Research of influence of the contents resin in CFRP on their mechanical properties
Mishkin S.I., Zhakova L.S., Klimenko O.N., Vasilchuk E.A. Research of influence of the contents resin in CFRP on their mechanical properties // Proceedings of VIAM. 2023. No. 2. DOI: 10.18577/2307-6046-2023-0-2-77-86. URL: https://www.viam-works.ru/en/journal/2023/2/7
Keywords
CFRP, thermo-oxidative destruction, carbon filler, resin content in CFRP, mechanical properties, thermosetting resin, thermoplastic, autoclave formation
Abstract
Research results on definition of the main mechanical properties constructional CFRP based on the carbon medium-modulus carbon fillers and woven carbon fillers and epoxy polymeric matrix depending on the mass contents are provided to them resin which determined by etching method. It is established that the mechanical characteristic same CFRP can change to 20 %. It is shown that for investigated CFRP the optimum contents resin is 33–34 mass of %.
Reference list
- Kablov E.N. Marketing of materials science, aircraft building and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5–6, pp. 40–44.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE "VIAM" in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
- Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
- Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
- Bondaletova L.I., Bondaletov V.G. Polymer composite materials: textbook at 2 parts. Tomsk: Tomsk Publ. House Polytech. Univ., 2013, part 1, 118 p.
- Kolobkov A.S. Polymer composite materials for various aircraft structures (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 05. Available at: http://www.viam-works.ru (accessed: December 12, 2021). DOI: 10.18577/2307-6046-2020-0-67-38-44.
- Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
- Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
- Mishkin S.I., Malakhovskiy S.S., Gunyaeva A.G., Gulyaev I.N. Features of definition the resin content in carbon fiber reinforced plastics based on various types of carbon fillers by thermo-oxidative destruction method. Trudy VIAM, 2020, no. 12 (94), paper no. 06. Available at: http://www.viam-works.ru (accessed: July 29, 2022). DOI: 10.18577/2307-6046-2020-0-12-59-66.
- State Standard R 56682–2015. Polymer and metal composites. Methods for determining the volume of the matrix, reinforcing filler and voids. Moscow: Standartinform, 2016, 26 p.
- Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
- ASTM D 3039 M-00. Standard Test Method for Tensile Properties of Polymer Matrix Composite Materials. ASTM International, 2000, pp. 1–13.
- ASTM D 6641M-14. Standard Test Method for Compressive Properties of Polymer Matrix Composite Materials Using a Combined Loading Compression (CLC) Test Fixture. ASTM International, 2014, pp. 1–9.
- ASTM D 2344 M-16. Standard Test Method for Short Beam Strength of Polymer Matrix Composite Materials and Their Laminates. ASTM International, 2016, pp. 1–8.