Study of the structure and mechanical properties of fasteners made of VT47 high-strength metastable β-titanium alloy

Arislanov A.A., Putyrskiy S.V., Shiryaev A.A., Volodin А.V., Bratukhin A.V.
Arislanov A.A., Putyrskiy S.V., Shiryaev A.A., Volodin А.V., Bratukhin A.V. Study of the structure and mechanical properties of fasteners made of VT47 high-strength metastable β-titanium alloy // Proceedings of VIAM. 2022. No. 6. DOI: 10.18577/2307-6046-2022-0-6-27-38. URL: https://www.viam-works.ru/en/journal/2022/6/3
Keywords
fasteners, deformation, cold forging, mechanical properties, microstructure, heat treatment
Abstract

The article presents the results of a complex of studies: analysis of the microstructure, determination of mechanical properties under the influence of breaking loads at break, shear, as well as determination of fatigue characteristics at room temperature of fasteners made of VT47 pseudo-β-titanium alloy. A comparative analysis of the obtained research results was carried out, showing the dependence of the mechanical properties of fasteners on the structure. The relevance of the use of VT47 pseudo-β-titanium alloy as material of fasteners is shown.

Reference list
  1. Kablov E.N. Dominant of the national technology initiative. Problems of accelerating the development of additive technologies in Russia. Metally Evrazii, 2017, no. 3, pp. 2–6.
  2. Kablov E.N. What is the future to be made of? Materials of a new generation, technologies for their creation and processing – the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  3. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α + β-titanium alloy based on a system of Ti–Al–Sn–Zr–Si–β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  4. Vlasov A.P. Progressive fasteners. Moscow: Mashinostroenie, 1991, 256 p.
  5. Volodin V.A. Fastening systems for highly loaded aircraft structures. Experience and prospects for use in civil aircraft. CALS International Encyclopedia. Aerospace engineering. Moscow: NITs ASK, 2015, pp. 125–128.
  6. Volodin V.A., Bratukhin V.A. Technological features of the manufacture of fastening systems for joining composite materials. Trudy NGTU im. R.Ye. Alekseyeva, 2017, no. 2 (117), pp. 113–117.
  7. Panin P.V., Nochovnaya N.A., Kablov D.E., Alekseev E.B., Shiryaev A.A., Novak A.V. A practical guide to the metallography of alloys based on titanium and its intermetallic compounds: textbook. allowance. Ed. E.N. Kablov. Moscow: VIAM, 2020, 200 p.
  8. Lyasotskaya V.S. Heat treatment of welded joints of titanium alloys. Moscow: Ecomet, 2003. 352 p.
  9. Nochovnaya N.A. Research of the influence of parameters of isothermal deformation and heat treatment on structure and mechanical properties punchings from alloy VT6ch. Trudy VIAM, 2017, no. 10 (58), paper no. 03. Available at: http://www.viam-works.ru (accessed: March 03, 2022). DOI: 10.18577/2071-9140-2017-0-10-3-3.
  10. Glazunov S.G., Yasinsky K.K. Titanium alloys for aviation technology and other industries. Tekhnologiya legkikh splavov, 1993, no. 7–8, pp. 47–54.
  11. Glazunov S.G., Moiseev V.N. Structural titanium alloys. Moscow: Metallurgiya, 1974, 368 p.
  12. Ilyin A.A., Kolachev B.A., Polkin I.S. Titanium alloys. Composition, structure, properties: reference. Moscow: VILS-MATI, 2009, 520 p.
  13. Moiseev V.N. Beta-titanium alloys and prospects for their development. Metallovedenie i termicheskaya obrabotka metallov, 1998, no. 12, pp. 11–14.
  14. Kolachev B.A., Sadkov V.V., Talalaev V.D. Vacuum annealing of titanium structures. Moscow: Mashinostroenie, 1991, 224 p.
  15. Leyens C., Peters M. Titanium and Titanium Alloys. Fundamentals and Applications. Weinheim: WILEY-VCH Verlag GmbH&Co. KGaA, 2003, 513 p.
  16. Whittaker J.T. Ductility and Use of Titanium Alloy and Stainless Steel Aerospace Fasteners: Degree of Master of Science in Mechanical Engineering. University of South Florida, 2015, 91 р.
  17. Birger I.A., Iosilevich G.B. Threaded and flange connections. Moscow: Mashinostroenie, 1990, 368 p.
  18. Kolganov I.M., Dubrovsky P.V., Arkhipov A.N. Manufacturability of aircraft structures, ways to improve. Part 1: textbook. Ulyanovsk: UlGTU, 2003, 148 p.
  19. Boyer R.R., Briggs R.D. The Use of β Titanium Alloys in the Aerospace Industry. Journal of Materials Engineering and Performance, 2005, vol. 14 (6), pp. 681–685.
  20. Duyunova V.A., Leonov A.A., Molodtsov S.V. VIAM's contribution to the development of light alloys and the corrosion control of rocket and space technology products. Trudy VIAM, 2020, no. 2 (86), paper no. 03. Available at: http://www.viam-works.ru (accessed: December 13, 2021). DOI: 10.18577/2307-6046-2020-0-2-22-30.
  21. Panin P.V., Lukina E.A., Alekseev E.B. Effect of hydrogen doping on structure and phase composition of sheet semi-products of VT23 titanium alloy. Trudy VIAM, 2018, no. 7 (67), paper no. 06. Available at: http://www.viam-works.ru (accessed: December 13, 2021). DOI: 10.18577/2307-6046-2018-0-7-49-57.
  22. Panin P.V., Dzunovich D.A., Lukina E.A. Effect of hydrogen doping on processing ductility and texture of sheet semi-products of VT23 titanium alloy. Trudy VIAM, 2018, no. 7 (67), paper no. 07. Available at: http://www.viam-works.ru (accessed: December 13, 202). DOI: 10.18577/2307-6046-2018-0-7-58-68.
  23. Santhosh R., Geetha M., NageswaraRao M. Recent Developments in Heat Treatment of Beta Titanium Alloys for Aerospace Applications. Transactions of the Indian Institute of Metals, 2017, vol. 70 (7), pp. 1681–1688.
  24. Bania P.J., Hutt A.J., Adams R.E. Ultra high strength titanium alloy for fasteners. Titanium-92 Science and Technology: Proceedings of the 7th World Conference on Titanium. Denver: Minerals, Metals & Materials Society, 1993, pp. 2899–2906.
  25. Zolotorevsky V.S. Mechanical properties of materials: a textbook for universities. 2nd ed. Moscow: Metallurgiya, 1983, 352 p.
  26. Inagaki I., Shirai Y., Takechi T., Ariyasu N. Application and Features of Titanium for the Aerospace Industry. Nippon Steel & Sumitomo Metal Technical, 2014, report no. 106, pp. 22–27.
  27. Duyunova V.A., Putyrskiy S.V., Arislanov A.A., Krokhina V.A., Shiryaev A.A. Analysis of the effect of heat treatment on the structure and mechanical properties of bars made of VT47 titanium alloy. Aviation materials and technologies, 2021, no. 4 (65), paper no. 03. Available at: http://www.journal.viam.ru (accessed: March 03, 2022). DOI: 10.18577/2713-0193-2021-0-4-26-34.