Study of the structure, distribution of carbide phase, hardness and tribotechnical characteristics of high-chromium bearing steels of the martensitic class

Sevalnev G.S., Vostrikov A.V., Nefedkin D.Yu., Moiseenkov V.V., Volkov R.B., Ulyanov E.I.
Sevalnev G.S., Vostrikov A.V., Nefedkin D.Yu., Moiseenkov V.V., Volkov R.B., Ulyanov E.I. Study of the structure, distribution of carbide phase, hardness and tribotechnical characteristics of high-chromium bearing steels of the martensitic class // Proceedings of VIAM. 2023. No. 10. DOI: 10.18577/2307-6046-2023-0-10-13-23. URL: https://www.viam-works.ru/en/journal/2023/10/2
Keywords
bearing steels, 60Kh13S-ShD, 95Kh18-Sh, 110Kh18M-ShD, microstructure, carbides size, wear resistance
Abstract

The paper presents a comparative analysis of the microstructure, size and distribution of carbides, hardness and tribotechnical properties during research and testing under the same conditions of bearing steel grades 60Kh13S-ShD, 95Kh18-Sh and 110Kh18M-ShD, commercially used in the Russian industry. Based on the results of the research, steel grades were identified that have the best set of properties after hardening heat treatment.

Reference list
  1. Spektor A.G., Zelbet B.M., Kiseleva S.A. Structure and properties of bearing steels. Moscow: Metallurgiya, 1980, 264 p.
  2. Sprishevsky A.I. Rolling bearings. Moscow: Mashinostroenie, 1968, 632 p.
  3. Pinegin S.V. Rolling bearings in machines. Moscow: Publ. House of the RAS of the USSR, 1961, 150 p.
  4. Instrument ball bearings: a reference book. Ed. K.N. Yavlensky et al. Moscow: Mashinostroenie, 1981, 351 p.
  5. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  6. Geller Yu.A. Tool steels. Moscow: Metallurgiya 1983, 525 p.
  7. Sevalnev G.S., Yakusheva N.A., Korobova E.N., Dulnev K.V. Study of the diffusion saturation kinetics of high-chromium carbon steels of the martensitic class after various types of chemical-heat treatment. Aviation materials and technologies, 2022, no. 3 (68), paper no. 01. Available at: http://www.journal.viam.ru (accessed: April 20, 2023). DOI: 10.18577/2713-0193-2022-0-3-3-14.
  8. Krishna S.C., Tharian K.T., Chakravarthi K.V.A. et al. Heat treatment and thermo-mechanical treatment to modify carbide banding in AISI 440C steel: a case study. Metallography, Microstructure, and Analysis, 2016, vol. 5, no. 2, pp. 108–115.
  9. Zheng C., Fu B., Tang Y. et al. Microstructure and mechanical properties of 9Cr18Mo martensitic stainless steel fabricated by strengthening-toughening treatment. Materials Science and Engineering: A, 2023, vol. 869, p. 144783.
  10. Yang J.R., Yu T.H., Wang C.H. Martensitic transformations in AISI 440C stainless steel. Materials Science and Engineering: A, 2006, vol. 438, pp. 276–280.
  11. Shen Y., Moghadam S.M., Sadeghi F. et al. Effect of retained austenite – Compressive residual stresses on rolling contact fatigue life of carburized AISI 8620 steel. International Journal of Fatigue, 2015, vol. 75, pp. 135–144.
  12. Gromov V.I., Kurpyakova N.A., Korobova E.N., Sedov O.V. New heat resistant steel for aircraft bearings. Trudy VIAM, 2019, no. 2 (74), paper no. 02. Available at: http://www.viam-works.ru (accessed: April 27, 2023). DOI: 10.18577/2307-6046-2019-0-2-17-23.
  13. Korobova E.N., Sevalnev G.S., Gromov V.I., Leonov A.V. Steels for the manufacture of roller bearings for special purposes (review). Trudy VIAM, 2021, no. 11 (105), paper no. 01. Available at: http://www.viam-works.ru (accessed: April 25, 2023). DOI: 10.18577/2307-6046-2021-0-11-3-11.
  14. Stive O.O.I., Bhadeshia H.K.D.H. Duplex hardening of steels for aeroengine bearings. ISIJ international, 2012, vol. 52, no. 11, pp. 1927–1934.
  15. Smirnov A.E., Shevchenko S.Y., Shchipunov V.S. et al. Special features of the carbonitriding of parts of instrument bearings designed for extreme service conditions. Metal Science and Heat Treatment, 2016, vol. 58, no. 5–6, pp. 287–292.
  16. Pakhomova S.A., Klimkina A.A., Gress M.A. Technology of heat treatment of corrosion-resistant bearings for the mining industry. Sovremennye innovatsionnyye tekhnologii podgotovki inzhenernykh kadrov dlya gornoy promyshlennosti i transporta, 2015, no. 1, pp. 98–104.
  17. Sevalnev G.S., Sevalneva T.G., Kolmakov A.G., Dulnev K.V., Yazvitsky M.Yu. Influence of the phase composition of austenitic-martensitic trip steel VNS9-Sh on the characteristics of dry sliding friction in tribocontact with steel ShKh15. Deformatsiya i razrusheniye materialov, 2021, no. 10, pp. 20–27. DOI: 10.31044/1814-4632-2021-10-20-27.
  18. Martensitic Stainless Steel for Knife Applications – Part 1: Fe–Cr–C. Computational Thermodynamics Calculation of Phase Diagrams using the CALPHAD Method. URL: http://www.calphad.com/ (accessed: April 26, 2023).
  19. Kazarin S.I. On the chipping of carbides on the surface of the grooves of bearing rings made of corrosion-resistant steel 110Х18М-ShD. Vestnik Samarskogo gosudarstvennogo tekhnicheskogo universiteta. Series: Technical Sciences, 2014, no. 2 (42), pp. 69–73.
  20. Special steels: 2 vols; trans. for Germ. 2nd ed. Moscow: Metallurgiya, 1966, vol. 1. 741 p.
  21. Special steels: 2 vols; trans. for Germ. 2nd ed. Moscow: Metallurgiya, 1966, vol. 2. 532 p.