Some structural features of aluminum alloys obtained by selective laser melting (review)

Sbitneva S.V., Lukinа E.A., Benarieb I.
Sbitneva S.V., Lukinа E.A., Benarieb I. Some structural features of aluminum alloys obtained by selective laser melting (review) // Proceedings of VIAM. 2023. No. 1. DOI: 10.18577/2307-6046-2023-0-1-69-83. URL: https://www.viam-works.ru/en/journal/2023/1/6
Keywords
selective laser melting, aluminum alloys, transmission electron microscopy, scanning electron microscopy, defects, microstructure
Abstract

Selective laser alloying (SLM) of metal powders is one of the most common methods of additive manufacturing of products. The most studied aluminum alloys for SLS technology are AlSi12 and AlSi10Mg alloys. In the paper, using the example of these alloys, some structural features of synthesized aluminum alloys are described, as well as typical defects that can form during synthesis depending on various factors. Scientific and technical literature data on the structure and mechanical properties of aluminum alloys of other alloying systems (Al–Cu–Mg, Al–Mg–Sc, Al–Zn–Mg–Cu) are presented.

Reference list
  1. Kablov E.N., Evgenov A.G., Bakradze M.M., Nerush S.V., Krupnina O.A. New generation materials and digital additive technologies for the production of resource parts FSUE «VIAM». Part 1. Materials and synthesis technologies. Electrometallurgiya, 2022, no. 1, pp. 2–12.
  2. Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S., Dynin N.V. New generation materials and digital additive technologies for the production of resource parts FSUE "VIAM". Part 3. Adaptation and creation of materials. Electrometallurgiya, 2022, no. 4, pp. 15–25.
  3. Knyazev A.E., Vostrikov A.V. Sieving of powders additive and powder manufacturings (review). Trudy VIAM, 2020, no. 11 (93), paper no. 02. Available at: http://www.viam-works.ru (accessed: October 20, 2022). DOI: 10.18577/2307-6046-2020-0-11-11-20.
  4. Tang H.P., Qian M., Liu N. et al. Effect of powder reuse times on additive manufacturing of Ti–6Al–4V by selective electron beam melting. Journal of the Minerals, 2015, vol. 67, pp. 555–563.
  5. Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  6. Babu S.S. Materials science aspects related to additive manufacturing. Scripta Materialia, 2017, vol. 135, pp. 97–99.
  7. Kimura T., Nakamoto T. Thermal and mechanical properties of commercial-purity aluminum fabricated using selective laser melting. Materials Transactions, 2017, vol. 58, pp. 799–805.
  8. Montero Sistiaga M.L., Mertens R., Vrancken B. et al. Changing the alloy composition of Al7075 for better processibility by selective laser melting. Materials Processing Technology, 2016, vol. 238, pp. 437–445.
  9. Kruth J., Levy G., Klocke F., Childs T.H.C. Consolidation phenomena in laser and powder-bed fusion layered manufacturing. CIRP Annals-Manufacturing Technology, 2007, vol. 56, pp. 730–759.
  10. Medvedev P.N., Gulyaev A.I. Analysis of the spatial distribution of cracks in a heat-resistant nickel alloy manufactured using SLM technology. Aviation materials and technologies, 2020, no. 1 (58), pp. 12–18. DOI: 10.18577/2071-9140-2022-0-1-12-18.
  11. Hönnige J.R., Colegrove P.A., Ganguly S. et al. Control of Residual Stress and Distortion in Aluminium Wire + Arc Additive Manufacture with Rolling. Additive Manufacturing, 2018, vol. 22, pp. 775–783.
  12. Brice C.A., Hofmeister W.H. Determination of Bulk Residual Stresses in Electron Beam Additive-Manufactured Aluminum. Metallurgical and Materials Transactions A, 2013, vol. 44, pp. 5147–5153.
  13. Fomina M.A., Dynin N.V., Shurtakov S.V., Morozova S.E. Corrosion behavior of Al–Si–Mg alloy made by selective laser melting method. Trudy VIAM, 2018, no. 4 (64), paper no. 11. Available at: http://www.viam-works.ru (accessed: October 03, 2022). DOI: 10.18577/2307-6046-2018-0-4-91-100.
  14. Dynin N.V., Zavodov A.V., Oglodkov M.S., Khasikov D.V. The influence of process parameters of selective laser melting on the structure of aluminum alloy Al–Si–Mg system. Trudy VIAM, 2017, no. 10 (58), paper no. 01. Available at: http://www.viam-works.ru (accessed: October 03, 2022). DOI: 10.18577/2307-6046-2017-0-10-1-1.
  15. Movenko D.A., Shurtakov S.V. Microcrack formation and controlling in nickel superalloys processed by selective laser melting (review). Aviation materials and technologies, 2022, no. 2 (67), paper no. 04. Available at: http://www.journal.viam.ru (accessed: October 20, 2022). DOI: 10.18577/2713-0193-2022-0-2-43-51.
  16. Siddique S., Imran M., Walther F. Very high cycle fatigue and fatigues crack propagation behavior of selective laser melted AlSi12 alloy. International Journal of Fatigue, 2017, vol. 94, pp. 246–254.
  17. Prashanth K.G., Scudino S., Eckert J. Tensile properties of Selective Laser Melted (SLM) Al–12Si at different temperatures. Technologies, 2016, vol. 4, pp. 38–46.
  18. Wang Z., Prashanth K.G., Scudino S. et al. Tensile properties of Al matrix composites reinforced with in situ devitrified Al84Gd6Ni7Co2 glassy particles. Alloys Compounds, 2014, vol. 586, pp. 419–422.
  19. Siddique S., Imran M., Walther F. Very high cycle fatigue and fatigues crack propagation behavior of selective laser melted AlSi12 alloy. International Journal of Fatigue, 2017, vol. 94, pp. 246–254.
  20. Handbook of Aluminum, vol. 2: Alloy Production and Materials Manufacturing. Eds. G.E. Totten, D.S. MacKenzie. CRC Press: Boca Raton, 2003. 736 p.
  21. Wang D., Yang Y., Chen Y. Study on energy input and its influences on single-track, multi-track, and multi-layer in SLM. International Journal of Advanced Manufacturing Technology, 2012, vol. 58, pp. 1189–1199.
  22. Wang P., Eckert J., Prsahanth K.G. et al. A review of particles-reinforced aluminum matrix composites fabricated by selective laser melting. Transactions of Nonferrous Metals Society of China, 2020, vol. 30, pp. 2001–2034.
  23. Vilaro T., Kottman-Rexerodt V., Thomas M. et al. Direct fabricated of a Ti–47Al–2Cr–2Nb alloy by selective laser melting and direct metal deposition processes. Advanced Materials Research, 2010, vol. 89, pp. 586–591.
  24. Culha O., Tekmen C., Toparli M., Tsunekawa Y. Mechanical properties of in situ Al2O3 formed Al–Si composite coating via atmospheric plasma spraying. Materials and Design, 2010, vol. 31, pp. 533–544.
  25. Wu J., Wang X.Q., Wang W. et al. Microstructure and strength of selectively laser melted AlSi10Mg. Acta Materials, 2016, vol. 117, pp. 311–320.
  26. Prashanth K.G. Work hardening in selective laser melted Al–12Si alloy. Materials Design Processing Communications, 2019, vol. 1 (2), art. e46.
  27. Zhang H., Zhu H., Nie X. et al. Fabrication and heat treatment of high strength Al–Cu–Mg alloy processed using selective laser melting. International Society for Optics and Photonics, 2016. DOI: 10.1117/12.2211362.
  28. Casati R., Lemke J.N., Alarcon A.Z., Vedani M. Aging behavior of high-strength Al Alloy 2618 produced by selective laser melting. Metallurgical and Materials Transactions A, 2017. Vol. 48 (2), pp. 575–579.
  29. Kotadia H.R., Gibbons G., Das A., Howes P.D. A review of laser powder bed fusion additive manufacturing of aluminium alloys: Microstructure and properties. Additive Manufacturing, 2021, vol. 46, pp. 1–23.
  30. Tan Q., Zhang J., Sun Q. et al. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles. Acta Materials, 2020, vol. 196, pp. 1–16.
  31. Wang P., Gammer C., Brenne F. et al. Microstructure and mechanical properties of a heat-treatable Al–3.5Cu–1.5Mg–1Si alloy produced by selective laser melting. Materials Science and Engineering A, 2018, vol. 711, pp. 562–570.
  32. Zhang H., Zhu H., Nie X. et al. Effect of zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al–Cu–Mg alloy. Scripta Materialia, 2017, vol. 134, pp. 6–10.
  33. Shchetinina N.D., Kuznetsova P.E., Dynin N.V., Selivanov A.A. Aluminum alloys with additions of Sc and Zr IN additive manufacturing (review) Aviation materials and technologies, 2021, no. 3 (64), paper no. 03. Available at: http://www.journal.viam.ru (accessed: October 22, 2022). DOI: 10.18577/2713-0193-2021-0-3-19-34.
  34. Li R., Wang M., Li Z. et al. Developing a high-strength Al–Mg–Si–Sc–Zr alloy for selective laser melting: crack-inhibiting and multiple strengthening mechanisms. Acta Materials, 2020, vol. 193, pp. 83–98.
  35. Li X.P., Wang X.J., Saunders M. et al. A selective laser melting and solution heat treatment refined Al–12Si alloy with a controllable ultrafineeutectic microstrcuture and 25 % tensile ductility. Acta Materialia, 2015, vol. 95, pp. 74–82.
  36. Kaufmann N., Imran M., Wischeropp T.M. et al. Influence of process parameters on the quality of aluminium alloy EN AW 7075 using selective laser melting (SLM). Physics Procedia, 2016, vol. 83, pp. 918–926.
  37. Martin J.H., Yahata B.D., Hundley J.M. et al. 3D printing of high-strength aluminium alloys. Nature, 2017, vol. 549, pp. 365–369.