High strength corrosion resistant steel VNS-74 as applied to aircraft fasteners

Tonysheva О.А., Voznesenskaya N.M., Gromov V.I., Leonov A.V.
Tonysheva О.А., Voznesenskaya N.M., Gromov V.I., Leonov A.V. High strength corrosion resistant steel VNS-74 as applied to aircraft fasteners // Proceedings of VIAM. 2022. No. 7. DOI: 10.18577/2307-6046-2022-0-7-3-12. URL: https://www.viam-works.ru/en/journal/2022/7/1
Keywords
corrosion resistant steel, heat treatment, mechanical properties, fasteners
Abstract

The article is devoted to the development of technology for smelting and deformation of VNS-74 (05Kh16N5AB) corrosion resistant steel with an increased nitrogen content (more than 0.10 % by weight). The structure and its influence on the hardness and strength characteristics of calibrated bars (different sections from 6 to 16 mm), made of steel VNS-74 by cold and hot deformation, are considered. The high technological plasticity of thin rods in the cold state, which is necessary for carrying out the operation of cold upsetting of the bolt heads, is shown. The mechanical properties and stress corrosion resistance of cold and hot heading bolts with 8° misalignment under the head and under the screw-nut and without misalignment were studied.

Reference list
  1. Kablov E.N. Without new materials, there is no future. Metallurg, 2013, no. 12, pp. 4–8.
  2. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  3. Kablov E.N. The key problem is materials. Trends and guidelines for Russia's innovative development. Moscow: VIAM, 2015, pp. 458–464.
  4. Yakusheva N.A. High-strength constructional steels for landing gears of perspective products of aircraft equipment. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 3–9. DOI: 10.18577/2071-9140-2020-0-2-3-9.
  5. Chizhevsky N.P. Iron and nitrogen. Tomsk: Typolitography of the Siberian Printing Association, 1914. 91 p.
  6. Bannykh I.O. Influence of alloying on the strength properties and hardening mechanisms of nitrogen-containing austenitic steels after hot deformation and annealing. Metally, 2017, no. 6, pp. 74–80.
  7. Kostina M.V., Bannykh O.A., Blinov V.M. Features of steels alloyed with nitrogen. Metallovedenie i termicheskaya obrabotka metallov, 2000, no. 12, pp. 3–6.
  8. Alekseev V.I. Prospects for the use of structural steels with a superequilibrium nitrogen content under conditions of elevated temperatures and hydrogen pressures. Metally, 2000, no. 4, pp. 47–52.
  9. Artemeva D.A., Anastasiadi G.P. Influence of alloying with nitrogen on the short-term and long-term mechanical properties of steel 07Kh12NMFB. Metallovedeniye i termicheskaya obrabotka metallov, 2018, no. 1, pp. 39–43.
  10. Sevalnev G.S., Antsyferova M.V., Dulnev K.V., Sevalneva T.G., Vlasov I.I. Influence of nitrogen concentration on the structure and properties of sparingly alloyed structural steel. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 10–16. DOI: 10.18577/2071-9140-2020-0-2-10-16.
  11. Tonysheva O.A., Voznesenskaya N.M., Shestakov I.I., Eliseyev E.A. Influence of modes of high-temperature thermomechanical processing on structure and properties of high-strength corrosion-resistant steel of austenitic-martensitic class 17Х13Н4К6САМ3ч. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 11–16. DOI: 10.18577/2307-6046-2017-0-1-11-16.
  12. Bannykh I.O., Bannykh O.A. Current state of research and application of high-nitrogen austenitic steels. Moscow: Nauka i tekhnologii, 2017, 64 p.
  13. Bhav Singh B., Sivakumar K., Balakrishna Bhat T. Effect of cold rolling on mechanical properties and ballistic performance of nitrogen-alloyed austenitic steels. International Journal of Impact Engineering, 2009, vol. 36, pp. 611–620.
  14. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  15. Rashev Ts.V. High nitrogen steels: Metallurgy under pressure. Sofia: Prof. Marin Drinov, 1995, 268 p.
  16. Krylov S.A., Evgenov A.G., Shherbakov A.I., Makarov A.A. New pressure electroslag remelting furnace PESR-0,1: development and prospects for improvement. Trudy VIAM, 2016, no. 5, paper no. 04. Available at: http://www.viam-works.ru (accessed: March 20, 2022). DOI: 10.18577/2307-6046-2016-0-5-4-4.
  17. Tonysheva O.A. Features of the formation of the structure and properties during smelting, heat treatment and plastic deformation of corrosion-resistant weldable chromium-nickel steels alloyed with nitrogen: thesis abstract, Cand. Sc. (Tech.). Moscow: VIAM, 2014, 27 p.
  18. Potak Ya.M., Sagalevich E.A. Structural diagram of wrought stainless steels. Metallovedeniei termicheskaya obrabotka metallov, 1971, no. 9, pp. 12–16.
  19. Goodremont E. Special steels: in 2 vols. Trans. from Germ. 2nd ed., rev. Moscow: Metallurgiya, 1966, vol. 2, p. 1097.
  20. Novikov I.I. Theory of heat treatment of metals. 3rd ed. Moscow: Metallurgiya, 1978, p. 47.