Influence of weft thread deflection in reinforcing filler on elastic-strength properties of PCM

Satdinov R.A., Savitsky R.S.
Satdinov R.A., Savitsky R.S. Influence of weft thread deflection in reinforcing filler on elastic-strength properties of PCM // Proceedings of VIAM. 2023. No. 2. DOI: 10.18577/2307-6046-2023-0-2-53-62. URL: https://www.viam-works.ru/en/journal/2023/2/5
Keywords
deviation, weft thread, properties, influence, deviation angle, strength
Abstract

Currently for the manufacture of prepregs a huge number of reinforcing fillers are produced. All fillers are subject to certain technical requirements, including appearance however there is no requirement for the angle of deflection of the weft thread relative to the warp of the fabric. In the framework of this work, the reasons for the deviation of the weft thread relative to the warp of the fabric, which lead to the formation of defective zones on the prepreg, are considered. The angle of deflection of the weft thread was measured. The effect of weft thread deflection on the final elastic-strength properties of a polymer composite material has been studied.

Reference list
  1. Kablov E.N. Marketing of materials science, aircraft building and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5–6, pp. 40–44.
  2. Mikhailin Yu.A. Fibrous polymeric composite materials in engineering. St. Petersburg: Nauchnye osnovy i tekhnologii, 2013, 720 p.
  3. Vlasenko F.S., Raskutin A.E., Doneckij K.I. Application of braided preforms for polymer composite materials in civil industries (review). Trudy VIAM, 2015, no. 1, paper no. 05. Available at: http://www.viam-works.ru (accessed: April 27, 2022). DOI: 10.18577/2307-6046-2015-0-1-5-5.
  4. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  6. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  7. Basharov E.A., Vagin A.Yu. Analysis of the use of composite materials in the design of helicopter airframes. Trudy MAI, 2017, no. 92, pp. 1–13.
  8. Zorin V.A. Experience in the use of composite materials in products of aviation and rocket-space technology. Konstruktsii iz kompozitsionnykh materialov, 2011, no. 4, pp. 44–59.
  9. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  10. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 1. Automated Tape Laying (ATL). Aviation materials and technologies, 2021, no. 2 (63), paper no. 06. Available at: http://www.journal.viam.ru (accessed: June 19, 2022). DOI: 10.18577/2713-0193-2021-0-2-51-61.
  11. Malysheva G.V., Grashchenkov D.V., Guzeva T.A. Evaluation of technological use efficiency of adhesives and glue prepregs in the manufacture of three-layer panels. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 26–30. DOI: 10.18577/2071-9140-2018-0-4-26-30.
  12. Sarychev I.A., Serkova E.A., Khmelnitsky V.V., Zastroginа O.B. Thermosetting binders for aircraft floor panel materials (review). Trudy VIAM, 2019, no. 7 (79), paper no. 03. Available at: http://www.viam-works.ru (accessed: June 22, 2022). DOI: 10.18577/2307-6049-2019-0-7-26-33.
  13. Veshkin E.A., Postnov V.I., Strelnikov S.V., Abramov P.A., Satdinov R.A. Experience in the application of technological control of PCM semi-finished products. Izvestiya Samarskogo nauchnogo tsentra RAN, 2014, vol. 16, no. 6 (2), pp. 393–398.
  14. Composite materials handbook. US Department of Defense handbook, 2002. Vol. 3: Polymer matrix composites materials usage, design, and analysis. 734 p.
  15. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  16. Postnova M.V., Postnov V.I. Development experience out-of-autoclave methods of formation PCM. Trudy VIAM, 2014, no. 4, paper no. 06. Available at: http://www.viam-works.ru (accessed: April 08, 2022). DOI 10.18577/2307-6046-2014-0-4-6-6.
  17. Satdinov R.A., Istyagin S.E., Veshkin E.A. Analysis of the temperature-time parameters mode curing PCM with specified characteristics. Trudy VIAM, 2017, no. 3, paper no. 9. Available at: http://www.viam-works.ru (accessed: March 13, 2022). DOI: 10.18577/2307-6046-2017-0-3-9-9.
  18. Dushin M.I., Hrulkov A.V., Muhametov R.R. A choice of technological parameters of autoclave formation of details from polymeric composite materials. Aviacionnye materialy i tehnologii, 2011, no. 3, pp. 20–26.
  19. Kobelev S.A., Danilov G.I. Cutting blanks from polymer composite materials using various lubricating-cooling technological means. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2009, vol. 11, no. 3 (2), pp. 464–468.
  20. Tager A.A. Physico-chemistry of polymers. Moscow: Scientific world, 2007, 128 p.
  21. Savitsky R.S. Influence of mechanical processing of samples during cutting on the testing of composites. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2017, vol. 19, no. 4 (2), pp. 214–219.
  22. Boychuk A.S., Generalov A.S., Stepanov A.V. NDT monitoring of CFRP structural health by ultrasonic phased array technique. Aviacionnye materialy i tehnologii, 2015, no. 3 (36), pp. 84–89. DOI: 10.18577/2071-9140-2015-0-3-84-89.
  23. Murashov V.V., Trifonova S.I. Quality control of polymer composite materials using ultrasonic time-of-flight velocimetric technique. Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 86–90. DOI: 10.18577/2071-9140-2015-0-4-86-90.
  24. Boychuk A.S., Generalov A.S., Dikov I.A. FRP parts and structures testing by phased array technique. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 45–50. DOI: 10.18577/2071-9140-2017-0-1-45-50.
  25. Non-destructive testing: reference book. Ed. V.V. Klyuev. Moscow: Mashinostroenie, 2006, vol. 3: Ultrasonic testing. Ed. I.N. Ermolov, Yu.V. Lange, 864 p.
  26. Antyufeeva N.V., Stolyankov Yu.V., Iskhodzhanova I.V. Research and assessment of the properties of polymer composite materials according to methods harmonized with international standards. Konstruktsii iz kompozitsionnykh materialov, 2013, no. 3, pp. 41–45.