Agglomeration of granules of high-temperature metal-ceramic material based on molybdenum

Bobrovkiy A.P., Atkin O.N., Efimochkin I.Yu., Bolshakova A.N.
Bobrovkiy A.P., Atkin O.N., Efimochkin I.Yu., Bolshakova A.N. Agglomeration of granules of high-temperature metal-ceramic material based on molybdenum // Proceedings of VIAM. 2023. No. 10. DOI: 10.18577/2307-6046-2023-0-10-43-51. URL: https://www.viam-works.ru/en/journal/2023/10/5
Keywords
metal-ceramic materials, mechanical alloying, powder metallurgy, agglomeration, additive technologies
Abstract

The process of agglomeration of granules of high-temperature metal-ceramic material based on molybdenum by high-temperature diffusion is discussed. The dependence of the size of the obtained granules on the agglomeration temperature is established. The influence of the agglomeration temperature on the strength of diffusion bonds arising between granules during high-temperature exposure is given is demonstrated.

Reference list
  1. Kashin D.S., Dergacheva P.E., Stekhov P.A. Heat resistant slurry coatings (review). Trudy VIAM, 2018, no. 5 (65), paper no. 08. Available at: http://www.viam-works.ru (accessed: July 17, 2023). DOI: 10.18577/2307-6046-2018-0-5-64-75.
  2. Trofimenko N.N., Efimochkin I.Yu., Bolshakova A.N. Problems of creation and prospects for the use of heat-resistant high-entropy alloys. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 3–8. DOI: 10.18577/2071-9140-2018-0-2-3-8.
  3. Grashchenkov D.V., Efimochkin I.Yu., Bolshakova A.N. High-temperature metal-matrix composite materials reinforced with particles and fibers of refractory compounds. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 318–328. DOI: 10.18577/2071-9140-2017-0-S-318-328.
  4. Kablov E.N. New generation materials are the basis of innovation, technological leadership and national security of Russia. Intellekt & Tekhnologii, 2016, no. 2, pp. 41–46.
  5. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  6. Svetlov I.L. High-temperature Nb–Si composites (beginning). Materialovedenie, 2010, no. 9, pp. 29–38.
  7. Svetlov I.L. High-temperature Nb–Si composites (end). Materialovedenie, 2010, no. 10, pp. 18–27.
  8. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
  9. Kablov E.N., Svetlov I.L., Efimochkin I.Yu. High-temperature Nb–Si composites. Vestnik MGTU im. N.E. Baumana, ser.: Mechanical engineering, 2011, no. SP2, pp. 164–173.
  10. Batienkov R.V., Burkovskaya N.P., Bolshakova A.N., Khudnev A.A. High temperature metal matrix composite materials (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 07. Available at: http://www.viam-works.ru (accessed: July 28, 2023). DOI: 10.18577/2307-6046-2020-0-67-45-61.
  11. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  12. Titov D.D., Kargin Yu.F., Lysenkov A.S., Popova N.A., Gorshkov V.A. Influence of WSi2 content and magnesium aluminosilicate additives on the oxidation and strength properties of MoSi2–WSi2 composites. Materialovedenie, 2012, no. 7, pp. 45–49.
  13. Klimkina A.A. Study of the structure and properties of molybdenum alloys obtained by additive technologies. XLVII Gagarin Readings: collection. tr. Intl. youth science conf. M.: FGBUN Institute of Problems of Mechanics named after. A.Yu. Ishlinsky Russian Academy of Sciences, 2021, p. 81.
  14. Varaksin A.V., Lisin V.L., Kostylev V.A. and others. Preparation of composite powders containing metal carbides. Butlerovskie soobshcheniya, 2015, vol. 43, no. 8, pp. 102–110.
  15. Varaksin A.V., Kostylev V.A., Lisin V.L. and others. Application of composite agglomerates based on WC and TiC, obtained using electrochemical technology, to create wear-resistant coatings by direct laser deposition. Butlerovskie soobshcheniya, 2016, vol. 48, no. 10, pp. 14–22.