Electrolyte-plasma polishing of parts made by selective laser sintering from metal powder composition of aluminum alloy grade VAS1
Part 1
UDC
669.018.95:621.791.724
DOI
10.18577/2307-6046-2023-0-12-19-27
Article PDF (Russian)
(674.57 KB)
How to cite
Dobrynin D.A., Pavlova T.V. Electrolyte-plasma polishing of parts made by selective laser sintering from metal powder composition of aluminum alloy grade VAS1. Part 1 // Proceedings of VIAM. 2023. No. 12. DOI: 10.18577/2307-6046-2023-0-12-19-27. URL: https://www.viam-works.ru/en/journal/2023/12/2
Keywords
electrolyte-plasma polishing, selective laser sintering, metal powder composition, aluminum alloy grade VAS1
Abstract
The article provides an overview of traditional surface polishing methods (mechanical, chemical and electrochemical), which are used for processing parts made by selective laser sintering from metal powder compositions. The main advantages and disadvantages of these methods are described. Taking into account the identified shortcomings, a more high-performance and environmentally friendly method of electrolyte-plasma surface polishing has been proposed. A number of works have been carried out aimed at developing an electrolyte composition for electrolyte-plasma polishing of parts made of metal powder composition aluminum alloy grade VAS1.
Reference list
- Kablov E.N., Evgenov A.G., Bakradze M.M., Nerush S.V., Krupnina O.A. New generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 1. Materials and synthesis technologies. Electrometallurgiya, 2022, no. 1, pp. 2–12. DOI: 10.31044/1684-5781-2022-0-1-2-12.
- Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S., Dynin N.V. New generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 3. Adaptation and creation of materials. Electrometallurgiya, 2022, no. 4, pp. 15–25. DOI: 10.31044/1684-5781-2022-0-4-15-25.
- Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S. New generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 4. Development of heat-resistant materials. Electrometallurgiya, 2022, no. 5, pp. 8–19. DOI: 10.31044/1684-5781-2022-0-5-8-19.
- Shchetinina N.D., Kuznetsova P.E., Dynin N.V., Selivanov A.A. Aluminum alloys with additions of Sc and Zr in additive manufacturing (review) Aviation materials and technologies, 2021, no. 3 (64), paper no. 03. Available at: http://www.journal.viam.ru (accessed: October 10, 2023). DOI: 10.18577/2713-0193-2021-0-3-19-34.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Peskova A.V., Sukhov D.I., Mazalov P.B. Examination of the formation of the titanium alloy VT6 structure obtained by additive manufacturing. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 38–44. DOI: 10.18577/2071-9140-2020-0-1-38-44.
- Nerush S.V., Sviridov A.V., Afansiev-Khodykin A.N., Galushka I.A., Tarasov S.A. Development of brazing technology for parts obtained by additive technologies from cobalt based metal powder composition. Aviation materials and technologies, 2022, no. 2 (67), paper no. 02. Available at: http://www.journal.viam.ru (accessed: October 10, 2023). DOI: 10.18577/2713-0193-2022-0-2-5-17.
- Marakhovskij P.S., Barinov D.Ya., Shorstov S.Yu., Vorobev N.N. On creation of physical and mathematical models of heat and mass transfer during manufacturing by additive technologies (review). Aviation materials and technologies, 2022, no. 2 (67), paper no. 10. Available at: http://www.journal.viam.ru (accessed: October 10, 2023). DOI: 10.18577/2713-0193-2022-0-2-111-119.
- Galvanic coatings in mechanical engineering: a reference book in 2 vol. Ed. M.A. Schluger. Moscow: Mashinostroenie, 1985, vol. 1, 240 p.
- Grilikhes S.Ya. Degreasing, etching and polishing of metals. Ed. P.M. Vyacheslavova. Ed. 5th, rev. and add. Leningrad: Mechanical Engineering, 1983, 101 p.
- Pogrebnyak A.D., Tyurin Yu.N., Boyko A.G., Zhadkevich M.L., Kalyshkanov M.K., Ruzimov Sh.M. Electrolyte-plasma processing and coating of metals and alloys. Uspekhi fiziki metallov, 2005, vol. 6, pp. 273–344.
- Volenko A.P., Boychenko O.V., Chirkunova N.V. Electrolyte-plasma processing of metal products. Vektor nauki TGU, 2012, no. 4 (22), pp. 144–147.
- Kulikov I.S., Vashchenko S.V., Kamenev A.Ya. Electrolytic-plasma processing of materials. Minsk: Belaruskaya Navuka, 2010, 232 p.
- Method of electrolyte-plasma processing of products made of aluminum and aluminum alloys: pat. 7291, Republic of Belarus; appl. 16.07.15; publ. 28.02.17.
- Zakharov S.V., Korotkikh M.T. Electrolytic-plasma polishing of complex-profile products made of aluminum alloy D16. Vestnik Kontserna VKO «Almaz–Antey», 2017, no. 3, pp. 83–87.