Synthesis and study of the properties of yttrium oxide sols

Lebedeva Yu.E., Chaynikova A.S., Shchegoleva N.E., Belyachenkov I.O., Turchenko M.V.
Lebedeva Yu.E., Chaynikova A.S., Shchegoleva N.E., Belyachenkov I.O., Turchenko M.V. Synthesis and study of the properties of yttrium oxide sols // Proceedings of VIAM. 2023. No. 2. DOI: 10.18577/2307-6046-2023-0-2-32-41. URL: https://www.viam-works.ru/en/journal/2023/2/3
Keywords
yttrium oxide, sol, ceramic materials, sintering, sol-gel method, phase formation
Abstract

Sols of yttrium oxide with a Y2O3 content of 1, 5, and 10 wt. % have been synthesized. The structure and properties of sols have been studied: particle size and morphology, ζ-potential. According to the results of the study by photon correlation spectroscopy, the distribution of particle sizes in sols was determined: the average particle size was 49.3 nm for a sol with a Y2O3 content of 1 wt. %, 67 nm for a sol with a Y2O3 content of 5 wt. % and 232 nm for a sol with a Y2O3 content 10 wt. %. According to the results of XRD studies, the average size of crystallites of yttrium oxide nanopowder was 38.5 nm, which correlates with the results of the TEM study – 30–50 nm. The ζ-potential of the sols decreases with an increase in the concentration of yttrium oxide from –0.14 mV to –3.21 mV, however, it is quite small and indicates a low aggregative stability of the sols.

Reference list
  1. Kuzmina I.G., Svetlov I.L., Evseeva N.L. Obtaining a directed crystallization of large-sized high-rise forms and rods with nanostructural hardening for casting GTD blades from NB-composites. Spetsialnye sposoby litya, 2016, no. 10, pp. 17–21.
  2. Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Kochetkov A.S. Features of the manufacturing technology of highly refractory ceramic molds for castings from γ-TiAl alloys. Trudy VIAM, 2020, no. 2 (86), paper no. 04. Available at: http://www.viam-works.ru (accessed: August 8, 2022). DOI: 10.18577/2307-6046-2020-0-2-31-40.
  3. Strelnikova S.S. Features of sintering of mullite ceramics from ash-gel powders with the addition of ite oxide. Perspektivnye materialy, 2011. no. 11, pp. 336–341.
  4. Kan Y., Zhang G., Wang P. et al. Yb2O3 and Y2O3 co-doped zirconia ceramics. Journal European Ceramic Society, 2006, vol. 26, is. 16, pp. 3607–3612.
  5. Cosentino I.C., Muccillo R. Powder synthesis and sintering of high density thoria-yttria ceramics. Journal of Nuclear Materials. 2002, vol. 304, is. 2–3, pp. 129–133.
  6. Lemyshev D.O., Lukin E.S., Makarov N.A., Popova N.A. The prospects for creating new optically transparent materials based on ite oxide and Italiaalumine grenade. Steklo i keramika, 2008, no. 4, pp. 25–27.
  7. Bakovets V.V., Trushnikova L.N., Korolkov I.V. and other synthesis of nanostructured phosphor Y2O3–Eu–Bi gel method. Zhurnal obshchey khimii, 2013, vol. 83, is. 1, pp. 3–11.
  8. Puzyrev I.S., Ivanov MG, Krutikova I.V. The physico-chemical properties of Nanoporos AL2O3 and Y2O3, obtained by laser synthesis, and their water dispersions. Izvestiya Akademii nauk. Seriya khimicheskaya, 2014, no. 7, pp. 1504–1510.
  9. Lakhdara Y., Tucka C., Binnerc J. et al. Additive manufacturing of advanced ceramic materials. Progress in Materials Science, 2021, vol. 116, art. 10736.
  10. Alhaji A., Shoja Razavi R., Ghasemi A., Loghman-Estarki M.R. Modification of Pechini sol-gel process for the synthesis of MgO–Y2O3 composite nanopowder using sucrose-mediated technique. Ceramics International, 2017, vol. 43, pp. 2541–2548.
  11. Cheng X., Yuan C., Blackburn S., Withey P.A. The study of the influence of binder systems in an Y2O3–ZrO2 facecoat material on the investment casting slurries and shells properties. Journal of the European Ceramic Society, 2014, vol. 34, no. 12, pp. 3061–3068.
  12. Cui R., Zhang H., Tang X. et al. Gong Interactions between γ-TiAl melt and Y2O3 ceramic material during directional solidification process. Transactions of Nonferrous Metals Society of China, 2011, vol. 21, pp. 2415–2420.
  13. Neto R., Duarte T., Alves J.L., Torres F. Experimental characterization of ceramic shells for investment casting of reactive alloys. Ciência & Tecnologia dos Materiais, 2017, vol. 29, pp. 34–39.
  14. Belova I.A. Synthesis and colloid-chemical properties of hydroxoids of ite oxoxide: thesis abstract Cand. Sc (Chem.). Moscow, 2010, 17 p.
  15. Evdokimov S.A., Shchegoleva N.E., Sorokin O.Yu. Ceramic materials aviation engineering (review). Trudy VIAM, 2018, no. 12 (72), paper no. 06. Available at: http://www.viam-works.ru (accessed: August 21, 2022). DOI: 10.18577/2307-6046-2018-0-12-54-61.
  16. Wang L., Fan S., Sun H. et al. Pressure-less joining of SiCf/SiC composites by Y2O3–Al2O3–SiO2 glass: Microstructure and properties. Ceramic International, 2020, vol. 46, no. 17, pp. 27046–27056.
  17. Zhou L., Huang J., Cao L. et al. A novel design of oxidation protective β-Y2Si2O7 nanowire toughened Y2SiO5/Y2O3–Al2O3–SiO2 glass ceramic coating for SiC coated carbon/carbon composites. Corrosion Science, 2018, vol. 135, pp. 233–242.
  18. Courcot E., Rebillat F., Teyssandier F., Louchet-Pouillerie C. Thermochemical stability of the Y2O3–SiO2 system. Journal of the European Ceramic Society, 2010, vol. 30, pp. 905–910.
  19. Sokolov A.V., Deynega G.I., Kuzmina N.A. Influence of Sc2O3 additive on sintering tempera-ture and properties of ZrO2–Y2O3 system oxide ceramics. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 64–69. DOI: 10.18577/2071-9140-2020-0-1-64-69.
  20. Kablov E.N., Doronin O.N., Artemenko N.I., Stukhov P.A., Marakhovsky P.S., Stolyarova V.L. The study of the physicochemical properties of ceramics based on the SM2O3–Y2O3–HFO2 system for the development of heat-protective coatings. Zhurnal neorganicheskoy khimii, 2020, vol. 65, no. 6, pp. 846–855.
  21. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.