Metabolic possibilities of bacteria with respect to synthetic hydrocarbons used in the production of non-metallic materials (review)

Ermishev V.Yu.
Ermishev V.Yu. Metabolic possibilities of bacteria with respect to synthetic hydrocarbons used in the production of non-metallic materials (review) // Proceedings of VIAM. 2023. No. 2. DOI: 10.18577/2307-6046-2023-0-2-132-146. URL: https://www.viam-works.ru/en/journal/2023/2/11
Keywords
biodegradation, bacterial strains, enzymatic reactions, synthetic polymer materials, polyethylene terephthalate, polyvinyl alcohol, nylon
Abstract

Current trends in various industries are aimed at the use of structural elements, their coatings and binders of non-metallic materials. The molecular structure of this group of components is basically contains organic, organoelement, straight or branched carbon-containing polymers obtained by chemical synthesis from derivatives of petroleum products. The widespread use of such materials increases the total area of their contact with the external environment, which leads to the gradual destruction of both the material itself and all structural elements as a whole. The issues of biodegradation and metabolic assimilation of polyethylene terephthalate, polyvinyls and nylon oligomers are considered.

Reference list
  1. Krivushina A.A., Bobyreva T.V., Goryashnik Yu.S., Bukharev G.M. Study of microorganisms the destructors of functional polymeric materials exposed under conditions of tropical climate simulation. Trudy VIAM, 2019, no. 7 (79), paper no. 09. Available at: http://www.viam-works.ru (accessed: September 24, 2022). DOI: 10.18577/2307-60460-2019-0-7-76-83.
  2. Movenko D.A., Laptev A.B., Golubev A.V., Kireev D.M. The analysis of the material surface biodegradation in the petrochemical plant cooling water system. Trudy VIAM, 2019, no. 7 (79), paper no. 12. Available at: http://viam-works.ru (accessed: September 24, 2022). DOI: 10.18577/2307-6046-2019-0-7-112-124.
  3. Kablov E.N., Startsev V.O. Climatic aging of aviation polymer composite materials. II. Development of methods for studying the early stages of aging. Russian metallurgy (Metally), 2020, vol. 2020, no. 10, pp. 1088–1094. DOI: 10.1134/S0036029520100110.
  4. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of aviation composite materials. III. Significant factors of aging. Deformatsiya i razrusheniye materialov, 2011, no. 1, pp. 34–40.
  5. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  6. Staudinger H. Über Polymerisation. Berichte der Deutschen Chemischen Gesellschaft, 1920, no. 53, p. 1081.
  7. Jordansky A.L., Zaikov G.E., Berlin A.A. Diffusion kinetics and hydrolysis biodegradable polymers. Mass loss and control of the release of low molecular weight substances. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2015, vol. 18, no. 2, pp. 2–11.
  8. Laptev A.B., Golubev A.V., Kireev D.M., Nikolaev E.V. To the question of biodegradation of polymeric materials in natural environments (review). Trudy VIAM, 2019, no. 9 (81), paper no. 11. Available at: http://www.viam-works.ru (accessed: September 24, 2022). DOI: 10.18577/2307-6046-2019-0-9-100-107.
  9. Focht D.D. Biodegradation. AccessScience, 2020, vol. 27, pp. 57–72. DOI: 10.1036/1097-8542.422025.
  10. Lucas N., Bienaime C., Belloy C. et al. Polymer biodegradation: mechanisms and estimation techniques. Chemosphere, 2008, no. 4, p. 429. DOI: 10.1016/j.chemosphere.2008.06.064.
  11. Cappitelli F., Sorlini C. Microorganisms attack synthetic polymers in items Representing our cultural heritage. Applied and Environmental Microbiology, 2008, vol. 74, no. 3, pp. 564–569. DOI: 10.1128/AEM.01768-07.
  12. Eskander S., Saleh H. Biodegradation: Process Mechanism. Environmental Science and Engineering, 2017, vol. 8, no. 1, pp. 1–31.
  13. Startsev O.V., Meletov V.P., Perov B.V., Mashinskaya G.P. Study of the mechanism of aging of organotextolite in a subtropical climate. Mechanics of Composite Materials, 1986, no. 3, pp. 462–467.
  14. Startsev O.V., Krotov A., Mashinskaya G. Climatic Ageing of Organic Fiber Reinforced Plastics: Water Effect. Journal Polymeric Material, 1997, vol. 37, pp. 161–171.
  15. Startsev O.V. Structural Heterogeneity and Physical Properties of Climatic Aged Polymeriс Composite Materials. EUROMЕCH 350: Proc. Conf. Image Analysis, Porous Materials and Physical Properties, 1996, pp. 114–117.
  16. Frisch H.L. Diffusion in polymers. Journal of Applied Polymer Science, 1970, no. 14, pp. 1657.
  17. Kablov E.N., Startsev V.O., Inozemtsev A.A. The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  18. Chetna S., Madhuri S. Studies on biodegradation of polyethylene terephthalate: A synthetic polymer. Journal of Microbiology and Biotechnology Research, 2012, no. 2, pp. 248–257. Available at: https://www.researchgate.net/publication/306202944 (accessed: September 24, 2022).
  19. Sinha V., Patel M.R., Patel J.V. Pet Waste Management by Chemical Recycling: A Review. Journal of Polymers and the Environment, 2010, no. 18, pp. 8–25. DOI: 10.1007/s10924-008-0106-7.
  20. Sharon M., Sharon C. Studies on biodegradation of polyethylene terephthalate: a synthetic polymer. Journal Microbiology and Biotechnology Research, 2012, vol. 2, pp. 248–257. Available at: https://www.researchgate.net/publication/306202944 (accessed: September 24, 2022).
  21. Ghosh S., Pal S., Ray S. Study of microbes having potentiality for biodegradation of plastics. Environmental Science and Pollution Research, 2013, vol. 20, pp. 4339–4355. DOI: 10.1007/s11356-013-1706.
  22. Danso D., Schmeisser C., Chow J. et al. New insights into the function and global distribution of polyethylene terephthalate PET-degrading bacteria and enzymes in marine and terrestrial metagenomes. Applied and Environmental Microbiology, 2018, vol. 84, pp. 3–17. DOI: 10.1128/AEM.02773-17.
  23. Zheng Y., Yanful E.K., Bassi A.S. A Review of Plastic Waste Biodegradation. Critical Reviews in Biotechnology, 2005, vol. 25, pp. 243–250. DOI: 10.1080/07388550500346359.
  24. Yoshida S., Hiraga K., Takehana T. et al. A bacterium that degrades and assimilates poly(ethylene terephthalate). Science, 2016, vol. 353, pp. 759–759.
  25. Tourova T.P., Sokolova D.Sh., Nazina T.N. et al. Phylogenetic Diversity of Microbial Communities from the Surface of Polyethylene Terephthalate Materials Exposed to Different Water Environments. Microbiology, 2020, vol. 89, no. 1, pp. 96–106. DOI: 10.1134/S0026261720010154.
  26. Liu C., Shi C., Zhu S. et al. Structural and functional characterization of polyethylene terephthalate hydrolase from Ideonella sakaiensis. Biochemical and Biophysical Research Communications, 2019, vol. 508, pp. 289–294. DOI: 10.1016/j.bbrc.2018.11.148.
  27. Loh K., Chua S. Ortho pathway of benzoate degradation in Pseudomonas putida: induction of meta pathway at high substrate concentrations. Enzyme and Microbial Technology, 2002, vol. 30, pp. 620–626. DOI: 10.1016/S0141-0229(02)00016-9.
  28. Banerjee A., Ghoshal A. Phenol degradation by Bacillus cereus: Pathway and kinetic modeling. Bioresource Technology, 2010, vol. 101, pp. 5501–5507. DOI: 10.1016/j.biortech.2010.02.018.
  29. Grant D.J., Patel J.C. The non-oxidative decarboxylation of p-hydroxybenzoic acid, gentisic acid, protocatechuic acid and gallic acid by Klebsiella aerogenes (Aerobacter aerogenes). Antonie van Leeuwenhoek, 1969, no. 35, pp. 325–343. DOI: 10.1007/BF02219153.
  30. Mpofu E., Chakraborty J., Suzuki-Minakuchi C. et al. Biotransformation of Monocyclic Phenolic Compounds by Bacillus licheniformis TAB7. Microorganisms, 2019, vol. 8, pp. 1–12. DOI: 10.3390/microorganisms8010026.
  31. Wilkes R.A., Aristilde L. Degradation and metabolism of synthetic plastics and associated products by Pseudomonas sp.: capabilities and challenges. Journal of Applied Microbiology, 2017, vol. 123, pp. 582–593. DOI: 10.1111/jam.13472.
  32. Revitt D.M., Worrall P. Low temperature biodegradation of airport deicing fluids. Water Science and Technology, 2003, vol. 48, no. 9, pp. 103–111.
  33. Narancic T., Kevin E. Plastic waste as a global challenge: are biodegradable plastics the answer to the plastic waste problem. Microbiology, 2019, vol. 165, рр. 129–137. DOI: 10.1099/mic.0.000749.
  34. Kricheldorf H.R., Nuyken O., Swift G. Handbook of polymer synthesis. Second edition. CRC Press, 2004, pp. 97–124.
  35. Premraj R., Mukesh D. Biodegradation of polymers. Indian Journal of Biotechnology, 2005, vol. 4, pp. 186–193.
  36. Hu X., Mamoto R., Shimomura Y. et al. Cell surface structure enhancing uptake of polyvinyl alcohol (PVA) is induced by PVA in the PVA-utilizing Sphingopyxis sp.strain 113P3. Archives of Microbiology, 2007, no. 188, pp. 235–241. DOI: 10.1007/s00203-007-0239-4.
  37. Kim M., Yoon M. Isolation of strains degrading poly(Vinyl alcohol) at high temperatures and their biodegradation ability. Polymer Degradation and Stability, 2010, no. 95, pp. 89–93. DOI: 10.1016/j.polymdegradstab.2009.09.014.
  38. Hatanaka T., Kawahara T., Asahi N., Tsuji M. Effects of the structure of poly(vinylalcohol) on the dehydrogenation reaction by poly(vinyl alcohol) dehydrogenase from Pseudomonas sp. 113P3. Bioscience, Biotechnology and Biochemistry, 1995, no. 59, pp. 1229–1231.
  39. Matsumura S., Tomizawa N., Toki A. et al. Novel Poly(vinyl alcohol)-Degrading Enzyme and the Degradation Mechanism. Macromolecules, 1999, vol. 32, no. 23, pp. 7753–7761. DOI: 10.1021/ma990727b.
  40. Klomklang W., Tani A., Kimbara K. et al. Biochemical and molecular characterization of a periplasmic hydrolase for oxidized polyvinyl alcohol from Sphingomonas sp. strain 113P3. Microbiology, 2005, vol. 151, pp. 1255–1262. DOI: 10.1099/mic.0.27655-0.
  41. Shimao M., Onishi S., Kato N., Sakazawa C. Pyrroloquinoline Quinone-Dependent Cytochrome Reduction in Polyvinyl Alcohol-Degrading Pseudomonas sp. Strain VM15C. Applied and Environmental Microbiology, 1989, vol. 55, no. 2, pp. 275–278. DOI: 10.1128/aem.55.2.275-278.1989.
  42. Hu X., Kawai F. Biochemistry of microbial polyvinyl alcohol degradation. Applied and Environmental Microbiology, 2009, vol. 84, pp. 227–237.
  43. Welgos R.J. Polyamides, Plastics. 2nd ed. Allied Chemical Corporation in EPSE, 1975, vol. 11, рр. 445–476.
  44. Kolosova A.S., Sokolskaya M.K., Vitkalova I.A., Torlova A.S., Pikalov E.S. Modern polymer composite materials and their application. Mezhdunarodnyy zhurnal prikladnykh i fundamentalnykh issledovaniy, 2018, no. 5, part 1, pp. 245–256.
  45. Palmer R.J. Polyamides, Plastics. Encyclopedia of Polymer Science and Technology, 2002, no. 3, p. 251. DOI: 10.1002/0471440264.pst251.
  46. Iizuka H., Tanabe I., Fukumura T., Kato K. Taxonomic study on the ε-caprolactam-utilizing bacteria. Journal of General Microbiology, 1967, no. 13, pp. 125–137.
  47. Вoronin A.M., Grishchenkov V.G., Kulakov L.A., Naumova R.P. Characteristics of plasmid pBS271 controlling epsilon-caprolactam degradation by bacteria in the genus Pseudomonas. Mikrobiologiya, 1986, no. 55 (2), p. 231.
  48. Friedrich J., Zalar P., Mohorcic M. et al. Ability of fungi to degrade synthetic polymer nylon-6. Chemosphere, 2007, no. 67, pp. 2089–2095. DOI: 10.1016/j.chemosphere.2006.09.038.
  49. Kakudo S., Negoro S., Urabe I., Okada H. Nylon Oligomer Degradation Gene, nylC, on Plasmid pOAD2 from a Flavobacterium Strain Encodes Endo-Type 6-Aminohexanoate Oligomer Hydrolase: Purification and Characterization of the nylC Gene Product. Applied and environmental microbiology, 1993, vol. 59, no. 11, pp. 3978–3980. DOI: 10.1128/aem.59.11.3978-3980.1993.
  50. Okada H., Negoro S., Kimura H., Nakamura S. Evolutionary adaptation of plasmid-encoded enzymes for degrading nylon oligomers. Nature, 1983, no. 306 (5939), pp. 203–206. DOI: 10.1038/306203a0.
  51. Baxi N., Shah A. Biological treatment of the components of solid oligomeric waste from a nylon-6 production plant. World Journal of Microbiology and Biotechnology, 2000, no. 16, pp. 835–840. DOI: 10.1023/A:1008971216941.
  52. Negoro S. Biodegradation of nylon Oligomers. Applied Microbiology and Biotechnology, 2000, no. 54, pp. 461–466. DOI: 10.1007/s002530000434.
  53. Parke D., Garcia M.A., Ornston L.N. Cloning and Genetic Characterization of dca Genes Required for Oxidation of Straight-Chain Dicarboxylic Acids in Acinetobacter sp. Strain ADP1. Applied and Environmental Microbiology, 2001, vol. 67, no. 10. DOI: 10.1128/AEM.67.10.4817-4827.2001.
  54. Takehara I., Fujii T., Tanimoto Y. et al. Metabolic pathway of 6-aminohexanoate in the nylon oligomer-degrading bacterium Arthrobacter sp. KI72: identification of the enzymes responsible for the conversion of 6-aminohexanoate to adipate. Applied Microbiology and Biotechnology, 2018, no. 102, vol. 2, pp. 801–814. DOI: 10.1007/s00253-017-8657-y.