Ceramics based on organosilicon polymers-precursors: properties and applications (review)

Shestakov A.M.
Shestakov A.M. Ceramics based on organosilicon polymers-precursors: properties and applications (review) // Proceedings of VIAM. 2023. No. 2. DOI: 10.18577/2307-6046-2023-0-2-113-131. URL: https://www.viam-works.ru/en/journal/2023/2/10
Keywords
silicon carbonitride, ceramics, organosilicon polymers, mechanical properties, microstructure, silicon oxycarbide, pyrolysis, application, chemical properties
Abstract

. Considers the chemical, physical and mechanical properties of polymer-derived ceramics obtained on the basis of organosilicon polymers. High resistance of ceramics to oxidation, creep, crystallization and phase separation up to temperatures above 1500 °C, high chemical resistance in harsh environments are noted. The unique set of properties of ceramics provides it with a wide range of applications, including in the composition of ceramic matrix composites (fibers and matrices), in 3D printing, in protective coatings and microcomponents for electronics. Promising areas of application of ceramics and specific examples of its current use in various constructions are considered.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Composites: today and tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  3. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  4. Grashchenkov D.V., Evdokimov S.A., Zhestkov B.E., Solntsev S.St., Shtapov V.V. Research of thermochemical influence of the air plasma flow on high-temperature ceramic composite material. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 31–40. DOI: 10.18577/2071-9140-2017-0-2-31-40.
  5. Kablov E.N., Nikiforov A.A., Demin S.A., Chesnokov D.V., Vinogradov S.S. Promising coatings for corrosion protection of carbon steels. Stal, 2016, no. 6, pp. 70–81.
  6. Grashchenkov D.V., Efimochkin I.Yu., Bolshakova A.N. High-temperature metal-matrix composite materials reinforced with particles and fibers of refractory compounds. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 318–328. DOI: 10.18577/2071-9140-2017-0-S-318-328.
  7. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S., Sevastyanov V.G. High-Temperature Structural Composite Materials Based on Glass and Ceramics for Advanced Aircraft Products. Steklo i keramika, 2012, no. 4, pp. 7–11.
  8. Sorokin O.Yu., Grashhenkov D.V., Solntsev S.St., Evdokimov S.A. Ceramic composite materials with high oxidation resistance for the novel aircrafts (review). Trudy VIAM, 2014, no. 6, paper no. 8. Available at: http://www.viam-works.ru (accessed: June 21, 2022). DOI: 10.18577/2307-6046-2014-0-6-8-8.
  9. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.St. Promising high-temperature ceramic composite materials. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, vol. 1, pp. 20–24.
  10. Sorokin O.Yu. On the issue of the mechanism of interaction between carbon materials and Si melt (review). Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 65–70. DOI: 10.18577/2071-9140-2015-0-1-65-70.
  11. Shestakov A.M. Ceramics based on organosilicon polymers-precursors: methods of preparation and properties (review). Trudy VIAM, 2020, no. 11 (93), paper no. 9. Available at: http://www.viam-works.ru (accessed: accessed: June 21, 2022). DOI: 10.18577/2307-6046-2020-0-11-76-92.
  12. Shestakov A.M. Ceramics based on organosilicon polymers-precursors: microstructure and properties (review). Part 1. Trudy VIAM, 2021, no. 8 (102), paper no. 03. Available at: http://www.viam-works.ru (accessed: June 21, 2022). DOI: 10.18577/2307-6046-2021-0-8-21-33.
  13. Shestakov A.M. Ceramics based on organosilicon polymers-precursors: microstructure and properties (review). Part 1. Trudy VIAM, 2021, no. 9 (103), paper no. 03. Available at: http://www.viam-works.ru (accessed: June 21, 2022). DOI: 10.18577/2307-6046-2021-0-9-22-32.
  14. Chollon G. Oxidation Behaviour of Polymer-Derived Ceramics. Polymer Derived Ceramics: From Nanostructure to Applications. Eds. P. Colombo, R. Riedel, G.D. Sorarù, H.-J. Kleebe. Lancaster: DEStech Publications Inc., 2010, pp. 292–307.
  15. Modena S., Sorarù G.D., Blum Y., Raj R. Passive Oxidation of an Effluent System: The Case of Polymer-Derived SiCO. Journal of the American Ceramic Society, 2005, vol. 88, pp. 339–345.
  16. Morcos R.M., Navrotsky A., Varga T. et al. Thermodynamically Stable SiwCxNyOz Polymer-Like, Amorphous Ceramics Made from Organic Precursors. Journal of the American Ceramic Society, 2008, vol. 91, pp. 2391–2393.
  17. Varga T., Navrotsky A., Moats J.L. et al. Thermodynamically Stable SixOyCz Polymer-Like Amorphous Ceramics. Journal of the American Ceramic Society, 2007, vol. 90, pp. 3213–3219.
  18. Colombo P., Mera G., Riedel R., Soraru G.D. Polymer-Derived Ceramics: 40 Years of Research and Innovation in Advanced Ceramics. Journal of the American Ceramic Society, 2010, vol. 93, pp. 1805–1837.
  19. Butchereit E., Nickel K.G., Muller A. Precursor-Derived Si–B–C–N Ceramics: Oxidation Kinetics. Journal of the American Ceramic Society, 2001, vol. 84, pp. 2184–2188.
  20. Saha A., Shah S.R., Raj R. Oxidation Behavior of SiCN–ZrO2 Fiber Prepared from Alkoxide-Modified Silazane. Journal of the American Ceramic Society, 2004, vol. 87, pp. 1556–1558.
  21. Sorarù G.D., Modena S., Guadagnino E. et al. Chemical Durability of Silicon Oxycarbide Glasses. Journal of the American Ceramic Society, 2002, vol. 85, pp. 1529–1536.
  22. Pena-Alonso R., Mariotto G., Gervais C. et al. New Insights on the High-Temperature Nanostructure Evolution of SiCO and B-Doped SiBOC Polymer-Derived Glasses. Chemistry of Materials, 2007, vol. 19, pp. 5694–5702.
  23. Yajima S., Hayashi J., Omori M., Okamura K. Development of a Silicon Carbide Fiber with High Tensile Strength. Nature, 1976, vol. 261, pp. 683–685.
  24. Hasegawa Y., Iimura M., Yajima S. Synthesis of Continuous Silicon Carbide Fibre. Part. 2. Conversion of Polycarbosilane Fibre into Silicon Carbide Fibres. Journal of Materials Science, 1980, vol. 15, pp. 720–728.
  25. Yajima S., Iwai T., Yamamura T. et al. Synthesis of a Polytitanocarbosilane and its Conversion into Inorganic Compounds. Journal of Materials Science, 1981, vol. 16, pp. 1349–1355.
  26. Ishikawa T., Kohtoku Y., Kumagawa K. et al. High-Strength, Alkali-Resistant Sintered SiC Fibre Stable up to 2200 °C. Nature, 1998, vol. 391, pp. 773–775.
  27. Bunsell A.R., Piant A. A Review of the Development of Three Generations of Small Diameter Silicon Carbide Fibres. Journal of Materials Science, 2006, vol. 41, pp. 823–839.
  28. Shestakov A.M., Khaskov M.A., Sorokin O.Yu. Organosilicon polymer compounds based inorganic fibers for high-temperature composite materials (review). Trudy VIAM, 2019, no. 1 (73), paper no. 09. Available at: http://viam-works.ru (accessed: June 21, 202). DOI: 10.18577/2307-6046-2019-0-1-74-91.
  29. Bernard S., Weinmann M., Gerstel P. et al. Boron-Modified Polysilazane as a Novel Single-Source Precursor for SiBCN Ceramic Fibers: Synthesis, Melt-Spinning, Curing and Ceramic Conversion. Journal of Materials Chemistry, 2005, vol. 15, pp. 289–299.
  30. Sorarù G.D., Mercadini M., Dal Maschio R. et al. Si–Al–O–N Fibers from Polymeric Precursor: Synthesis, Structural, and Mechanical Characterization. Journal of the American Ceramic Society, 1993, vol. 76, pp. 2595–2600.
  31. Sorarù G.D., Dallapiccola E., D’Andrea G. Mechanical Characterization of Sol-Gel-Derived Silicon Oxycarbide Glasses. Journal of the American Ceramic Society, 1996, vol. 79, pp. 2074–2080.
  32. Renlund G.M., Prochazka S., Doremus R.H. Silicon Oxycarbide Glasses: Part II. Structure and Properties. Journal of Materials Research, 1991, vol. 6, pp. 2723–2734.
  33. Nishimura T., Haug R., Bill J., Thurn G., Aldinger F. Mechanical and Thermal Properties of Si–C–N Material from Polyvinylsilazane. Journal of Materials Science, 1998, vol. 33, pp. 5237–5241.
  34. Janakiraman N., Aldinger F. Fabrication and Characterization of Fully Dense Si–C–N Ceramics from a Poly(ureamethylvinyl)Silazane Precursor. Journal of the European Ceramic Society, 2009, vol. 29, pp. 163–173.
  35. Shah S.R., Raj R. Mechanical Properties of a Fully Dense Polymer Derived Ceramic Made by a Novel Pressure Casting Process. Acta Materialia, 2002, vol. 50, pp. 4093–4103.
  36. Walter S., Sorarù G.D., Brequel H., Enzo S. Microstructural and Mechanical Characterization of Sol-Gel-Derived SiOC Glasses. Journal of the European Ceramic Society, 2002, vol. 22, pp. 2389–2400.
  37. Kroll P. Modelling and Simulation of Amorphous Silicon Oxycarbide. Journal of Materials Chemistry, 2003, vol. 13, pp. 1657–1668.
  38. Rouxel T. Elastic Properties and Short-to Medium-Range Order in Glasses. Journal of the American Ceramic Society, 2007, vol. 90, pp. 3019–3039.
  39. Moysan C., Riedel R., Harshe R. et al. Mechanical Characterization of a Polysiloxane-Derived SiOC Glass. Journal of the European Ceramic Society, 2007, vol. 27, pp. 397–403.
  40. Moraes K.V., Interrante L.V. Processing, Fracture Toughness, and Vickers Hardness of Allylhydridopolycarbosilane-Derived Silicon Carbide. Journal of the American Ceramic Society, 2003, vol. 86, pp. 342–346.
  41. Bauer A., Christ M., Zimmermann A., Aldinger F. Fracture Toughness of Amorphous Precursor-Derived Ceramics in the Silicon–Carbon–Nitrogen System. Journal of the American Ceramic Society, 2001, vol. 84, pp. 2203–2207.
  42. Bernard S., Weinmann M., Cornu D. et al. Preparation of High-Temperature Stable Si–B–C–N Fibers from Tailored Single Source Polyborosilazanes. Journal of the European Ceramic Society, 2005, vol. 25, pp. 251–256.
  43. Cornu D., Bernard S., Duperrier S. et al. Alkylaminoborazine-Based Precursors for the Preparation of Boron Nitride Fibers by the Polymer-Derived Ceramics (PDCs) Route. Journal of the European Ceramic Society, 2005, vol. 25, pp. 111–121.
  44. Kokott S., Heymann L., Motz G. Rheology and Processability of Multi-Walled Carbon Nanotubes-ABSE Polycarbosilazane Composites. Journal of the European Ceramic Society, 2008, vol. 28, pp. 1015–1021.
  45. Ishikawa T. Photocatalytic Fiber with Gradient Surface Structure Produced from a Polycarbosilane and its Applications. International Journal of Applied Ceramic Technology, 2004, vol. 1, pp. 49–55.
  46. Shestakov A.M., Minakov V.T., Shvets N.I. et al. Ceramic-forming polymeric precursors based on polycarbosilane and diallylbisphenol A. Zhurnal prikladnoy khimii, 2014, vol. 87, no. 11, pp. 1626–1635.
  47. Minakov V.T., Shvets N.I., Zaitsev B.A. et al. Study of the influence of Rolivsan on the process of obtaining a ceramic matrix from a polycarbosilane precursor. Zhurnal prikladnoy khimii, 2016, vol. 89, no. 2, pp. 161–167.
  48. Shestakov A.M., Shvets N.I., Rozenenkova V.A., Khaskov M.A. Ceramic-forming compositions based on polycarbosilane and modified polyorganosilazanes. Zhurnal prikladnoy khimii, 2017, vol. 90, no. 8, pp. 1066–1073.
  49. Vorobyov A.G., Borovik I.N., Kazennov I.S. et al. Development of liquid-propellant low-thrust rocket engines with a combustion chamber made of carbon-ceramic composite material. Vestnik MAI, 2010, vol. 17, no. 3, pp. 135–142.
  50. Sherwood W.J. Composite Fabrication and CMCs. Polymer Derived Ceramics: From Nanostructure to Applications. Eds. P. Colombo, R. Riedel, G.D. Sorarù, H.-J. Kleebe. Lancaster: DEStech Publications Inc., 2010, pp. 326–340.
  51. Yeon S.-H., Reddington P., Gogotsi Y. et al. Carbide-Derived-Carbons with Hierarchical Porosity from a Preceramic Polymer. Carbon, 2010, vol. 48, pp. 201–210.
  52. Pivin J.C., Sendova-Vassileva M., Colombo P., Martucci A. Photoluminescence of Composite Ceramics Derived from Polysiloxanes and Polycarbosilanes by Ion Irradiation. Materials Science and Engineering: B, 2000, vol. 69–70, pp. 574–577.
  53. Khaskov M.A., Shestakov A.M., Sorokin O.Yu. et al. The formation of Si–C–N interfacial coating on carbon fibers. Materials Today: Proceedings, 2018, vol. 5, pp. 26046–26051.
  54. Gadow R., Kern F. Liquid-Phase Coating of Carbion Fibers with Pre-Ceramic Polymer Precursors: Process and Applications. Advanced Engineering Materials, 2002, vol. 4, pp. 883–886.
  55. Lim T.W., Son Y., Yang D.-Y. et al. Net Shape Manufacturing of Three-Dimensional SiCN Ceramic Microstructures Using an Isotropic Shrinkage Method by Introducing Shrinkage Guiders. International Journal of Applied Ceramic Technology, 2008, vol. 5, pp. 258–264.
  56. Eckel Z.C., Zhou C., Martin J.H. et al. Additive manufacturing of polymer-derived ceramics. Science, 2016, vol. 351, pp. 58–62.
  57. Li S., Duan W.Y., Zhao T. et al. The fabrication of SiBCN ceramic components from preceramic polymers by digital light processing (DLP) 3D printing technology. Journal of the European Ceramic Society, 2018, vol. 38, pp. 4597–4603.
  58. Zocca A., Gomes C.M., Staude A. et al. SiOC ceramics with ordered porosity by 3D-printing of a preceramic polymer. Journal of Materials Research, 2013, vol. 28, pp. 2243–2252.
  59. Chen H., Wang X., Xue F. et al. 3D printing of SiC ceramic: Direct ink writing with a solution of preceramic polymers. Journal of the European Ceramic Society, 2018, vol. 38, pp. 5294–5300.
  60. Pierin G., Grotta C., Colombo P., Mattevi C. Direct Ink Writing of micrometric SiOC ceramic structures using a preceramic polymer. Journal of the European Ceramic Society, 2016, vol. 36, pp. 1589–1594.
  61. Fu Sh., Zhu M., Zhu Y. Organosilicon polymer-derived ceramics: An overview. Journal of Advanced Ceramics, 2019, vol. 8, pp. 457–478.
  62. Liebau-Kunzmann V., Fasel C., Kolb R., Riedel R. Lithium Containing Silazanes as Precursors for SiCN: Li Ceramics – A Potential Material for Electrochemical Applications. Journal of the European Ceramic Society, 2006, vol. 26, pp. 3897–3901.
  63. Ferrari S., Orlandi M., Turani S. et al. Use of Polysiloxane Resins in Friction Materials. Advances in Applied Ceramics, 2009, vol. 108, pp. 461–467.
  64. Ceramic Electric Resistor: pat. 5961888 US; filed 10.08.98; publ. 05.10.99.
  65. Riedel R., Toma L., Janssen E. Piezoresistive Effect in SiOC Ceramics for Integrated Pressure Sensors. Journal of the American Ceramic Society, 2010, vol. 93, pp. 920–924.