Production of single-crystal castings with a given axial and azimuthal orientations
Toloraya V.N., Ostroukhova G.A. Production of single-crystal castings with a given axial and azimuthal orientations // Proceedings of VIAM. 2022. No. 8. DOI: 10.18577/2307-6046-2022-0-8-3-13. URL: https://www.viam-works.ru/en/journal/2022/8/1
Keywords
seed, turbine blade, single-crystal structure, crystallographic orientation (CGO), axial CGO, azimuthal CGO, metallographic and diffractometric method
Abstract
Deals with the issues of determining and evaluating the crystallographic orientation (CGO) of single-crystal castings from nickel heat-resistant alloys obtained by the method of directed crystallization. The methods of setting the axial and azimuthal CGO in castings using seed crystals (seedings) from alloys of the Ni–W system are described. Presents methods for obtaining castings of turbine blades with a single-crystal structure of a given spatial orientation , which allows significantly reducing the level of thermal stresses for cooled blades.
Reference list
- Kablov E.N., Toloraya V.N., Demonis I.M., Orekhov N.G. Directed crystallization of heat-resistant nickel alloys. Tekhnologiya legkikh splavov, 2007, no. 2, pp. 60–70.
- Toloraya V.N., Kablov E.N., Demonis I.M. The technology for obtaining monocrystalline castings of turbine blades of the GTD of a given crystallographic orientation from rinis-containing heat-resistant alloys. Foundry heat-resistant alloys. The effect of S.T. Kishkin. Mosocw: Nauka, 2006, pp. 206–218.
- Petrushin N.V., Ospennikova O.G., Svetlov I.L. Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 72−103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
- Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: June 24, 2021). DOI: 10.18577/2307-6046-2020-0-3-3-12.
- Copley S.M., Kear B.H. Temperature and Orientation Dependence of the Flow Stress of Stoichiometric Ni3al (γ'-phase). Materials Science and Engineering, 1972, vol. 10, pp. 87–95.
- Svetlov I.L., Sukhanov N.N., Krivko A.I. The temperature-oriented dependence of the characteristics of short-term strength, the youth module and the linear expansion of the ZhS6F monocristals. Problemy prochnosti, 1987, no. 4, pp. 51–56.
- Svetlov I.L., Epishin A.I., Krivko A.I. Anisotropy of the Poisson of the Nickel alloy monocrystals. Dan USSR, 1988, vol. 302, no. 6, pp. 1372–1375.
- Krivko A.I., Epishin A.I., Svetlov I.L., Samoilov A.I. Calculation of thermal stresses and thermal resistance of anisotropic materials. Message I. Problemy prochnosti, 1989, no. 2, pp. 3–9.
- Krivko A.I., Epishin A.I., Svetlov I.L., Samoilov A.I. Calculation of thermal stresses and thermal resistance of anisotropic materials. Message II. Problemy prochnosti, 1989, no. 4, pp. 43–48.
- Dalnev R.A., Svetlov I.L., Bychkov N.G. Orientation dependence of thermal fatigue of nickel
- alloy monocrinists. Problemy prochnosti, 1988, no. 11, pp. 3–9.
- Shalin R.E., Svetlov I.L., Kachanov E.B., Toloraya V.N., Gavrilin O.S. Monocrystals of nickel heat-resistant alloys. Moscow: Mashinostroyenie, 1997, pp. 162–166.
- Toloraya V.N., Kablov E.N., Orekhov N.G., Ostroukhova G.A. The structure and growth defects of the monocristals of nickel heat-resistant alloys. Gorny informatsionno-analiticheskiy byulleten, 2005, no. S5, pp. 190–202.
- Kuzmina N.A., Lifshits V.A., Potrakhov E.N., Potrakhov N.N. Comparative structure control of single-crystal castings of nickel superalloys x-ray diffraction methods of oscillation and Laue. Trudy VIAM, 2019, no. 9 (81), paper no. 02. Available at: http://www.viam-works.ru (accessed: December 4, 2021). DOI: 10.18577/2307-6046-2019-0-9-15-25.
- Kuzmina N.A., Pyankova L.A. Control of crystallographic orientation of monocrystalline nickel castings heat-resistant alloys by х-ray diffractometry. Trudy VIAM, 2019, no. 12 (84), paper no. 02. Available at: http://www.viam-works.ru (accessed: December 4, 2021). DOI: 10.18577/2307-6046-2019-0-12-11-19.
- Nazarkin R.M. Small-sized x-ray diffractometers for structure and phase analysis purposes