Mechanisms of creep in the temperature range 750−850 °С of nickel-based superalloy with zero γ/γ′-lattice misfit

Petrushin N.V., Zaysev D.V., Svetlov I.L., Karashaev M.M., Epishin A.I.
Petrushin N.V., Zaysev D.V., Svetlov I.L., Karashaev M.M., Epishin A.I. Mechanisms of creep in the temperature range 750−850 °С of nickel-based superalloy with zero γ/γ′-lattice misfit // Proceedings of VIAM. 2023. No. 12. DOI: 10.18577/2307-6046-2023-0-12-3-18. URL: https://www.viam-works.ru/en/journal/2023/12/1
Keywords
nickel-based superalloys, computer design, phase stability, creep, long-term creep strength, deformation-induced structural faults, microsegregation of alloying elements, creep mechanisms
Abstract

Using the powder-metallurgy nickel-based superalloy VZh178P as a prototype the chemical composition of an experimental gas turbine disk alloy with zero γ/γ'-misfit and high phase stability was calculated by the method of computer design. After equiaxed solidification and heat treatment the microstructure of alloy represents a γ-phase strengthened by spherical particles of the γ'-phase with a size of ~0,2 μm. After creep tests (750 °C, σ = 650 MPa, τ = 99 h and 850 °C, σ = 300 MPa, τ = 705 h), the microstructure studies and analysis of the creep mechanisms of the alloy were carried out. No traces of the formation of TPU phases were found in the alloy.

Reference list
  1. Kablov E.N. Materials and technologies of the VIAM for the «Aviator». Permskie aviatsionnye dvigateli, 2014, no. 31, pp. 43–47.
  2. Garibov G.S., Grits N.M., Vostrikov A.V., Fedorenko E.A. Development and study of a new granular high-strength heat-resistant nickel alloy VV752P for promising aircraft equipment. Tekhnologiya legkikh splavov, 2011, no. 1, pp. 7–11.
  3. Logunov A.V., Shmotin Yu.N., Khramin R.V. et al. The influence of alloying elements on the strength properties of heat -resistant nickel alloys for gas turbine disks. Electrometallurgiya, 2021, no. 3, pp. 2–13.
  4. Barba D., Alabort E., Pedrazzini S. et al. On the microtwinning mechanism in a single crystal superalloy. Acta Materialia, 2017, vol. 135, pp. 314‒329. DOI: 10.1016/j.actamat.2017.05.072.
  5. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), paper no. 03. Available at: http://www.journal.viam.ru (accessed: October 04, 2023). DOI: 10.18577/2713-0193-2023-0-1-30-50.
  6. Smith T.M., Esser B.D., Antolin N. et al. Segregation and η-phase formation along stacking faults during creep at intermediate temperatures in Ni-base superalloys. Acta Materialia, 2015, vol. 100, pp. 19‒31. DOI: 10.1016/j.actamat.2015.08.053.
  7. Barba D., Smith T.M., Miao J. et al. Segregation-assisted plasticity in Ni-based superalloys. Metallurgical Materials Transactions, 2018, vol. 49A, pp. 4173−4185. DOI: 10.1007/s11661-018-4567-6.
  8. Smith T.M., Gabb T.P., Wertz K.N. et al. Enhancing the creep strength of next-generation disk superalloys via local phase transformation strengthening. Superalloys 2020. Pennsylvania: Minerals, Metals, Materials Series, 2020, pp. 726–736.
  9. Lilensten L., Antonov S., Gault B. et al. Enhanced creep performance in a polycrystalline superalloy driven by atomic-scale phase transformation along planar faults. Acta Materialia, 2021, vol. 202, pp. 232‒242.
  10. Svetlov I.L., Zaitsev D.V., Karashaev M.M., Epishin A.I., Petrushin N.V. The microsgation of the alloying elements on deformation defects of the structure in granular nickel alloy. Fizika metallov i metallovedenie, 2023, vol. 124, no. 6, pp. 517−523. DOI: 10.31857/S0015323023600296.
  11. Viswanathan G.B., Sarosi P.M., Henry M.F. et al. Investigation of creep deformation mechanisms at intermediate temperatures in René 88 DT. Acta Materialia, 2005, vol. 53, pp. 3041–3057.
  12. Ber L.B., Rogozhkin S.V., Khomich A.A., Zaluzhny A.G. The distribution of atoms of the alloying elements between the particles γ- and γʹ-fasm in a heat-resistant nickel alloy. Fizika metallov i metallovedenie, 2022, vol. 123, no. 2, pp. 177–191.
  13. Rogozhkin S.V., Ber L.B., Nikitin A.A., Khomich A.A., Raznitsyn O.A., Lukyanchuk A.A., Shutov A.S., Karashaev M.M., Zaluzhny A.G. The study of granular nickel alloy by nuclear-zonian tomography. Fizika metallov i metallovedenie, 2020, vol. 121, no. 1, pp. 1–12.
  14. Saada G., Veyssiere P. Kear-Wilsdorf locks and mechanical properties of L12 alloys. MRS Online Proceedings Library, 1992, vol. 288, pp. 411−416. DOI: 10.1557/PROC-288-411.
  15. Rae C., Vorontsov V., Kovarik L., Mills M. Dislocations in a Ni-based superalloy during low temperature creep. MATEC Web of Conferences, 2014, art. 01006. DOI: 10.1051/matecconf/20141401006.
  16. Smith T.M., Unocic R.R., Deutchman H., Mills M.J. Creep deformation mechanism mapping in nickel base disk superalloys. Materials at High Temperatures, 2016, vol. 33, no. 4−5, pp. 372−383. DOI: 10.1080/09603409.2016.1180858.
  17. Zaysev D.V., Sbitneva S.V., Ber L.B., Zavodov A.V. Determination of the main phase’s particles chemical composition in products from granulated nickel superalloy EP741NP. Trudy VIAM, 2016, no. 9, paper no. 08. Available at: http://www.viam-works.ru (accessed: October 04, 2023). DOI: 10.18577/2307-6046-2016-0-9-7-7.
  18. Petrushin N.V., Ospennikova O.G., Svetlov I.L. Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 72−103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
  19. Logunov A.V. Heat-resistant nickel alloys for shoulder blades and disks of gas turbines. Rybinsk: Gas turbine technologies, 2017, 854 p.
  20. Jena A.K., Chaturvedj M.C. The role of alloying elements in the design of nickel-base superalloys. Journal of Material Science, 1984, vol. 19, pp. 3121–3139.
  21. Murakumo T., Kobayashi T., Koizumi Y., Harada H. Creep behavior of Ni-base single-crystal superalloys with various γ'-volume fraction. Acta Materialia, 2004, vol. 52, pp. 3737–3744.
  22. Unocic R.R., Vismanathan G.B., Sarosi P.M. et al. Mechanisms of creep deformation in polycrystalline Ni-base disk superalloy. Materials Science and Engineering A, 2008, vol. 483−484, pp. 25‒32.
  23. Bakradze M.M., Skugorev A.V., Bubnov M.V., Derevzov A.S., Sumynikov M.N., Shestakov A.A. Development of technology for obtaining blanks of gas turbine gas turbine engines from a new granular heat-resistant alloy VZh178P method + deformation. Tekhnologiya legkikh splavov, 2018, no. 3, pp. 21–27.
  24. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  25. Kablov E.N., Petrushin N.V. Computer method for constructing casting heat-resistant nickel alloys. Aviacionnye materialy i tehnologii, 2004, no. 1, pp. 3–21.
  26. Petrushin N.V., Visik E.M., Elyutin E.S. Improvement of the chemical composition and structure of castable nickel-base superalloy with low density. Part 2. Trudy VIAM, 2021, no. 4 (98), paper no. 01. Available at: http://www.viam-works.ru (accessed: October 04, 2023). DOI: 10.18577/2307-6046-2021-0-4-3-15.
  27. Samoilov A.I., Morozova G.I., Krivko A.I., Afonicheva O.S. The analytical method for optimizing the alloying of heat-resistant nickel alloys. Materialovedenie, 2000, no. 2, pp. 14–17.
  28. Morozova G.I. Compensation for the imbalance of the focus of heat-resistant nickel alloys. Metallovedenie i termicheskaya obrabotka metallov, 2012, no. 12 (690), pp. 52–56.
  29. Morinaga M., Yukawa N., Adachi H., Ezaki H. New phacomp and its applications to alloy design. Superalloys 1984. Pennsylvania: Minerals, Metals & Materials Society, 1984, pp. 523–532.
  30. Martin J., Dortart R. The stability of the microstructure of metal systems. Moscow: Atomizdat, 1978, 280 p.
  31. Reed R.C. The Superalloys. Fundamentals and Applications. Cambridge: United Kingdom at University Press, 2006, 372 p.
  32. Logunov A.V., Shmotin Yu.N. Modern heat-resistant nickel alloys for gas turbine disks (materials and technologies). Moscow: Nauka i tekhnologiya, 2013, 264 p.
  33. Samojlov A.I., Nazarkin R.M., Moiseeva N.S. Definition miss-fit in fragmental single crystals of nickel hot strength alloys. Trudy VIAM, 2013, no. 5, paper no. 02. Available at: http://www.viam-works.ru (accessed: August 31, 2023).
  34. Letnikov M.N., Lomberg B.S., Ospennikova O.G., Bakradze M.M. The influence of quench rate on microstructure and mechanical properties of nickel-based wrought superalloy VZh175-ID. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 21–30. DOI: 10.18577/2071-9140-2019-0-2-21-30.
  35. Glatzel U. Microstructure and internal strains of undeformed and creep-deformed samples of a nickel-base superalloy. Berlin: Verlag Dr. Köster, 1994, 80 p.
  36. Karunaratne M.S.A., Kyaw S., Jones A. et al. Modeling the coefficient of thermal expansion in Ni-based superalloys and bond coatings. Journal Materials Science, 2016, vol. 51, pp. 4213–4226. DOI: 10.1007/s10853-015-9554-3.
  37. Petrushin N.V., Epishin A.I., Svetlov I.L., Nolce G., Elyutin E.S., Soloviev A.E. The influence of the sign γ/γ′-Mismephite on the structure and long-term strength of monocrystals of nickel heat-resistant alloys. Materialovedenie, 2022, no. 3, pp. 17–26. DOI: 10.31044/1684-579x-2022-0-3-17-26.
  38. Epishin A.I., Petrushin N.V., Svetlov I.L., Nolce G. Model for predicting the temperature dependence of γ/γʹ-Mysfit in heat-resistant nickel alloys. Materialovedenie, 2021, no. 3, pp. 9–18. DOI: 10.31044/1684-579X-2021-0-3-9-18.
  39. Kablov E.N., Golubovsky E.R. The heat resistance of nickel alloys. Moscow: Mechanical Engineering, 1998, 463 p.
  40. Larson F.R., Miller J. A time-temperature relationship for rupture and creep stresses. Transactions ASME, 1952, vol. 74, pp. 765–771.
  41. High-Temperature High-Strength Nickel Base Superalloy ‒ Data Supplement. Toronto: Nickel Development Institute, 1995, no. 393, pp. 1−19.
  42. Petrushin N.V., Golinets S.A., Rimsha E.G., Ryzhkov P.V. Mechanical properties of corrosion-resistant nickel-based superalloy VZhL23. Trudy VIAM, 2023, no. 8 (126), paper no. 01. Available at: http://www.viam-works.ru (accessed: October 04, 2023). DOI: 10.18577/2307-6046-2023-0-8-3-12.
  43. Nabarro F.R.N. Rafting in superalloys. Metallurgical and Materials Transactions A, 1996, vol. 27, no. 3, pp. 513‒530. DOI: 10.1007/BF02648942.
  44. Lashko N.F., Zaslavskaya L.V., Kozlova M.N., Morozova G.I., Sorokina K.P., Yakovleva E.F. Physico-chemical phase analysis of steels and alloys. Moscow: Metallurgy, 1978, 336 p.
  45. Hirt D.Zh., Lota I. Theory of dislocations. Moscow: Atomizdat, 1972, 600 p.