The influence of various modes of hot isostatic pressed and heat treatment on structure and properties of castings from the VT40L alloy
Makushina M.A., Kochetkov A.S., Vinogradov I.D. The influence of various modes of hot isostatic pressed and heat treatment on structure and properties of castings from the VT40L alloy // Proceedings of VIAM. 2023. No. 10. DOI: 10.18577/2307-6046-2023-0-10-24-34. URL: https://www.viam-works.ru/en/journal/2023/10/3
Keywords
titanium, cast alloys, cast samples, high cycle fatigue, tensile strength, hot isostatic pressed, heat treatment
Abstract
This article presents the results of studies of the influence of various modes of hot isostatic pressing (HIP) and heat treatment on the mechanical properties and structure of cast samples from the VT40L alloy. The temperature of the polymorphic transformation in the alloy was determined experimentally using the test quenching method. Tensile tests were carried out to determine the short-term strength and yield strength, the endurance limit on the basis of N = 2·107 cycle, impact strength and hardness were determined. Based on the test results, a casting processing mode was selected that provides a set of properties necessary for parts of aircraft products.
Reference list
- Kablov E.N. The role of fundamental research in the creation of new generation materials. Report XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, pp. 24.
- Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
- Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
- Tarasenko E.N., Prokhodtseva L.V., Rudakov A.G. High-strength economically alloyed titanium alloy with increased durability for precision shaped casting. Aviacionnye materialy i tehnologii, 2005, no. 2, pp. 37–42.
- Putyrskiy S.V., Yakovlev A.L., Nochovnaya N.A., Krokhina V.A. Research of different heat treatment modes influence on properties of semi-finished products and welded joints from titanium alloy ВТ22М. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 3–10. DOI: 10.18577/2071-9140-2019-0-1-3-10.
- Krokhina V.A., Putyrskiy S.V., Gribkov M.S. Analysis of structure and mechanical properties of welded joint from titanium alloy VT22M. Aviation materials and technologies, 2022, no. 2 (67), paper no. 05. Available at: http://www.journal.viam.ru (accessed: September 08, 2023). DOI: 10.18577/2713-0193-2022-0-2-52-62. (дата обращения: 08.09.2023).
- Alekseev E.B., Nochovnaya N.A., Panin P.V., Novak A.V. Technological plasticity, structure and phase composition of a pilot titanium ortho alloy with 13 wt. рct. aluminum. Trudy VIAM, 2015, no. 12, paper no. 08. Available at: http://www.viam-works.ru (accessed: September 08, 2023). DOI: 10.18577/2307-6046-2015-0-12-8-8.
- Ilyin A.A., Kolachev B.A., Polkin I.S. Titanium alloys. Composition, structure, properties: reference book. Moscow: VILS; MATI, 2009, 520 p.
- Kablov E.N., Akinina M.V., Volkova E.F., Mostyaev I.V., Leonov A.A. The research of aspects of phase composition and fine structure of magnesium alloy ML9 in the as-cast and heat-treated conditions. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 17–24. DOI: 10.18577/2071-9140-2020-0-2-17-24.
- Panin P.V., Zavodov A.V., Lukina E.A. Effect of thermal exposure on microstructure evolution and mechanical properties of cast beta-solidifying TiAl-based alloy doped with Gd. Intermetallics, 2022, vol. 145, art. 107534. DOI: 10.1016/j.intermet.2022.107534.
- Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
- Makushina M.А., Kochetkov A.S., Vinogradov I.D. Statistical evaluation of the homogeneity of the chemical composition of vacuum-arc remelting ingots from economic alloy titanium VT40L. Trudy VIAM, 2022, no. 11 (117), paper no. 03. Available at: http://www.viam-works.ru (accessed: September 08, 2023). DOI: 10.18577/2307-6046-2022-0-11- 27-36.
- Kochetkov A.S., Panin P.V., Nochovnaya N.A., Makushina M.A. Study of chemical heterogeneity of beta-hardening TiAl alloy ingots of variable composition. Metallurg, 2020, no. 9, pp. 93–100.
- Duyunova V.A., Oglodkov M.S., Putyrskiy S.V., Kochetkov A.S., Zueva O.V. Modern technologies for melting titanium alloy ingots (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 03. Available at: http://www.journal.viam.ru (accessed: September 08, 2023). DOI: 10.18577/2071-9140-2022-0-1-30-40.
- Dobatkin V.I., Anoshkin N.F., Andreev A.L., Bochvar G.A., Musatov M.I., Tetyukhin V.V., Chistyakov E.P. Ingots of titanium alloys. Moscow: Metallurgiay, 1966, 287 p.
- Panin P.V., Nochovnaya N.A., Kablov D.E., Alekseev E.B., Shiryaev A.A., Novak A.V. Practical guide to metallography of alloys based on titanium and its intermetallic compounds: textbook. Ed. E.N. Kablov. Moscow: VIAM, 2020, 200 p.
- Belov V.D., Fadeev A.V., Ivashchenko A.I., Beltyukova S.O. Vacuum melting and production of shaped castings from titanium and thianium alloys. Moscow: Publ. House of MISiS, 2013, 107 p.
- Bratukhin A.G., Bibikov E.L., Glazunov S.G. et al. Production of shaped castings from titanium alloys. 2nd ed., rev. and add. Moscow: VILS, 1998, 293 p.
- Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallic alloys based on titanium and nickel. Ed. E.N. Kablov. 2nd ed. Moscow: VIAM, 2019, 316 p.
- Sergeev V.V., Galitsky N.V., Kiselev V.P., Kozlov V.M. Titanium metallurgy. Moscow: Metallurgiya, 1971, 320 p.
- Yasinsky K.K., Tarasenko E.N. New high-strength cast titanium alloy VT40L. Aviacionnye materialy i tehnologii, 2007, no. 1, pp. 58–60.
- Kolachev B.A., Eliseev Yu.S., Bratukhin A.G., Talalaev V.D. Titanium alloys in the design and production of aircraft engines and aerospace equipment. Moscow: MAI, 2001, 412 p.
- Aviation materials: reference book in 13 vols. Ed. E.N. Kablov. 7th ed., rev. and add. Moscow: VIAM, 2010, vol. 6: Titanium alloys, 96 р.