Calculation of the temperature dependence of the magnetization of sintered materials Pr–Dy–Fe–Co–B using molecular field approximation theory

Korolev D.V., Valeev R.A., Morgunov R.B., Piskorsky V.P.
Korolev D.V., Valeev R.A., Morgunov R.B., Piskorsky V.P. Calculation of the temperature dependence of the magnetization of sintered materials Pr–Dy–Fe–Co–B using molecular field approximation theory // Proceedings of VIAM. 2023. No. 2. DOI: 10.18577/2307-6046-2023-0-2-42-52. URL: https://www.viam-works.ru/en/journal/2023/2/4
Keywords
anisotropy field, magnetization, gyroscope, basic tetragonal phase, molecular field approximation, Brillouin function, rare earth ion, Curie temperature, squareness coefficient
Abstract

Provides a theoretical calculation of the magnetization of sintered materials Pr–Dy–Fe–Co–B and provides quantitative estimates of the dependence of magnetization on the concentration of dysprosium and cobalt. The optimal concentrations of these elements have been established, leading to the minimization of the temperature coefficient of induction. Experimental data on the dependence of magnetization on temperature are obtained. Experimental and theoretical dependences agree well with each other. This indicates the presence of predictive capabilities of the developed calculation model and allows us to hope for such a selection of concentrations of chemical elements that would make the magnetic properties of ring magnets in gyroscopes insensitive to temperature in the required operating range.

Reference list
  1. Topilskaya S.V., Borodulin D.S., Kornyukhin A.V. An experimental assessment of acceptable mechanical influences on a dynamically customizable gyroscope. Vestnik MGTU im. N.E. Baumana. Ser. Priborostroyenie, 2018, no. 4, pp. 69–79. DOI: 10.18698/0236-3933-2018-4-69-79.
  2. Fateev V.V., Nedezertsev V.P., Lyut M.N. Vibration sensor of angular velocity. Vestnik MGTU im. N.E. Baumana. Ser. Priborostroyenie, 1999, no. 1 (33), pp. 59–68.
  3. Kolosov Yu.A., Lyakhovetsky Yu.G., Rakhtenko E.R. Gyroscopic systems. Design of gyroscopic systems. Moscow: Higher School, 1977, 233 p.
  4. Dubinin A.V. Improving the resource of a gas-dynamic support of a small -sized dynamically customizable gyroscope for spacecraft: thesis, Cand. Sc. (Tech.). Moscow: Publishing House of Bauman MSTU, 2015, 118 p.
  5. Dynamically adjustable gyroscope: pat. 2248524 Rus. Federation; filed 29.04.04; publ. 20.03.05.
  6. Arzamasov B.N., Makarova V.I., Mukhin G.G. Materials Science. Moscow: Publishing House of Bauman MSTU, 2008, 648 p.
  7. Matveev V.A., Podchezertsev V.P., Fateev V.V. Gyroscopic stabilizers on dynamically customized vibrational gyroscopes. Moscow: Mashinostroenie, 1988, 263 p.
  8. Timoshenko S.P. Fluctuations in engineering. Moscow: Mashinostroenie, 1985, 472 p.
  9. Pelpor D.S., Matveev V.A., Arsenyev V.D. Dynamically customized gyroscopes. Theory and design. Moscow: Mashinostroenie, 1988, 263 p.
  10. Chirkin D.S., Roslovets P.V., Tatarinov F.V., Novikov L.Z. Reducing the drift of a dynamically customized gyroscope from launch to launch. Inzhenernyy zhurnal: nauka i innovatsii, 2017, no. 1. DOI: 10.18698/2308-6033-2017-1-1579.
  11. Morgunov R.B., Piskorskiy V.P., Valeev R.A., Korolev D.V. The thermal stability of rare-earth magnets supported by means of the magnetocaloric effect. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 88–94. DOI: 10.18577/2071-9140-2019-0-1-88-94.
  12. Piskorsky V.P., Valeev R.A., Korolev D.V., Morgunov R.B., Rezchikova I.I. Terbium and gadolinium dopin g influence on thermal stability and magnetic properties of sintered magnets Pr–Tb–Gd–Fe–Co–B. Trudy VIAM, 2019, no. 7 (79), paper no. 07. Available at: http://www.viam-works.ru (accessed: August 12, 2022). DOI: 10.18577/2307-6046-2019-0-7-59-66.
  13. Buzenkov A.V., Valeev R.A., Piskorsky V.P., Morgunov R.B. The effect of the content of yttrium on the properties of the sintered Magnets Nd–Dy–Y–Fe–Co–B. Trudy VIAM, 2022, no. 4 (110), paper no. 11. Available at: http://www.viam-works.ru (accessed: August 15, 2022). DOI: 10.18577/2307-6046-2022-0-4-108-117.
  14. Korolev D.V., Piskorskii V.P., Valeev R.A., Bakradze M.M., Dvoretskaya E.V., Koplak O.V., Morgunov R.B. Rare-earth RE–TM–B micromag-nets engineering (review). Aviation materials and technology, 2021, no. 1 (62), paper no. 05. Available at: http://www.journal.viam.ru (accessed: August 15, 2022). DOI: 10.18577/2713-0193-2021-0-1-44-60.
  15. Kablov E.N., Piskorsky V.P., Burkhanov G.S., Valeev R.A., Moiseeva N.S. et al. Thermostable ring magnets with a radial texture based on ND (PR)–DY–FE–CO–B. Fizika i khimiya obrabotki materialov, 2011, no. 3, pp. 43–47.
  16. Li H.-S., Zhang Z.-W., Dang M.-Z. Molecular field theory analysis of R2Fe14B intermetallic compounds. Journal of Magnetism and Magnetic Materials, 1988, vol. 71, pp. 355–358.
  17. Pedziwiatr A.T., Wallace W.E. Structure and magnetism of the R2Fe14–xCoxB ferromagnetic systems (R = Dy and Er). Journal of Magnetism and Magnetic Materials, 1987, vol. 66, pp. 61–68.
  18. Tenaud Ph., Lemaire H., Vial F. Recent improvements in NdFeB sintered magnets. Journal of Magnetism and Magnetic Materials, 1991, vol. 101, pp. 328–332.
  19. Radwanski R.J., Franse J.J. M. Rare-earth in the magnetocrystalline anisotropy energy in R2Fe14B. Journal of Physical Review B, 1987, vol. 36, no. 16, pp. 8616–8621.
  20. Petziwiatr A.T., Chen H.Y., Wallace W.E. Magnetism of Tb2Fe14–xCoxB system. Journal of Magnetism and Magnetic Materials, 1987, vol. 67, pp. 311–315.
  21. Marinescu M., McGinnis K., Liu J.F., Walmer M.H. High (BH)max permanent magnets with near-zero reversible temperature coefficient of BR. Proceedings of 20th International Workshop on Rare Earth Permanent Magnets and Their Applications. Crete, 2008, pp. 1–6.