Research of the properties of epoxy compositions modified with polyarylsulphone and polymer composite materials based on them

Salakhova R.K., Veshkin E.A, Sudyin Yu.I., Tihobrazov A.B.
Salakhova R.K., Veshkin E.A, Sudyin Yu.I., Tihobrazov A.B. Research of the properties of epoxy compositions modified with polyarylsulphone and polymer composite materials based on them // Proceedings of VIAM. 2023. No. 12. DOI: 10.18577/2307-6046-2023-0-12-53-62. URL: https://www.viam-works.ru/en/journal/2023/12/5
Keywords
epoxy binder, polyarylsulfone PSFF-30, physical and mechanical properties, pore volume fraction, degree of curing, glass transition temperature, glass and carbon plastics
Abstract

The composition of an epoxy composition modified with polyarylsulfone PSFF-30 was proposed and the physicochemical and rheological properties of the resulting melt binder were studied. Based on an epoxy-polysulfone binder, glass and carbon fiber plastic samples were made using the vacuum furnace molding method, and the strength and thermophysical characteristics of the polymers were assessed. It has been established that this modification of the epoxy- polysulfone binder reduces the volume fraction of pores in fiberglass with woven filler T-10-14 by 2,7 times, and in carbon fiber with filler VTkU-2.200 – 2 times.

Reference list
  1. Kablov E.N. The sixth technological structure. Nauka i zhizn, 2010, no. 4, pp. 2–7.
  2. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  3. Kablov E.N. To the 80th anniversary of VIAM. Zavodskaya laboratoriya. Diagnostika materialov, 2012, vol. 78, no. 5, pp. 79–82.
  4. Salakhova R.K., Tikhoobrazov A.B., Smirnova T.B., Kirilin S.G. Nickel plating of carbon and fiberglass in order to increase the erosion resistance of PCM structures. Uprochnyayushchie tekhnologii i pokrytiya, 2021, vol. 17, no. 5 (197), pp. 221–227.
  5. Salakhova R.K., Tikhoobrazov A.B., Smirnova T.B., Kirilin S.G. Chemical-galvanic metallization of carbon and fiberglass. Galvanotekhnika i obrabotka poverkhnosti, 2020, vol. 28, no. 3, pp. 13–21.
  6. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  7. Vorobyov A. Epoxy resins. Komponenty i tekhnologii, 2003, no. 8. pp. 170–173.
  8. Petrova A.P., Mukhametov R.R. Binders for polymer composite materials based on epoxy oligomers. Klei. Germetiki. Tekhnologii, 2018, no. 7, pp. 21–27.
  9. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE «VIAM» in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  10. Sopotov R.I., Gorbunova I.Yu., Onuchin D.V. et al. The influence of polysulfone and polyethersulfone modifiers on the thermomechanical properties of an epoxyamine binder. Uspekhi v khimii i khimicheskoy tekhnologii, 2015, vol. 29, no. 10, pp. 62–64.
  11. Sergeeva E.A., Abdullin I.Sh., Zenitova L.A., Kostina K.D. Analysis of methods for modifying fibrous materials. Vestnik tekhnologicheskogo universiteta, 2015, vol. 18, no. 20, pp. 164–167.
  12. Kopitsyna M.N., Bessonov I.V., Kotomin S.V. Crack resistance of epoxy binders modified with thermoplastic polysulfone and furfural acetone resin. Inzhenernyy zhurnal: nauka i innovatsii, 2016, no. 12, pp. 1–9.
  13. Starostina I.V., Petrova A.P., Shevchenko Yu.N., Shishimirov M.V. Control thermoplastic binding for PCM (review). Trudy VIAM, 2019, no. 4 (76), paper no. 11. Available at: http://viam-works.ru (accessed: August 09, 2023). DOI: 10.18577/2307-6046-2019-0-4-99-107.
  14. Solodilov V.I., Korokhin R.A., Gorbatkina Yu.A., Kuperman A.M. Organoplastics based on complex hybrid matrices, including polysulfone and carbon nanotubes as epoxy resin modifiers. Khimicheskaya fizika, 2012¸ vol. 31, no. 6, pp. 63–71.
  15. Khasbulatova Z.S. Aromatic polysulfones. Plasticheskiye massy, 2009, no. 4, pp. 20–23.
  16. Shteiberg E.M., Sergeeva E.A., Zenitova L.A., Abdullin I.Sh. Application and production of polysulfone. Review. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2012, vol. 15, no. 20, pp. 168–171.
  17. Borodulin A.S. Plasticizers for epoxy adhesives and binders. Klei. Germetiki. Tekhnologii, 2012, no. 7, pp. 31–35.
  18. Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polymer composite materials on a thermoplastic matrix. Izvestiya vuzov. Khimiya i khimicheskaya tekhnologiya, 2016, vol. 59, is. 10, pp. 61–71.
  19. Gurenkov V.M., Gorshkov V.О., Chebotarev V.P., Prudskova Т.N., Andreeva Т.I. Comparative analysis of properties of polyetheretherketone of domestic and foreign production. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 41–47. DOI: 10.18577/2071-9140-2019-0-3-41-47.
  20. Kostromina N.V., Olikhova Yu.V., Malakhovsky S.S., Gorbunova I.Yu. Development of epoxy binders modified with heat-resistant thermoplastics for the creation of reinforced composite materials. Plasticheskiye massy, 2022, no. 9–10, pp. 17–19.
  21. Besednov K.L., Babin A.N., Grebeneva T.A., Tkachuk A.I., Pleshakov D.V. Study of the dissolution processes of polysulfones in epoxy resins. Uspekhi v khimii i khimicheskoy tekhnologii, 2016, vol. 30, no. 8, pp. 15–17.
  22. Zagora A.G., Tkachuk A.I., Terekhov I.V., Mukhametov R.R. Methods of chemical modification of epoxy oligomers (review). Trudy VIAM, 2021, no. 7 (101), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 23, 2023). DOI: 10.18577/2307-6046-2021-0-7-73-85.
  23. Mishkin S.I., Klimenko O.N., Kutcevich K.E. Determination of stickiness of prepregs on the basis of carbon fillers the sounding method. Trudy VIAM, 2018, no. 3 (109), paper no. 04. Available at: http://www.viam-works.ru (accessed: August 17, 2023). DOI: 10.18577/2307-6046-2022-0-3-35-43.
  24. Malysheva G.V., Akhmetova E.Sh., Marycheva A.N. Estimation of the glass transition temperature of epoxy binders modified with polysulfone. Fizika i khimiya stekla, 2014, vol. 40, no. 5, pp. 718–724.