. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE "VIAM" in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  21. Mishurov K.S., Pavlovskiy K.A., Imametdinov E.Sh. fiber reinforced plastic) VKU-27L. Trudy VIAM, 2018, no. 3 (63), paper no. 07. Available at: http://www.viam-works.ru (accessed: October 10, 2022). DOI: 10.18577/2307-6046-2018-0-3-60-67.
  22. Perov N.S., Startsev V.O., Chutskova E.Yu., Gulyaev A.I., Abramov D.V. Properties of carbon plastic based on polycyanurate binder after exposure to various natural and artificial environments. Materialovedenie, 2017, no. 2, pp. 3–9.
  23. Slavin A.V., Startsev O.V. Properties of aircraft glass- and carbonfibers reinforced plastics at the early stage of natural weathering. Trudy VIAM, 2018, no. 9 (69), paper no. 8. Available at: http://www.viam-works.ru (accessed: October 10, 2022). DOI: 10.18577/2307-6046-2018-0-9-71-82.
  24. Startsev V.O., Slavin A.V. Carbon and glass reinforced polymer based on solvent-free binders resistance to the impact of a moderate cold and moderate warm climate. Trudy VIAM, 2021, no. 5 (99), paper no. 12. Available at: http://www.viam-works.ru (accessed: October 10, 2022). DOI: 10.18577/2307-6046-2021-0-5-114-126.
  25. Startsev O.V., Perepechko I.I. Molecular mobility and relaxation in an epoxy matrix. 1. Influence of the reinforcing filler. Mechanics of Composite Materials, 1984, vol. 20, no. 3, pp. 271–274.
  26. Startsev V.O., Nikolaev E.V., Vardanyan A.M., Nechaev A.A. The influence of climatic factors on residual stresses in nanomodified cyanate ester-based CFRP. Trudy VIAM, 2021, no.8 (102), paper no. 12. Available at: http://www.viam-works.ru (accessed: October 10, 2022). DOI: 10.18577/2307-6046-2021-0-8-104-112.
  27. Startsev O.V., Kurs I.S., Deev I.S., Nikishin E.F. Thermal expansion of KMU-4L carbon fiber after 12 years of exposure in outer space. Voprosy materialovedeniya, 2013, no. 4 (76), pp. 77–85.
  28. Lebedev M.P., Startsev O.V., Petrov M.G., Kopyrin M.M. Formation of microcracks during climatic aging of polymer composite materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2022, no. 4, pp. 2–11.
  29. Sidorina A.I., Safronov A.M., Kutsevich K.E., Klimenko O.N. Carbon fabrics for aircraft products. Trudy VIAM, 2020, no. 12 (94), paper no. 05. Available at: http://www.viam-works.ru (accessed: October 10, 2022). DOI: 10.18577/2307-6046-2020-0-12-47-58.
  30. Kablov E.N., Startsev V.O., Inozemtsev A.A. The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  31. Crossman F.W., Mauri R.E., Warren W.J. Hygrothermal damage mechanisms in graphite-epoxy composites. NASA Contractor Reports, 1979, no. 3189. 157 p.
  32. Asai S., Goto K., Yoneyama S., Arikawa S., Kobayashi S. Effect of space environment on thermal and mechanical properties of CFRP. ICCM International Conferences on Composite Materials, 2015, vol. 2015, art. 43-16-2.
  33. Herakovich C.T., Hyer M.W. Damage-induced property changes in composites subjected to cyclic thermal loading. Engineering Fracture Mechanics, 1986, vol. 25, no. 5–6, pp. 779–791.
  34. Lafarie-Frenot M., Rouquie S. Influence of oxidative environments on damage in c/epoxy laminates subjected to thermal cycling. Composites Science and Technology, 2004, vol. 64, no. 10–11, pp. 1725–1735.
  35. Bowles D.E., Tompkins S.S. Prediction of Coefficients of Thermal Expansion for Unidirectional Composites. Journal of Composite Materials, 1989, vol. 23, no. 4, pp. 370–388.
  36. Rogers K.F., Kingston-Lee D.M., Phillips L.N. et al. The thermal expansion of carbon-fibre reinforced plastics. Journal of Materials Science, 1981, vol. 16, no. 10, pp. 2803–2818.
  37. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R., Grashchenkov D.V. Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis Part 3. Calculation of activation energy and thermal resource of polymeric composite materials on the basis of epoxy matrix. Trudy VIAM, 2016, no. 5 (41), paper no. 11. Available at: http://www.viam-works.ru (accessed: October 10, 2022). DOI: 10.18577/2307-6046-2016-0-5-11-11.
  38. Startsev O.V., Vapirov Y.M., Lebedev M.P., Kychkin A.K. Comparison of Glass-Transition Temperatures for Epoxy Polymers Obtained by Methods of Thermal Analysis. Mechanics of Composite Materials, 2020, vol. 56, no. 2, pp. 227–240.
  39. Evdokimov A.A., Petrova A.P., Pavlovskiy K.A., Gulyaev I.N. The influence of climatic ageing on the properties of PCM-based epoxy resin systems. Trudy VIAM, 2021, no. 3 (97), paper no. 12. Available at: http://www.viam-works.ru (accessed: October 10, 2022). DOI: 10.18577/2307-6046-2021-0-3-128-136.
  40. Kong E.S.-W. Physical aging in epoxy matrices and composites. Epoxy Resins and Composites. Berlin, 1986, pp. 125–171.
  41. Inamdar A., Yang Y.H., Prisacaru A. et al. High temperature aging of epoxy-based molding compound and its effect on mechanical behavior of molded electronic package. Polymer Degradation and Stability, 2021, vol. 188, art. 109572.
  42. Ogata M., Kinjo N., Kawata T. Effects of crosslinking on physical properties of phenol-formaldehyde novolac cured epoxy resins. Journal of Applied Polymer Science, 1993, vol. 48, no. 4, pp. 583–601.
  43. Khamidulin O.L., Madiyarova G.I., Rezvykh A.V. et al. Comparative analysis of thermal expansion and heat capacity of polymers based on a number of epoxy novolac resins in a wide temperature range. Vestnik tekhnologicheskogo universiteta, 2021, vol. 24, pp. 40–44.
  44. Startsev O.V., Krotov A.S., Golub P.D. Effect of climatic and radiation ageing on properties of VPS-7 glass fibre reinforced epoxy composite. Polymer Degradation and Stability, 1999, vol. 63, no. 3, pp. 353–358.
  45. Marahovskiy P.S., Maltceva E.Yu., Barinov D.Ya., Zuev A.V., Smirnov M.V. Experience in measuring the thermal linear expansion coefficient of combined cords using organic and glass fibers. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 82–87. DOI: 10.18577/2071-9140-2019-0-1-82-87.
  46. Park S.Y., Choi W.J., Choi C.H., Choi H.S. An experimental study into aging unidirectional carbon fiber epoxy composite under thermal cycling and moisture absorption. Composite Structures, 2019, vol. 207, pp. 81–92.
  47. Kablov E.N., Startsev V.O. The Influence of Internal Stresses on the Aging of Polymer Composite Materials: a Review. Mechanics of Composite Materials, 2021, vol. 57, no. 5, pp. 565–576.
  48. Shi Z., Zou C., Zhou F., Zhao J. Analysis of the Mechanical Properties and Damage Mechanism of Carbon Fiber/Epoxy Composites under UV Aging. Materials, 2022, vol. 15, no. 8, p. 2919.
  49. Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples’ temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577/2071-9140-2020-0-4-47-58.