Investigation of the influence of the direction of the basal planes in a carbon frame and a metal composite material of the Al–C system on the temperature coefficient of linear expansion

Nyafkin A.N., Kosolapov D.V., Zhabin A.N.
Nyafkin A.N., Kosolapov D.V., Zhabin A.N. Investigation of the influence of the direction of the basal planes in a carbon frame and a metal composite material of the Al–C system on the temperature coefficient of linear expansion // Proceedings of VIAM. 2023. No. 10. DOI: 10.18577/2307-6046-2023-0-10-35-42. URL: https://www.viam-works.ru/en/journal/2023/10/4
Keywords
carbon material, cast aluminum alloy, metal composite material, vacuum-compression impregnation, basal planes, temperature coefficient of linear expansion
Abstract

A porous carbon material and a metal composite material (MCM) based on an aluminum casting alloy of the Al–Si–Cu system containing 79±2 % (vol.) carbon, obtained using the vacuum-compression impregnation technology, have been studied. A study of the structure of MCM was carried out, the density, volumetric filling and temperature coefficients of linear expansion (TCLE) of the carbon frame and MCM were measured in the temperature range from 20 to 200 °C. It has been established that depending on the direction of the basal planes, the TCLE value decreases by 30–35 % at the carbon frame and by 15–20 % at MCM.

Reference list
  1. Zweben C. Advances in photonics thermal management and packaging materials. Proceedings of SPIE – The International Society for Optical Engineering, 2008. DOI: 10.1117/12.761748.
  2. Vishnyakov L.R., Kokhany V.L., Moroz V.P., Kladnitsky E.I. Aluminum composites for tribotechnical purposes, obtained by vacuum-compression impregnation. Composite materials in industry: materials of the 23rd Intern. conf. Yalta, 2003, pp. 161–162.
  3. Structure and properties of composite materials: collection. scientific tr. Ed. K.I. Portnoy. Moscow: Mashinostroyenie, 1979, 253 p.
  4. Kotval P.S. Wear resistant aluminum – a new approach: cast surface composites. Journal of Metals, 1974, vol. 26, no. 1, pp.13–17.
  5. Pepper R.T., Upp J.W., Rossi R.C., Kendall E.G. The tensile properties of graphite-fiber reinforced Al–Si alloy. Metallurgical Transactions, 1971, vol. 2, no. 1, pp. 117–120.
  6. Salibekov S.E., Zabolotsky A.A. Study of the influence of nickel coatings on fiber on the structure and properties of aluminum-carbon fiber composite material. Fiber and dispersion-strengthened composite materials. Moscow: Nauka, 1976, pp. 33–37.
  7. Device for producing a product from a metal matrix composite material: pat. 110310 Rus. Federation; appl. 31.05.11; publ. 20.11.11.
  8. Method for producing a product from a composite material: patent. 2448808 Rus. Federation; appl. 05.10.10; publ. 27.04.12.
  9. Kablov E.N., Solovyanchik L.V., Kondrashov S.V. and others. Electrically conductive hydrophobic polymer composite materials based on oxidized carbon nanotubes modified with tetrafluoroethylene telomers. Rossiyskie nanotekhnologii, 2016, vol. 11, no. 11–12, pp. 91–97.
  10. Lukina E.A., Zaitsev D.V., Romanenko V.A. Structure and properties of a composite material based on aluminum alloy with the addition of carbon nanotubes. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 27–34. DOI: 10.18577/2071-9140-2019-0-4-27-34.
  11. Kablov E.N., Belov E.V., Trapeznikov A.V., Leonov A.A., Zaitsev D.V. Strengthening features and aging kinetics of high-strength cast aluminum alloy AL4MS based on Al–Si–Cu–Mg system. Aviation materials and technologies, 2021, no. 2 (63), paper no. 03. Available at: http://www.journal.viam.ru (accessed: July 17, 2023). DOI: 10.18577/2713-0193-2021-0-2-24-34.
  12. Nyafkin A.N., Shavnev A.A., Kurbatkina E.I., Kosolapov D.V. Studying the effect of silicon carbide particle size on the linear thermal expansion coefficient of the composite material based on aluminum alloy. Trudy VIAM, 2020, no. 2 (86), paper no. 05. Available at: http://www.viam-works.ru (accessed: July 25, 2023). DOI: 10.18577/2307-6046-2020-0-2-41-49.
  13. ASTM E228. Standard test method for linear thermal expansion of solid materials with a push-rod dilatometer. West Conshohocken, PA: ASTM International, 2017, pp. 1–10. DOI: 10.1520/Е0228-17.
  14. Parker W.J., Jenkins R.J., Butler С.Р., Abbott G.L. Rash method of determining thermal diffusivity, heat capacity and thermal conductivity. Journal of Applied Physics, 1961, no. 32, pp. 1679–1684.
  15. ASTM E831. Standard test method for linear thermal expansion of solid materials by thermomechanical analysis. West Conshohocken, PA: ASTM International, 2019, pp. 1–5. DOI: 10.1520/Е0831-19.
  16. Nyafkin A.N., Loshchinin Yu.V., Kurbatkina E.I., Kosolapov D.V. Investigation of influence of silicon carbide fractional composition on thermal conductivity of compo-site material based on aluminium alloy. Trudy VIAM, 2019, no. 11 (83), paper no. 6. Available at: http://www.viam-works.ru (accessed: July 21, 2023). DOI: 10.18577/2307-6046-2019-0-11-53-59.
  17. State Standard 18898–89 (ISO 2738–87). Powder products. Methods for determining density, oil content and porosity. Moscow: Publ. house of standards, 1990, 10 p.
  18. State Standard R 22309–2015 (ISO 22309–2011). State system for ensuring the uniformity of measurements. Electron probe microanalysis. Quantitative analysis using energy dispersive spectrometry for elements with atomic number 11 (Na) and higher. Moscow: Standartinform, 2015, 19 p.