Investigation of microstructure and phase composition of the metallic composite material Al–Si–Mg system modified by silicon carbide particles by mechanical alloying
Part 2
UDC
669.018.95
DOI
10.18577/2307-6046-2023-0-1-107-118
Article PDF (Russian)
(947.04 KB)
How to cite
Zhitnyuk S.V., Medvedev P.N. Investigation of microstructure and phase composition of the metallic composite material Al–Si–Mg system modified by silicon carbide particles by mechanical alloying. Part 2 // Proceedings of VIAM. 2023. No. 1. DOI: 10.18577/2307-6046-2023-0-1-107-118. URL: https://www.viam-works.ru/en/journal/2023/1/9
Keywords
mechanical alloying, composite material, microstructure, aluminum alloy, silicon carbide, synchronous radiation, phase analysis
Abstract
The process of mechanical alloying of aluminum alloy BAC1 with silicon carbide particles in a ball mill has been studied. An analysis of the stages of the process of mechanical alloying in the preparation of BAC1–SiC powder compositions was carried out and characteristic microstructures corresponding to each stage were identified. A hypothesis was formulated about the effect of collisions of granule particles on the formation of the structure of composite particles during mechanical alloying of an aluminum alloy BAC1 with silicon carbide SiC, which satisfactorily describes the experimental results obtained.
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Dominant of the national technology initiative. Problems of accelerating the development of additive technologies in Russia. Metally of Evrazii, 2017, no. 3, pp. 2–6.
- Kablov E.N., Shchetanov B.V., Grashhenkov D.V., Shavnev A.A., Nyafkin A.N. Metalmatrix composite materials on the basis of Al–SiC. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 373–380.
- Sergeeva A.M., Lovizin N.S., Sosnin A.А. About combined technology of continuous casting of aluminum alloys with synchronous deformation of the metal. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 9–16. DOI: 10.18577/2071-9140-2018-0-2-9-16.
- Gorbovets M.A., Belyayev M.S., Ryzhkov P.V. Fatigue strength of heat-resistant nickel alloys produced by selective laser melting. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 50–55. DOI: 10.18577/2071-9140-2018-0-3-50-55.
- Bulina N.V., Malikov A.G., Orishich А.М., Klochkov G.G. Research of the structural-phase composition of laser weld joint depending on the thermal processing of the aluminum alloy V-1469. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 31–39. DOI: 10.18577/2071-9140-2019-0-2-31-39.
- Lukina E.A., Zaitsev D.V., Romanenko V.A. Structure and properties of a composite material based on aluminum alloy with the addition of carbon nanotubes. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 27–34. DOI: 10.18577/2071-9140-2019-0-4-27-34.
- Astashkin A.I., Babanov V.V., Selivanov A.A., Tkachenko E.A., Gusev D.V., Tsarev M.V. Improving the hardenability of massive forgings from alloys of the Al–Zn–Mg–Cu system by balanced alloying with zinc and magnesium. Aviation materials and technologies, 2021, no. 2 (63), paper no. 04. Available at: http://www.journal.viam.ru (accessed: November 28, 2022). DOI: 10.18577/2713-0193-2021-0-2-35-42.
- Shchetinina N.D., Kuznetsova P.E., Dynin N.V., Selivanov A.A. Aluminum alloys with additions of Sc and Zr IN additive manufacturing (review) Aviation materials and technologies, 2021, no. 3 (64), paper no. 03. Available at: http://www.journal.viam.ru (accessed: November 28, 2022). DOI: 10.18577/2713-0193-2021-0-3-19-34.
- Shavnev A.A., Nerush S.V., Kurbatkina E.I., Kosolapov D.V., Medvedev P.N. Investigation of the structure of a metal composite material of the Al–Si–Mg–SiC system obtained using mechanical alloying. Izvestiya vuzov. Poroshkovaya metallurgiya i funktsionalnye pokrytiya, 2022, no. 1, pp. 17–25. DOI: 10.17073/1997-308X-2022-1-17-25.
- Famodimu O.H., Stanford M., Oduoza C.F., Zhang L. Effect of process parameters on the density and porosity of laser melted AlSi10Mg/SiC metal matrix composite. Frontiers of Mechanical Engineering, 2018, vol. 13, pp. 520–527.
- Riquelme A., Rodrigo P., Escalera-Rodríguez M.D., Rams J. Additively Manufactured Al/SiC Cylindrical Structures by Laser Metal Deposition. Materials, 2020, vol. 13, is. 15, art. 3331. DOI: 10.3390/ma13153331.
- Tang M., Pistorius P.C. Anisotropic Mechanical Behavior of AlSi10Mg Parts Produced by Selective Laser Melting. The Journal of the Minerals, Metals & Materials Society, 2017, vol. 69, pp. 516–522. DOI: 10.1007/s11837-016-2230-5.
- Diagrams of the state of binary metal systems: D44: a reference book in 3 vols. Ed. N.P. Lyakishev. Moscow: Mashinostroenie, 1996, vol. 1, 992 p.
- Medvedev P.N., Kashapov O.S., Reshetilo L.P. Investigation of surface layers of titanium alloy VT41 after mechanical processing. Voprosy materialovedeniya, 2022, no. 1 (109), pp. 54–63.