The influence of artificial aging on the properties of coating systems based on chromate-free primer VG-44 using epoxy, polyurethane, acrylic urethane and fluoropolyurethane enamels

Kuznetsova V.A., Emelyanov V.V., Marchenko S.A., Kovrizhkina N.A.
Kuznetsova V.A., Emelyanov V.V., Marchenko S.A., Kovrizhkina N.A. The influence of artificial aging on the properties of coating systems based on chromate-free primer VG-44 using epoxy, polyurethane, acrylic urethane and fluoropolyurethane enamels // Proceedings of VIAM. 2023. No. 10. DOI: 10.18577/2307-6046-2023-0-10-119-131. URL: https://www.viam-works.ru/en/journal/2023/10/11
Keywords
chromate-free primer, paint coating systems, adhesion, tensile strength, impact strength, water absorption, gloss, artificial aging
Abstract

The adhesion and impact strength of paint coating systems based on the chromate-free primer VG-44 with enamels VE-69, AK-1206, UR-1161 and EP-140 after artificial aging using the LI-14 method (–60÷+80) were studied.)°С during 16 cycles, as well as after thermal aging at temperatures of 80 °C – 1000 hours and 100 °C – 500 hours. The decorative properties of coatings based on the chromate-free primer VG-44 with enamels VE-69, AK-1206, UR-1161 and EP-140 after artificial aging were determined. It has been shown that artificial aging of the above paintwork systems does not have a significant effect on the strength of coatings upon impact, but leads to a decrease in tensile strength, as well as a decrease in the gloss of the coatings.

Reference list
  1. Zhitomirsky G.I. Aircraft design. Moscow: Mashinostroyenie, 1991, 400 p.
  2. Kablov E.N. Main directions of development of materials for aerospace technology of the 21st century. Perspektivnyye materialy, 2000, no. 3, pp. 27–36.
  3. Kablov E.N. Aviation materials science in the 21st century. Prospects and objectives. Aviation materials. Selected works of VIAM 1932–2002. Moscow: MISIS–VIAM, 2002, pp. 23–47.
  4. Kablov E.N. New generation materials are the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  5. Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), paper no. 07. Available at: http://www.viam-works.ru. (accessed: August 17, 2023). DOI: 10.18577/2307-6046-2019-0-5-62-67.
  6. Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A. Main directions for improving the operational, technological and environmental characteristics of paint and varnish coatings for aircraft. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 96–102.
  7. Fomina M.A., Karimova S.A. Analysis of the corrosion state of airframe materials of Su type aircraft after long periods of operation. Korroziya: materialy, zashchita, 2014, no. 9, pp. 20–24.
  8. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  9. Kozlova A.A., Kondrashov E.K. Systems of paint coatings for anticorrosive protection of magnesium alloys. Aviacionnye materialy i tehnologii, 2014, no. 2, pp. 44–47. DOI: 10.18577/2071-9140-2014-0-2-44-47.
  10. Ptitsyn A.S. The thickness of the paint coating as one of the factors of its quality and durability. Alleya nauki, 2018, vol. 5, no. 10, pp. 896–901.
  11. Popov A.A., Rapoport N.Ya., Zaikov G.E. Oxidation of oriented and strained polymers. Moscow: Khimiya, 1987, 232 p.
  12. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  13. Zheleznyak V.G., Serdcelyubova A.S., Merkulova Yu.I., Skivko P.V. Paint coating system based on polyurethane enamel for protecting heated frontal surfaces of aviation products. Aviation materials and technologies, 2022, no. 1 (66), paper no. 10. Available at: http://www.journal.viam.ru (ассеssed: August 24, 2023). DOI: 10.18577/2713-0193-2022-0-1-120-128.
  14. Serdtselyubova A.S., Merkulova Yu.I., Zagora A.G., Kurshev E.V. Research of film-forming parameters and protective properties of basecoat/clearcoat system. Aviation materials and technologies, 2023, no. 1 (70), paper no. 07. Available at: http://www.journal.viam.ru (accessed: August 17, 2023). DOI: 10.18577/2713-0193-2022-0-1-93-104.
  15. Merkulova Yu.I., Kurshev E.V., Vdovin A.I., Andreeva N.P. Microstructural and electrochemical studies of paint coatings under natural climate tests of tropical climate of North America. Aviation materials and technologies, 2022, no. 2 (67), paper no. 11. Available at: http://www.journal.viam.ru (accessed: August 04, 2023). DOI: 10.18577/2713-0193-2022-0-2-120-130.
  16. Semenova L.V., Nefedov N.I., Belova M.V., Laptev A.B. Systems of paint coatings for helicopter equipment. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 56–61. DOI: 10.18577/2071-9140-2017-0-4-56-61.
  17. Kuznetsova V.A., Marchenko S.A., Emelyanov V.V., Zheleznyak V.G. Study of the influence of molecular mass of epoxy oligomers and hardeners on the operational properties of paint coatings. Aviation materials and technology, 2021. no. 1 (62), paper no. 07. Available at: http://www.journal.viam.ru (accessed: September 17, 2023). DOI: 10.18577/2713-0193-2021-0-1-71-79.
  18. Protasov V.N. Prediction of the duration of preservation of the strength of polymer coatings in operating environments. Lakokrasochnyye materialy i ikh primenenie, 1989, no. 2, pp. 77–80.
  19. Grassi N., Scott J. Destruction and stabilization of polymers: trans. from Engl. Moscow: Mir, 1988, 446 p.
  20. Lambourn R., Mashlyakovsky L.N., Frost A.M. Paints and varnishes and coatings. Theory and practice. St. Petersburg: Khimiya, 1991, 512 p.
  21. Merkulova Yu.I., Kuznetsova V.A., Kodachenko E.N., Zheleznyak V.G. Study of the influence of the primer layer’s chemical nature on the properties of the coating system based on fluoropolyurethane enamel. Aviation materials and technologies, 2022, no. 1 (66), paper no. 09. Available at: http://www.journal.viam.ru (accessed: September 17, 2023). DOI: 10.18577/2713-0193-2022-0-1-110-119.
  22. Merkulova Yu.I., Kuznetsova V.A., Novikova T.A. Investigation of properties of coating system based on fluorine polyurethane enamel and primer with low toxical pigment content. Trudy VIAM, 2019, no. 5 (77), paper no. 08. Available at: http://www.viam-works.ru. (accessed: August 06, 2023). DOI: 10.18577/2307-6046-2019-0-5-68-75.
  23. Skorokhodova O.N., Kazakova E.E. New developments in the field of protective coatings. Lakokrasochnaya promyshlennost, 2017, no. 5, p. 14.
  24. Drinberg A.S., Itsko E.F., Kalinskaya T.V. Anti-corrosion primers. St. Petersburg: NIPROINS LKM i PSOP, 2006, 168 p.
  25. Rosenfeld I.L., Rubinshtein F.I. Anti-corrosion primers and inhibited paint and varnish coatings. Moscow: Khimiya, 1980, 200 p.
  26. Anti-corrosion pigment: pat. 2330054 Rus. Federation; appl. 04.05.07; publ. 27.07.08.
  27. Ashuiko V.A., Ivanova N.P., Salychits O.I. Properties of anti-corrosion phosphate-containing pigments for paint and varnish coatings of metals. Energy- and material-saving environmentally friendly technologies: abstracts of the Xth Int. Conf. Grodno, 2013, pp. 117–118.
  28. Emirova I.V., Alekseev A.A. New anti-corrosion pigments. Izvestiya vuzov. Khimiya i khimicheskaya tekhnologiya, 2009, vol. 52, pp. 113–114.
  29. Chebotareva E.G., Ogrel L.Yu. Current trends in the modification of epoxy oligomers. Fundamentalnye issledovaniya, 2008, no. 4, pp. 102–104.
  30. Kirillov A.N., Sofina S.Yu., Garipov R.M., Deberdeev R.Ya. Modification of epoxyamine compositions with epoxyurethane oligomers. Lakokrasochnyye materialy i ikh primenenie, 2003, no. 4, pp. 25–28.
  31. Kirillov A.N., Garipov R.M., Deberdeev R.Ya. The influence of epoxyurethane modifiers on the properties of epoxy varnish coatings. Articles IX All-Rus. conf. “Structure and dynamics of molecular systems”. Yalchik, 2002, pp. 236–239.
  32. Parshina M.S., Soldatov M.A., Makarova V.A., Serenko O.A., Muzafarov A.M. The influence of the chemical structure of organofluorine copolymer modifiers on the moisture resistance of amine-curing epoxy resin. Lakokrasochnyye materialy i ikh primenenie, 2018, no. 3, pp. 15–19.
  33. Problems of protective coatings: Review of materials of the European conference “Protective coating”. Dusseldorf (Germany). Lakokrasochnyye materialy i ikh primenenie, 2013, no. 9, pp. 33–35.
  34. Kuznetsova V.A., Zheleznyak V.G., Silaeva A.A. Influence of mechanical characteristics of priming coverings on stability to cyclic mechanical loads of systems of the erosion resistant disperse reinforced coatings. Trudy VIAM, 2018, no. 6 (66), paper no. 07. (accessed: August 13, 2023). DOI: 10.18577/2307-6046-2018-0-6-59-67.
  35. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.