The methodological features of testing on fire resistance the samples with intumescent coatings

Volnyj O.S., Barbotko S.L., Venediktova M.A., Lutsenko A.N.
Volnyj O.S., Barbotko S.L., Venediktova M.A., Lutsenko A.N. The methodological features of testing on fire resistance the samples with intumescent coatings // Proceedings of VIAM. 2022. No. 9. DOI: 10.18577/2307-6046-2022-0-9-131-142. URL: https://www.viam-works.ru/en/journal/2022/9/11
Keywords
fire resistance, fire proof, fire test, fire safety, intumescent coating, fire retardant coating
Abstract

Fire tests were carried out to determine the effectiveness of the fire-retardant intumescent coating. It has been established that the standard methodology for conducting fire tests does not provide adequate reproducible results. A modification of the methodology was proposed and a large number of samples (˃30) were tested. It has been established that when using a modified test procedure, high reproducibility of the results obtained is ensured.

Reference list
  1. About fire safety: Federal Law (December 21, 1994, No. 69-FZ). Available at: https: //www.consultant.ru/document/cons_doc_LAW_5438/ (accessed: February 01, 2022).
  2. Technical regulations on fire safety requirements: Feder. Law (July 22, 2008, No. 123-FZ). Available at: https://docs.cntd.ru/document/902111644 (accessed: February 01, 2022).
  3. The list of national standards containing the rules and methods of research (testing) and measurements, including the rules for sampling, necessary for the application and execution of the Federal Law "Technical Regulations on Fire Safety Requirements" and the implementation of conformity assessment: Order of the Government of the Russian Federation of (March 10, 2009, No. 304-r). Available at: https://docs.cntd.ru/document/902146883 (accessed: February 01, 2022).
  4. Airworthiness standards for transport category aircraft: AP-25: approved. Decree of the 28th session of the Council on Aviation and the Use of Airspace on 11.12.2008. 3rd ed. with amendments 1-6. Moscow: Aviaizdat, 2009, 267 p.
  5. Airworthiness Standards: Transport Category Airplanes: Part 25. Code of Federal Regulation. Available at: https://www.ecfr.gov/cgi-bin/text-idx?SID=9091f0ebbfbf1539cdb87015908ad369&mc=true&node=pt14.1.25&rgn=div5 (accessed: February 01, 2022).
  6. Barbotko S.L., Volny O.S., Kirienko O.A., Shurkova E.N. Evaluation of the fire safety of polymeric materials for aviation purposes: state analysis, test methods, development prospects, methodological features. Ed. E.N. Kablov. Moscow: VIAM, 2018, 424 p.
  7. Aircraft Materials Fire Test Handbook: Report DOT/FAA/AR-00/12. Federal Aviation Administration. Atlantic City, 2000, 234 p. Available at: https://www.abbottaerospace.com/downloads/
  8. dot-faa-ar-00-12-aircraft-materials-fire-test-handbook/ (accessed: February 01, 2022).
  9. Fire Protection: Systems: AC 25.869-1A. Aircraft Certification Service, Transport Airplane Directorate. 2007, 11 p. Available at: https://www.faa.gov/regulations_policies/advisory_circulars/index.cfm/go/document.information/documentID/74393 (accessed: February 10, 2022).
  10. Certification of Electrical Wiring Interconnection Systems on Transport Category Airplanes: AC 25.1701-1. Aircraft Certification Service, Transport Airplane Directorate, 2007, 92 p. Available at: https://www.faa.gov/regulations_policies/advisory_circulars/index.cfm/go/document.information/documentID/73476 (accessed: February 10, 2022).
  11. Engine fire Protection: AC 33.17-1A. Aircraft Certification Service Engine & Propeller Directorate – Rulemaking & Policy, 2009, 12 p. Available at: https://www.faa.gov/regulations_policies/advisory_circulars/index.cfm/go/document.information/documentID/99608 (accessed: February 10, 2022).
  12. Powerplant Installation and Propulsion System Component Fire Protection Test Methods, Standards, and Criteria: AC 20-135. Policy and Innovation Division, 1990, 18 p. Available at: https://www.faa.gov/regulations_policies/advisory_circulars/index.cfm/go/document.information/documentID/22194 (accessed: February 10, 2022).
  13. Certification Specifications and Acceptable Means of Compliance for Large Aeroplanes: CS-25. 2020. URL: https://www.easa.europa.eu/sites/default/files/dfu/CS-25%20Amendment%2024.pdf (accessed: February 01, 2022).
  14. Revised Power Plant Engineering Report No. 3A. Standard Fire Test Apparatus and Procedure (For Flexible Hose Assemblies): AC 20-104. Aviation Safety – Aircraft Certification Service, Aircraft Engineering Division, 1978, 35 p. Available at: https://www.faa.gov/regulations_policies/advisory_circulars/index.cfm/go/document.information/documentID/22049/ Available at: https://www.faa.gov/regulations_policies/advisory_circulars/index.cfm/go/document.information/documentID/22049 (accessed: February 01, 2022).
  15. Barbotko S.L., Kirienko O.A., Volny O.S., Lutsenko A.N. Fire hazard analysis of aircraft engine nacelles and other fire hazardous areas; used methods of fire testing of materials and structural elements for compliance with the requirements of aviation standards. Problemy bezopasnosti poletov, 2017, no. 5, p. 3–24.
  16. ISO 2685:1998(E). Aircraft – Environmental test procedure for airborne equipment – Resistance to fire in designated fire zones. International Standard Organization, 1998, 34 p.
  17. Le Neve S. Fire behavior of structural composite materials. 5th International Aircraft Fire and Cabin Safety Research Conference. Atlantic City, 2007, 27 p.
  18. Le Neve S. Fire behavior of structural composite materials (progress in the work). 6th International Aircraft Fire and Cabin Safety Research Conference. 2010, 39 p.
  19. Le Neve S. AC 20-135 / ISO 2685 Fire tests on components used in fire zones. Comparison of gas burner to oil burner. Proceedings of the FAA Materials Meeting. Atlantic City, 2008, 26 p.
  20. Development of Next Generation Burner Characteristics for Fire Testing of Power Plant Materials and Components: Report DOT/FAA/TC-13/38 / Department of Aerospace Engineering and Engineering Mechanics University of Cincinnati. Cincinnati, 2015, 52 p.
  21. Laborie D. Fire Test Burner Evaluation. International Aircraft Systems Fire Protection Working Group Meeting. Atlantic City, 2015, 8 p.
  22. Kablov E.N. New generation materials and technologies for their digital processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, vo. 2, pp. 225–228.
  23. Kablov E.N. Marketing of materials science, aircraft building and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5–6, pp. 40–44.
  24. Kablov E.N. Materials are the basis of any business. Delovaya Slava Rossii, 2013, no. 2, pp. 4–9.
  25. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  26. Venediktova M.A., Petrova A.P., Barbotko S.L., Bryk Yа.A. Application of new environmentally friendly organophosphorus flame retardants in the composition of heat-protective putty. Trudy VIAM, 2020, no. 9 (91), paper no. 04. Available at: http://www.viam-works.ru (accessed: February 24, 2022). DOI: 10.18577/2307-6046-2020-0-9-35-43.
  27. Venediktova M.A., Evdokimov A.A., Kras- nov L.L., Petrova A.P. Research of possibility of application of fireproof paste for increase of fire safety of designs from polymeric composite materials. Trudy VIAM, 2021, no. 9 (103), paper no. 07. Available at: http://www.viam-works.ru (accessed: February 24, 2022). DOI: 10.18577/2307-6046-2021-0-9-67-75.
  28. Antipov V.V. Scientific and technological foundations for the development of a new generation of layered alumina-glass-reinforced plastics with variable physical and mechanical properties based on low-density aluminum-lithium alloy sheets: thesis abstract, Dr. Sc. (Tech.). Samara: Samara State Tech. Univarsity, 2021, 44 p.
  29. Barbotko S.L., Volny O.S., Bochenkov M.M. Methods for assessing the fire hazard of heat-fireproof materials. Materialy All-Rus. Sci.-tech. conf. "Fundamental and applied research in the field of sealing, sealing and fire-protective materials". Moscow: VIAM, 2019, pp. 105–118.
  30. Fire safety: RTs-AP 33.17 / Interstate Aviation Committee. Aviation Register. Moscow: IAC, 2005, 15 p.
  31. Barbotko S.L., Volny O.S., Veshkin E.A., Goncharov V.A. Evaluation of the fire resistance of materials and structural elements for aviation equipment. Aviatsionnaya promyshlennost, 2018, no. 2, pp. 63–67.
  32. Barbotko S.L., Volnyy O.S., Kiriyenko O.A., Shurkova E.N. Creation of the mathematical model and calculation of sample temperatures at tests on fire resistance. Trudy VIAM, 2017, no. 7 (55), paper no. 12. Available at: http://www.viam-works.ru (accessed: February 01, 2022). DOI: 10.18577/2307-6046-2017-0-7-12-12.
  33. Garashchenko A.N., Kulkov A.A., Strakhov V.L. The effect of the service life on the flame-retardant efficiency of the bulging coatings and the fire resistance of structures. Aviation materials and technologies, 2022, no. 2 (67), paper no. 09. Available at: http://www.journal.viam.ru (accessed: June 29, 2022). DOI: 10.18577/2713-0193-2022-0-2-97-110.