Process research of wire-cut electrical discharge machining of polymeric composite materials

Donetskiy K.I., Ablyaz T.R., Plotnikov E.V., Shlykov E.S., Kamenskih A.A., Osinnikov I.V., Panteleev I.A., Mubassarova V.A.
Donetskiy K.I., Ablyaz T.R., Plotnikov E.V., Shlykov E.S., Kamenskih A.A., Osinnikov I.V., Panteleev I.A., Mubassarova V.A. Process research of wire-cut electrical discharge machining of polymeric composite materials // Proceedings of VIAM. 2023. No. 12. DOI: 10.18577/2307-6046-2023-0-12-74-86. URL: https://www.viam-works.ru/en/journal/2023/12/7
Keywords
polymer composite materials, carbon fiber polymer, wire-cut electrical discharge machining, interelectrode gap, tomographic scanning, factorial experiment
Abstract

The modern polymer composite materials of the new generation are capable of meeting increased requirements for elastic-strength characteristics and their operational stability, which are necessary to ensure the operability of structures. Blade processing this materials is associated with a number of technological difficulties. An urgent task is the development of technology for wire-cut electrical discharge machining of polymer composite materials. A full factorial experiment was conducted. A theoretical model has been obtained that allows one to calculate the tool correction value when writing a control program for processing a part. A study of the 3D structure of the carbon composite material VKU-29 was carried out. It is shown that the structure of the composite is homogeneous.

Reference list
  1. Application of polymer composite materials in the production and repair of machines: textbook. Moscow: MADI, 2016, 264 p.
  2. Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, рр. 225–228.
  3. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), p. 3.
  4. Hsissou R., Benhiba F., Echihi S. et al. New epoxy composite polymers as a potential anticorrosive coatings for carbon steel in 3,5 % NaCl solution: Experimental and computational approaches. Chemical Data Collections, 2021, vol. 31, art. 100619. DOI: 10.1016/j.cdc.2020.100619.
  5. Hsissou R., Bekhta A., Dagdag O. et al. Rheological properties of composite polymers and hybrid nanocomposites. Heliyon, 2020, vol. 6, is. 6, art. e04187. DOI: 10.1016/j.heliyon.2020.e04187.
  6. Kablov E.N. The role of fundamental research in the creation of new generation materials. Report XXI Mendeleev Congress on General and Applied Chemistry: in 6 vol. St. Petersburg, 2019, vol. 4, p. 24.
  7. Slavin A.V., Donetskiy K.I., Khrulkov A.V. Prospects for the use of polymer composite materials in aircraft structures in 2025–2035 (review). Trudy VIAM, 2022, no. 11 (117), paper no. 08. Available at: http://www.viam-works.ru (accessed: September 26, 2023). DOI: 10.1877/2307-6046-2022-0-11-81-92.
  8. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://journal.viam.ru (accessed: September 01, 2023). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  9. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  10. Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  11. Dyshenko V.S., Donetskiy K.I., Minibaev M.I., Ablyaz T.R., Shlykov E.S., Shiryaev V.V. Methods of mechanical and electrical discharge machining of polymer composite materials (review). Trudy VIAM, 2018, no. 3 (109), paper no. 10. Available at: http://www.viam-works.ru (accessed: September 20, 2023). DOI: 10.18577/2307-6046-2022-0-3-102-120.
  12. Ablyaz T.R., Donetsky K.I., Shlykov E.S., Muratov K.R., Dyshenko V.S., Minibaev M.I. Complex analysis of methods for processing polymer composite materials. STIN, 2022, no. 6, pp. 5–8.
  13. Sidorina A.I. Multiaxial carbon fabrics in the products of aviation technology (review). Aviation materials and technologies, 2021, no. 3 (64), paper no. 10. Available at: http://www.journal.viam.ru (accessed: September 20, 2023). DOI: 10.18577/2713-0193-2021-0-3-105-116.
  14. Panner Selvam M., Ranjith Kumar P. Optimization Kerf Width and Surface Roughness in Wirecut Electrical Discharge Machining Using Brass Wire. Mechanics and Mechanical Engineering, 2017, vol. 21, no. 1, pp. 37–55.
  15. Maher I., Lingb L.H., Sarhan A.A.D. Improve wire EDM performance at different machining parameters – ANFIS modeling. IFAC-Papers OnLine, 2015, vol. 48-1, pp. 105–110. DOI: 10.1016/j.ifacol.2015.05.109.
  16. Mu-Tian Yan, Yi-Peng Lai. Surface quality improvement of wire-EDM using a fine-finish power supply. International Journal of Machine Tools and Manufacture, 2007, no. 47, pp. 1686–1694. DOI: 10.1016/j.ijmachtools.2007.01.006.
  17. Abbas N.M., Solomon D.G., Bahari Md.F. A review on current research trends in electrical discharge machining (EDM). International Journal of Machine Tools & Manufacture, 2007, no. 47, pp. 1214–1228. DOI: 10.1016/j.ijmachtools.2006.08.026.
  18. Shlykov E.S., Ablyaz T.R., Oglezneva S.A. Electrical Discharge Machining of Polymer Composites. Russian Engineering Research, 2020, vol. 40, no. 10, pp. 878–879.
  19. Ablyaz T.R., Muratov K.R., Shlykov E.S. et al. Electric-Discharge Machining of Polymer Composites. Russian Engineering Research, 2019, vol. 39, no. 10, p. 898900.
  20. Fukuzawa Y., Katougi H., Mohri N. et al. Machining properties of ceramics with an electric discharge machine. Proceedings of the XII ISEM, 1998, pp. 445–454.
  21. Mohri N., Fukuzawa Y., Tani T. et al. Assisting electrode method for machining insulating ceramics. Annals CIRP, 1996, no. 45 (1), pp. 201–204.
  22. Mohri N., Fukusima Y., Fukuzawa Y. et al. Layer generation process on work-piece in electrical discharge machining. Annals CIRP, 2003, no. 52 (1), pp. 161–164.
  23. Lauwers B., Kruth J.P., Liu W. et al. Investigation of Material Removal Mechanisms in EDM of Composite Ceramic Materials. Journal of Materials Processing Technology, 2004, no. 149, pp. 347–352.
  24. Puertas I., Luis C. A Study on the Electrical Discharge Machining of Conductive Ceramics. Journal of Materials Processing Technology, 2004, vol. 153–154/1–3, pp. 1033–1038.
  25. Kucukturk C., Çogun C. A New Method for Machining of Electrically Nonconductive Workpieces Using Electric Discharge. Machining Technique, Machining Science and Technology, 2010, vol. 14, pp. 189–207.
  26. Hosel T., Müller C., Reinecke H. Simple Techniques of Spark Erosive Structuring of Electrically Nonconductive Zirconia (ZrO2), 4M. 4M/ICOMM 2009. The Global Conference on Micro Manufacture, 2009.
  27. Wüthrich R., Fascio V. Machining of non-conducting materials using electrochemical discharge phenomenon – an overview. International Journal of Machine Tools and Manufacture, 2005, vol. 45, pp. 1095–1098.
  28. Schubert A., Zeidler H., Wolf N., Hackert M. Micro electro discharge machining of electrically nonconductive ceramics. AIP Conference Proceedings, 2011, pp. 1303–1308.
  29. Cnudde V., Boone M.N. High-resolution X-ray computed tomography in geosciences: A review of the current technology and applications. Earth-Science Reviews, 2013, vol. 123, pp. 1–17.
  30. Feldkamp L.A., Jesion G. 3-D X-ray computed tomography. Review Progress Quantitative Nondestructive Evalution, 1986, vol. 5a, pp. 555–566.
  31. Hanna R.D., Ketcham R.A. X-ray computed tomography of planetary materials: A primer and review of recent studies. Geochemistry, 2017, vol. 77, is. 4, pp. 547–572.
  32. Stock S.R., Sasov A., Liu X., Salmon P.L. Compensation of mechanical inaccuracies in micro-CT and nano-CT. Developments in X-ray Tomography VI. Washington, DC: SPIE, 2008. DOI: 10.1117/12.793212.