Self-organization of conductive networks in thermoplastic materials (review)
Kondrashov S.V., Solovyanchik L.V., Minaeva L.A. Self-organization of conductive networks in thermoplastic materials (review) // Proceedings of VIAM. 2022. No. 8. DOI: 10.18577/2307-6046-2022-0-8-31-48. URL: https://www.viam-works.ru/en/journal/2022/8/3
Keywords
thermoplastics, electrically conductive properties, carbon black, carbon nanotubes, phase segregation, morphology, structure
Abstract
A significant reduction in the percolation threshold of carbon-containing particles in thermoplastic composites can be achieved by distributing the functional filler not over the entire volume of the composite, but only in its part. Regulation of the forces of interaction of functional particles with each other and polymer phases, as well as polymer phases among themselves, by choosing a filler, its covalent and non-covalent modification, as well as the composition of the polymer mixture is an effective tool for obtaining thermoplastic composites with a given level of functional properties.
Reference list
- Kablov E.N. Chemistry in aviation materials science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 3–4.
- Kablov E.N. Materials of a new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
- Kablov E.N. Aerospace materials science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
- Gurenkov V.M., Gorshkov V.О., Chebotarev V.P., Prudskova Т.N., Andreeva Т.I. Comparative analysis of properties of polyetheretherketone of domestic and foreign production. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 41–47. DOI: 10.18577/2071-9140-2019-0-3-41-47.
- Gulyaev A.I., Medvedev P.N., Sbitneva S.V., Petrov A.A. Experimental research of «fiber–matrix» adhesion strength in carbon fiber epoxy/polysulphone composite. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 80–86. DOI: 10.18577/2071-9140-2019-0-4-80-86.
- Kablov E.N., Kulagina G.S., Zhelezina G.F., Lonskii S.L., Kurshev E.V. Microstructure research of the unidirectional organoplastic based on Rusar-NT aramid fibers and epoxy-polysulfone binder. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 19–26. DOI: 10.18577/2071-9140-2020-0-4-19-26.
- Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2021, no. 4 (65), paper no. 04. Available at: http://www.journal.viam.ru (accessed: May 12, 2022). DOI: 10.18577/2071-9140-2022-0-1-41-50.
- Joshi S., Rawat K., Karunakaran C. et al. 4D printing of materials for the future: opportunities and challenges. Applied Materials Today, 2020, vol. 18, p. 100490.
- Khosravani M.R., Reinicke T. Applications of additive manufacturing in fabrication of sensors – A review. Sensors and Actuators A: Physical, 2020, vol. 305, no. 4, pp. 111916.
- Adohi B.P., Mdarhri A., Prunier C. et al. A comparison between physical properties of carbon black-polymer and carbon nanotubes-polymer composites. Journal of Applied Physics, 2010, vol. 108, no. 7, p. 074108.
- Zhang Q., Wang J., Zhang B.Y. et al. Improved electrical conductivity of polymer/carbon black composites by simultaneous dispersion and interaction-induced network assembly. Composites Science and Technology, 2019, vol. 179, pp. 106–114.
- Havlin S., Bunde A. Percolation II. Fractals and disordered systems. Berlin; Heidelberg: Springer, 1991, pp. 97–150.
- Stauffer D., Aharony A. Introduction to percolation theory. Rev. second ed. London: CRC press, 2014, 192 p.
- Shevchenko V.G. Fundamentals of physics of polymer composite materials: textbook. Moscow: MGU, 2010, 98 p.
- Influence of thermo-rheological history on electrical and rheological properties of polymer–carbon nanotube composites. Polymer–Carbon Nanotube Composites: Preperetion, properties and applications. Ed. T. McNally, P. Pötschke. Woodhead Publising, 2011, pp. 295–328.
- Bauhofer W., Kovacs J.Z. A review and analysis of electrical percolation in carbon nanotube polymer composites. Composites science and technology, 2009, vol. 69, no. 10, pp. 1486–1498.
- McLachlan D.S., Heaney M.B. Complex ac conductivity of a carbon black composite as a function of frequency, composition, and temperature. Physical Review B, 1999, vol. 60, no. 18, pp. 12746.
- Barrau S., Demont P., Peigney A. et al. DC and AC conductivity of carbon nanotubes – polyepoxy composites. Macromolecules, 2003, vol. 36, no. 14, pp. 5187–5194.
- Fu Y., Liu L., Zhang J. Manipulating dispersion and distribution of graphene in PLA through novel interface engineering for improved conductive properties. ACS applied materials & interfaces, 2014, vol. 6, no. 16, pp. 14069–14075.
- Kirkpatrick S. Percolation and conduction. Reviews of modern physics, 1973, vol. 45, no. 4, pp. 574.
- Dyre J.C., Schrøder T.B. Universality of ac conduction in disordered solids. Reviews of Modern Physics, 2000, vol. 72, no. 3, pp. 873–892.
- Elastomer–carbon nanotube composites. Polymer–Carbon Nanotube Composites: Preperetion, properties and applications. Ed. T. McNally, P. Pötschke. Woodhead Publising, 2011,
- pp. 193–229.
- Kanbur Y., Küçükyavuz Z. Electrical and mechanical properties of polypropylene/carbon black composites. Journal of Reinforced Plastics and Composites, 2009, vol. 28, no. 18, pp. 2251–2260.
- Meincke O., Kaempfer D., Weickmann H. et al. Mechanical properties and electrical conductivity of carbon-nanotube filled polyamide-6 and its blends with acrylonitrile/butadiene/styrene. Polymer, 2004, vol. 45, no. 3, pp. 739–748.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Sumita M., Sakata K., Asai S. et al. Dispersion of fillers and the electrical conductivity of polymer blends filled with carbon black. Polymer bulletin, 1991, vol. 25, no. 2, pp. 265–271.
- Sumita A., Sakata K., Hayakawa Y. et al. Double percolation effect on the electrical conductivity of conductive particles filled polymer blends. Colloid and Polymer Science, 1992, vol. 270, no. 2, pp. 134–139.
- Gupta S., Ou R., Gerhardt R.A. Effect of the fabrication method on the electrical properties of poly (acrylonitrile-co-butadiene-co-styrene)/carbon black composites. Journal of Electronic Materials, 2006, vol. 35, no. 2, pp. 224–229.
- Mamunya Y.P., Lebovka N.I., Lisunova M.O. et al. Conductive polymer composites with ultralow percolation threshold containing carbon nanotubes. Journal of Nanostructured Polymers and Nanocomposites, 2008, vol. 4, no. 1, pp. 21–27.
- Grunlan J., Mehrabi A., Bannon M. et al. Water‐based single‐walled‐nanotube‐filled polymer composite with an exceptionally low percolation threshold. Advanced Materials, 2004, vol. 16, no. 2, pp. 150–153.
- Grossiord N., Loos J., van Laake L. et al. High‐Conductivity Polymer Nanocomposites Obtained by Tailoring the Characteristics of Carbon Nanotube Fillers. Advanced Functional Materials, 2008, vol. 18, no. 20, pp. 3226–3234.
- Miriyala S.M., Kim Y.S., Liu L. et al. Segregated networks of carbon black in poly(vinyl acetate) latex: influence of clay on the electrical and mechanical behavior. Macromolecular Chemistry and Physics, 2008, vol. 209, no. 23, pp. 2399–2409.
- Deng H., Lin L., Ji M. et al. Progress on the morphological control of conductive network in conductive polymer composites and the use as electroactive multifunctional materials. Progress in Polymer Science, 2014, vol. 39, no. 4, pp. 627–655.
- Carbon nanotubes in multiphase polymer blends. Polymer–Carbon Nanotube Composites: Preperetion, properties and applications. Ed. T. McNally, P. Pötschke. Woodhead Publising, 2011, pp. 587–620.
- Pötschke P., Pegel S., Claes M. et al. A novel strategy to incorporate carbon nanotubes into thermoplastic matrices. Macromolecular Rapid Communications, 2008, vol. 29, no. 3, pp. 244–251.
- Volkov V.A. Colloidal chemistry. Surface phenomena and dispersed systems. St. Petersburg: Lan, 2015, 672 p.
- Wu S. Polymer interface and adhesion. Routledge, 2017, 630 р.
- Pan Y. Electrical, Morphological and Rheological Properties of Carbon Black Filled Polymer Blends: Dis. Erlangen: Friedrich-Alexander-Universitat Erlangen-Nurnberg (FAU), 2017, 123 p.
- Chen J., Shi Y.Y., Yang J.H. et al. A simple strategy to achieve very low percolation threshold via the selective distribution of carbon nanotubes at the interface of polymer blends. Journal of Materials Chemistry, 2012, vol. 22, no. 42, pp. 22398–22404.
- Al-Saleh M.H., Sundararaj U. An innovative method to reduce percolation threshold of carbon black filled immiscible polymer blends. Composites. Part A: Applied Science and Manufacturing, 2008, vol. 39, no. 2, pp. 284–293.
- Gubbels F., Jеrоme R., Teyssie P. et al. Selective localization of carbon black in immiscible polymer blends: a useful tool to design electrical conductive composites. Macromolecules, 1994, vol. 27, no. 7, pp. 1972–1974.
- Nair S.T., Vijayan P.P., Xavier P. et al. Selective localisation of multi walled carbon nanotubes in polypropylene/natural rubber blends to reduce the percolation threshold. Composites Science and Technology, 2015, vol. 116, pp. 9–17.
- Bose S., Bhattacharyya A.R., Bondre A.P. et al. Rheology, electrical conductivity, and the phase behavior of cocontinuous PA6/ABS blends with MWNT: Correlating the aspect ratio of MWNT with the percolation threshold. Journal of Polymer Science. Part B: Polymer Physics, 2008, vol. 46, no. 15, pp. 1619–1631.
- Hu J., Zhang H.B., Hong S. et al. Simultaneous improvement in both electrical conductivity and toughness of polyamide 6 nanocomposites filled with elastomer and carbon black particles. Industrial & Engineering Chemistry Research, 2014, vol. 53, no. 6, pp. 2270–2276.
- Pang H., Xu L., Yan D.X. et al. Conductive polymer composites with segregated structures. Progress in Polymer Science, 2014, vol. 39, no. 11, pp. 1908–1933.
- Garmabi H., Naficy S. Developing electrically conductive polypropylene/polyamide6/carbon black composites with microfibrillar morphology. Journal of applied polymer science, 2007, vol. 106, no. 5, pp. 3461–3467.
- Fenouillot F., Cassagnau P., Majesté J.C. Uneven distribution of nanoparticles in immiscible fluids: Morphology development in polymer blends. Polymer, 2009, vol. 50, no. 6, pp. 1333–1350.
- Gubbels F., Jerome R., Vanlathem E. Kinetic and thermodynamic control of the selective localization of carbon black at the interface of immiscible polymer blends. Chemistry of materials, 1998, vol. 10, no. 5, pp. 1227–1235.
- Huang J., Mao C., Zhu Y. et al. Control of carbon nanotubes at the interface of a co-continuous immiscible polymer blend to fabricate conductive composites with ultralow percolation thresholds. Carbon, 2014, vol. 73, pp. 267–274.
- Li H., Tuo X., Yan G. et al. Comparison of Three Interfacial Conductive Networks Formed in Carbon Black-Filled PA6/PBT Blends. Polymers, 2021, vol. 13, no. 17, p. 2926.
- Göldel A., Marmur A., Kasaliwal G.R. et al. Shape-dependent localization of carbon nanotubes and carbon black in an immiscible polymer blend during melt mixing. Macromolecules, 2011, vol. 44, no. 15, pp. 6094–6102.