Tensile testing of composite materials samples

Erasov V.S., Sibayev I.G., Sutubalov A.I.
Erasov V.S., Sibayev I.G., Sutubalov A.I. Tensile testing of composite materials samples // Proceedings of VIAM. 2023. No. 12. DOI: 10.18577/2307-6046-2023-0-12-98-114. URL: https://www.viam-works.ru/en/journal/2023/12/9
Keywords
stretching, sample, deformation, stress, fracture, survivability
Abstract

Methodological and material science problems arising during mechanical tensile tests of samples made of composite materials are considered. An overview of the methods of tensile testing of polymer composite materials (PCM) is given. The characteristics of the material determined during the tensile test are considered, including the main one – the deformation diagram under the «rigid» loading mode. A unified sample for testing PCM with various reinforcement schemes and new more functional designations of types of destruction are proposed.

Reference list
  1. Tarnopolsky Yu.M., Kintsis T.Ya. Methods of static testing of reinforced plastics. 3rd ed., rev. and add. Moscow: Khimiya, 1981, 272 p.
  2. ASTM D4762-18. Standard Guide for Testing Polymer Matrix Composite Materials. American Society for Testing and Materials, 2018, 25 p.
  3. ASTM D3039/D3039M-17. Standard Test Methods for Tensile Properties of Polymer Matrix Composite Materials. American Society for Testing and Materials, 2017, 13 p.
  4. State Standard R 56785–2015. Polymer composites. Tensile test method for flat samples. Moscow: Standartinform, 2015, 20 p.
  5. State Standard 32656–2017. Polymer composites. Test methods. Tensile tests. Moscow: Standartinform, 2017, 32 p.
  6. State Standard 25.601–80. Calculations and strength tests. Methods of mechanical testing of composite materials with a polymer matrix (composites). Method of tensile testing of flat samples at normal, elevated and low temperatures. Moscow: Standards Publishing House, 1980, 15 p.
  7. ISO 527-4:2021. Plastics – Determination of tensile properties – Part 5: Test conditions for unidirectional fibre-reinforced plastic composites, 2021, 27 p.
  8. EN 2561:1995. Aerospace series – Carbon fibre reinforced plastics – Unidirectional laminates – Tensile test parallel to the fibre direction. CEN, 1995, 14 p.
  9. EN 2597:1998. Aerospace series – Carbon fibre reinforced plastics – Unidirectional laminates – Tensile test perpendicular to the fibre direction. CEN, 1998, 16 p.
  10. State Standard 32658–2014. Polymer composites. Determination of mechanical characteristics during shear in the plane of reinforcement by tensile testing at an angle of ±45 degrees. Moscow: Standartinform, 2014, 15 p.
  11. ASTM D5766/D5766M-11. Standard Test Method for Open-Hole Tensile Strength of Polymer Matrix Composite Laminates. American Society for Testing and Materials, 2018. 7 p.
  12. ASTM D6742/D6742M-12. Standard Practice for Filled-Hole Tension and Compression Testing of Polymer Matrix Composite Laminates. American Society for Testing and Materials, 2012, 8 p.
  13. Vildeman V.E., Tretyakov V.P. Testing of materials with construction of complete strain diagrams. Problemy mashinostroyeniya i nadezhnosti mashin, 2013, no. 2. pp. 93–98.
  14. Zabulonov D.Yu., Myktybekov B., Ukhov P.A. Comparison of domestic and foreign methods for testing polymer composite materials. Nauchnyye trudy (Vestnik MATI), 2009, no. 15 (87). pp. 287–292.
  15. Adamov A.A., Laptev M.Yu., Gorshkova E.G. Analysis of domestic and foreign regulatory framework for mechanical testing of polymer composite materials. Konstruktsii iz kompozitsionnykh materialov, 2012, no. 3. pp. 72–77.
  16. Ilyichev A.V., Raskutin A.E., Gulyaev I.N. Comparison of the geometric dimensions of PCM samples used in international ASTM standards and domestic GOST standards. Novosti materialovedeniya. Nauka i tekhnika, 2015, no. 4 (16), art. 05. Available at: http://www.materialsnews.ru (accessed: August 09, 2023).
  17. Ilyichev A.V. Comparison of GOST and ASTM standards for mechanical tensile testing of PCM. Comments on standards, specifications, certificates: supplement to journal «Vse materialy. Entsiklopedicheskiy spravochnik», 2015, no. 8, pp. 2–9.
  18. Evdokimov A.A., Gulyaev I.N., Zelenina I.V. Investigation of the physicomechanical properties and microstructure of volume-reinforced carbon fiber reinforced plastic. Trudy VIAM, 2019, no. 4 (76), paper no. 05. Available at: http://viam-works.ru (accessed: August 16, 2023). DOI: 10.18577/2307-6046-2019-0-4-38-47.
  19. Shershak P.V., Ryabovol D.Yu. Standards for dynamic mechanical testing of plastics and polymer composite materials. Aviatsionnaya promyshlennost, 2017, no. 4, pp. 48–52.
  20. Wildeman V.E., Sokolkin Yu.V., Tashkinov A.A. Mechanics of inelastic deformation and fracture of composite materials. Ed. Yu.V. Sokolkina. Moscow: Fizmatlit, 1997, 288 p.
  21. Principles of creating composite polymer materials. Moscow: Khimiya, 1990, 240 p.
  22. Pobedrya B.E. Mechanics of composite materials. Moscow: Moscow State Univ. Publ. House, 1984, 352 p.
  23. Composite materials: reference book. Ed. D.M. Karpinos. Kyiv: Naukova Dumka, 1985, 592 p.
  24. Vanin G.A. Micromechanics of composite materials. Kyiv: Naukova Dumka, 1985, 304 p.
  25. Gunyaev G.M. Structure and properties of polymer fiber composites. Moscow: Khimiya, 1981, 232 p.
  26. Vasiliev V.V., Protasov V.D., Bolotin V.V. Composite materials: reference book. Ed. V.V. Vasilyeva, Yu.M. Tarnopolsky. Moscow: Mashinostroyenie, 1990, 512 p.
  27. Vasiliev V.V. Mechanics of structures made of composite materials. Moscow: Mashinostroyenie, 1988, 270 p.
  28. Christensen R.M. Introduction to the mechanics of composites. Moscow: Mir, 1982, 336 p.
  29. Mechanics of composite materials. Ed. J. Sendecki. Moscow: Mir, 1978, 564 p.
  30. Jones R.M. Mechanics of Composite materials. 2nd ed. Taylor & Francis, 1999, 519 p.
  31. Woven structural composites. Moscow: Mir, 1990, 432 p.
  32. Tarnopolsky Yu.M., Zhigun I.G., Polyakov V.A. Spatially reinforced composite materials. Moscow: Mashinostroyenie, 1987, 224 p.
  33. Gorshkov A.G., Starovoitov E.I., Tarlakovsky D.V. Theory of elasticity and plasticity. Moscow: Fizmatlit, 2002, 416 p.
  34. Dimitrienko Yu.I. Fundamentals of solid mechanics. Moscow: Bauman MSTU Publ. house, 2013, vol. 4: Continuum mechanics, 624 p.
  35. Goldman A.Ya. Prediction of deformation-strength properties of polymer and composite materials. Leningrad: Khimiya, 1988, 272 p.
  36. Dimitrienko Yu.I., Kashkarov A.I. Calculation of the effective characteristics of composites with a periodic structure by the finite element method. Vestnik MGTU im. N.E. Baumana, ser.: Natural Sciences, 2002, no. 2, pp. 95–108.
  37. Monocrystal fibers and materials reinforced by them. Ed. A.T. Tumanov. Moscow: Mir, 1973, 464 p.
  38. ASTM E83-10. Practice for Verification and Classification of Extensometer Systems. American Society for Testing and Materials, 2010, 19 p.
  39. State Standard 12423–2013 (ISO 291:2008). Plastics. Conditioning conditions and testing of samples (specimen). Moscow: Standartinform, 2014, 11 p.
  40. Podzhivotov N.Yu., Kablov E.N., Antipov V.V., Erasov V.S., Serebrennikova N.Yu., Abdul-lin M.R., Limonin M.V. Layered metal-polymer materials in aircraft structural elements. Perspektivnye materialy, 2016, no. 10, pp. 5–19.
  41. Grinevich D.V., Yakovlev N.O., Slavin A.V. The criteria of the failure of polymer matrix composites (review). Trudy VIAM, 2019, no. 7 (79), paper no. 11. Available at: http://viam-works.ru (accessed: August 16, 2023). DOI: 10.18577/2307-6046-2019-0-7-92-111.
  42. Dimitrienko Yu.I., Gubareva E.A., Sborshchikov S.V., Erasov V.S., Yakovlev N.O. Numerical modeling and experimental study of the deformation of elastoplastic plates under compression. Matematicheskoe modelirovanie i chislennye metody, 2015, no. 1 (5), pp. 67–82.
  43. Yakovlev N.O., Erasov V.S., Petrova A.P. Comparison of regulatory frameworks in different countries for testing adhesive joints of materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2014, no. 7, pp. 2–8.
  44. Yakovlev N.O., Gulyaev A.I., Popkova E.A. Assessment of geometric parameters of carbon fibers. Mat. XIV All-Rus. conf. on testing and research into the properties of materials «Physical and mechanical tests, strength and reliability of modern structural and functional materials». Moscow: National Research Center «Kurchatov Institute» – VIAM, 2022, pp. 227–239.
  45. Erasov V.S., Yakovlev N.O., Nuzhnyj G.A. Qualification tests and researches of durability of aviation materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 440–448.
  46. Yakovlev N.O., Popkova E.A., Landik D.N. Deformation as a quality criterion for carbon fiber. Reports VII All-Rus. scientific-technical conf. “The role of fundamental research in the implementation of strategic directions for the development of materials and technologies for their processing for the period until 2030”. Moscow: VIAM, 2021, pp. 198–203.
  47. Slavin А.V., Silkin A.N., Grinevich D.V., Yakovlev N.O. Composite materials with a 3D-reinforced structure (review). Trudy VIAM, 2022, no. 8 (114), paper no. 09. Available at: http://www.viam-works.ru (accessed: August 16, 2023). DOI: 10.18577/2307-6046-2022-0-8-113-122.
  48. Kablov E.N. Quality control of materials is a guarantee of safe operation of aviation equipment. Aviacionnye materialy i tekhnologii, 2001, no. 1, pp. 3–8.
  49. Oreshko E.I., Erasov V.S., Yakovlev N.O., Utkin D.A. Methods for determining the mechanical characteristics of materials using indentation (review). Aviation materials and technology, 2021, no. 1 (62), paper no. 10. Available at: http://www.journal.viam.ru (accessed: August 16, 2023). DOI: 10.18577/2071-9140-2021-0-1-104-118.