The basic principles of creation of formula cold-resistant rubbers stock for the products maintained in the conditions of the arctic climate (review)

Vakhrusheva Ja.A., Yumashev O.B., Chaykun A.М.
Vakhrusheva Ja.A., Yumashev O.B., Chaykun A.М. The basic principles of creation of formula cold-resistant rubbers stock for the products maintained in the conditions of the arctic climate (review) // Proceedings of VIAM. 2022. No. 8. DOI: 10.18577/2307-6046-2022-0-8-77-87. URL: https://www.viam-works.ru/en/journal/2022/8/6
Keywords
rubber, cold resistance rubber, ozone-resistance rubber, polar rubber, non-polar rubber.
Abstract

The article is devoted to the analysis of current trends necessary in the creation of rubber compound formulations for special-purpose rubber products, operable under conditions of prolonged exposure to low temperatures. The main operational characteristics of rubbers based on polar and non-polar rubbers are given. The results of new research by scientists from the National research center «Kurchatov institute» state research center of the Russian Federation on the creation of elastomeric materials for work under conditions of prolonged exposure to negative temperatures are systematized, the features of creating frost-resistant rubber are described, and an analysis of the main options for choosing the required ratio of rubbers and ingredients is carried out.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Reports of XX Mendeleevsky Congress for General and Applied Chemistry: in 5 vols. Ekaterinburg: UB of RAS, 2016, vol. 3, pp. 25–26.
  3. Kablov E.N. The sixth technological way. Nauka i zhizn, 2010, no. 4, pp. 2–7.
  4. History of aviation materials science. VIAM – 80 years: years and people. Ed. E.N. Kablov. M.: VIAM, 2012, pp. 346–348.
  5. Kablov E.N. Airospace materials science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
  6. The Big Reference Book for Specialist in Rubbers: in 2 parts. Moscow: Tekhinform, 2012. 1385 p.
  7. Technology of rubber: recipe and testing: trans. from Engl. Ed. J.S. Dik. St. Petersburg: Scientific foundations and technologies, 2010, 620 p.
  8. Fedyukin D.P., Makhlis F.A. Technical and technological properties of razin. Moscow: Khimiya, 1985, 240 p.
  9. Makhlis F.A., Fedyukin D.L. Terminological reference for rubber. Moscow: Khimiya, 1989, 400 p.
  10. Kornev A.E., Bukanov A.M., Sheverdaev O.N. Technology of elastomeric materials. Moscow: East, 2009, 502 p.
  11. Agayants I.M. Five centuries of rubber and rubber. Moscow: Modern-A, 2002, 432 p.
  12. Koshelev F.F., Kornev A.E., Bukanov A.M. General technology of rubber. 4th ed. Moscow: Khimiya, 1978, 528 p.
  13. Ososhnik I.A., Shutilin Yu.F., Karmanova O.V. Production of rubber technical products. Voronezh: Voronezh State Technology Academy, 2007, 972 p.
  14. Grishin B.S. Materials of the rubber industry (information and analytical database): in 2 vols. Kazan: KSTU, 2010, vol. 1, 596 p.
  15. Rubber and resin. Science and technology. Ed. J. Mark, B. Erman, F. Eirich; trans. from English. Ed. A.A. Berlin, Yu.L. Morozova. Dolgoprudny: Intelligence, 2011, 768 p.
  16. Nudelman Z.N. Poftorcacus: basics, processing, application. Moscow: RIAS, 2007, 383 p.
  17. Semenova S.N., Chaykun A.M., Suleymanov R.R. Ethylene-propylene-diene rubber and its use in rubber materials for special purposes (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 23–30. DOI: 10.18577/2071-9140-2019-0-3-23-30.
  18. Semenova S.N., Suleymanov R.R., Chaykun A.M. Mixing ethylene-propylene-diene and methylphenylsiloxane rubbers in the formulation of cold and ozone resistant rubber. Trudy VIAM, 2019, no. 9 (81), paper no. 07. Available at: http://www.viam-works.ru (accessed: June 14, 2022). DOI: 10.18577/2307-6046-2019-0-9-64-72.
  19. Shuldeshov E.M. Sound-proof properties of aviation heatsound-proof materials. Trudy VIAM, 2019, no. 12 (84), paper no. 05. Available at: http://www.viam-works.ru (accessed: June 14, 2022). DOI: 10.18577/2307-6046-2019-0-12-37-45.
  20. Semenova S.N., Chaikun A.M., Suleimanov R.R. The influence of the vulcanizing system on the temperature properties of rubber based on ethylenepropylene rubber. Kauchuk i rezina, 2020, vol. 79, no. 4, pp. 210–213.
  21. Semenova S.N., Chaykun A.M. Highly heat-resistant silicone rubber compositions (review). Trudy VIAM, 2020, no. 11 (93), paper no. 04. Available at: http://www.viam-works.ru (accessed: June 14, 2022). DOI: 10.18577/2307-6046-2020-0-11-31-37.
  22. Chaykun A.M., Eliseev O.A., Naumov I.S., Venediktova M.A. Compounding principles in the field of frost resistant rubbers. Aviacionnye materialy i tehnologii, 2013, no. 3, pp. 53–55.
  23. The norms of flight fit of the transport category aircraft: AP-25: approved by a resolution of the 28th session of the Council for Aviation and the use of airspace on 11.12.2008. 3rd ed. with amendments 1–6. Moscow: Aviazdat, 2009, 267 p.
  24. Efimov V.A., Shvedkova A.K., Korenkova T.G., Kirillov V.N. Research of polymeric constructional materials at influence of climatic factors and loadings in laboratory and natural conditions. Trudy VIAM, 2013, no. 1, paper no. 05. Available at: http://viam-works.ru (accessed: June 14, 2022).
  25. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Prospects for the use of carbon-containing nanoparticles in binders for polymer composite materials. Rossiyskiye nanotekhnologii, 2013, vol. 8,
  26. no. 3-4, pp. 24–42.
  27. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climate aging of composite aviation materials. III. Significant aging factors. Deformatsiya i razrusheniye materialov, 2011, no. 1, pp. 34–40.
  28. Zemsky D.N., Chirkova Yu.N. New ingredients of rubber mixtures. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2013, vol. 16, no. 12, pp. 143–145.
  29. Compositional oil- and gas-resistant, frozen-resistant material: pat. 2437903 Rus. Federation; filed 114.04.08; publ. 27.12.11.
  30. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  31. Eliseev O.A., Krasnov L.L., Zajceva E.I., Savenkova A.V. Development and modifying of elastomeric materials for application in all weather conditions. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 309–314.
  32. Chaikun A.M., Eliseev O.A., Naumov I.S., Venediktova M.A. Features of old-resistant rubbers on the basis on different unvulcanized rubbers. Trudy VIAM, no. 12, paper no. 04. Available at: http://www.viam-works.ru (accessed: June 14, 2022).
  33. Erasov V.S., Kotova E.A. Erosion resistance of aviation materials to influence of solid (dust) particles. Aviacionnye materialy i tehnologii, 2011, no. 3, pp. 30–36.
  34. Kablov E.N. Chemistry in aviation material science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 3–4.
  35. Chernsky I.N., Popov S.N., Goldstrakh I.Z. Design and calculation of frost-resistant mobile seals. Novosibirsk: Nauka, 1992, 123 p.
  36. Technology of rubber: recipe and testing. Ed. J.S. Savage; trans. from English. Ed. V.A. Shershnev. St. Petersburg: Scientific foundations and technologies, 2010, 620 p.
  37. Kargin V.A. Encyclopedia of polymers: in 3 vols. Moscow: Sovetskaya Entsiklopediya, 1972, vol. 1: A–K, 609 p.
  38. Petrova N.N., Portnyagina V.V., Fedotova E.S. The prospects for the use of a new plasticizer of diboxyeladipinate for the production of rubberous intelligence with increased frost resistance. Kauchuk i rezina, 2008, no. 2, pp. 18–22.
  39. Portnyagina V.V., Sokolova M.D., Petrova N.N. et al. Modification of rubberizes by natural zeolites when creating frost-resistant seals of the mining technique of the North. Gorny informatsionno-analiticheskiy byulleten, 2012, no. 11, pp. 392–401.
  40. Sokolova M.D., Davydova M.L., Shadrinov N.V., Morova L.Ya. Development of elastomeric nanocomposites for sealing for the technique of the North. Izvestiya Samarskogo nauchnogo
  41. tsentra RAN, 2011, vol. 13, no. 1 (2), pp. 397–401.
  42. Wound-resistant mixture based on propylene radiation rubber: pat. 2294346 Rus. Federation; filed 20.05.05; publ. 27.02.07.
  43. Tseolithic frost -resistant rubber mixture: pat. 2326903 Rus. Federation; filed 31.08.06; publ. 20.06.08.
  44. A rubber mixture modified by the composition of super-molecular weight polyethylene and magnesium nanoshpinel: pat. 2425851 Rus. Federation; filed 09.03.11; publ. 10.08.11.
  45. Savelyev A.V., Vrukova V.G. The effect of fillers on adhesive strength of incompatible polymers. Kauchuk i rezina, 1986, no. 9, p. 31.
  46. Zaikin A.E., Galikhanov M.F., Archireev V.P. The effect of the filler on the thermodynamic stability of polymer mixtures. Vysokomolekulyarnyye soyedineniya, Ser.: B, 1997, vol. 39, no. 6, pp. 1060–1063.
  47. Davydova M.L., Sokolova M.D. A promising technological method for obtaining polymer –elastomeric material. Voprosy materialovedeniya, 2013, no. 3 (75), pp. 41–47.
  48. Shadrinov N.V., Sokolova M.D., Okhlopkova A.A. et al. Enhancement of compatibility between ultrahigh-Molecular-Weight polyethylene particles and butadiene-Nitrile rubber matrix with nanoscale ceramic particles and characterization of evolving layer. Bulletin of the Korean Chemical Society, 2013, vol. 34, no. 12, pp. 3762–3766.
  49. Shadrinov N.V., Sokolova D.D. A study of the influence of activated zeolite on the deformation of polymerialstomeric composites by the method of atomic-power microscopy. Materialovedenie, 2014, no. 7, pp. 17–22.
  50. Portnyagina V.V., Petrova N.N., Sibiryakova E.M. Study of the influence of bentonites on the structure and properties of razin based on propylenexide rubber. Works of the IV Eurasian Symposium on the problems of the strength of materials and machines for the regions of the cold climate. Yakutsk, 2008, 1 CD.
  51. Frost-resistant rubber mixture based on propyilentic rubber: pat. 2294341 Rus. Federation; filed 20.05.05; publ. 27.02.07.
  52. Lysova G.A., Dontsov A.A. Hydrated butadien-nitrile rubber. Properties. Recipe. Application: thematic review. Moscow: TsNIITEneftekhim, 1991, 58 p.
  53. Anisimov B.Yu., Dukman A.S., Namnitov N.S., Polyakov S.A. Hydrination of butadien-nitrile rubber. Kauchuk i rezina, 2007, no. 2, p. 32.