Sevalnev G.S., Korobova E.N., Dvoretskov R.M., Doroshenko A.V., Samoilova I.I. Influence of the degree of martensitic structure dispersion and size of carbide phase on the frictional interaction under conditions of dry sliding friction of high-carbon complex alloy steel // Proceedings of VIAM. 2022. No. 6. DOI: 10.18577/2307-6046-2022-0-6-15-26. URL: https://www.viam-works.ru/en/journal/2022/6/2
Keywords
bearing, wear resistance, friction, dispersion of martensite, microstructure, hardness
Abstract

The article considers the effect of the martensitic structure dispersion degree on the tribotechnical characteristic of high carbon complex-alloyed steel. After hardening heat treatment of samples with a various degree of deformation there have been obtained samples with a structure from fine- to large-needle martensite. According to the results of the wear test under conditions of dry sliding friction it has been found that samples with a structure of fine-needle martensite have a wear rate lower by 50 and 70 % compared to medium- and large-needle martensitic structures.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Without new materials – there is no future. Metallurg, 2013, no. 12, pp. 4–8.
  3. Kablov E.N. What to make the future from? The materials of the new generation, the technology of their creation and processing are the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  4. Kablov E.N. The materials of the new generation are the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  5. Pinegin S.V. Rolling supports in cars. Moscow: Publishing House of the AS USSR, 1961. 150 p.
  6. Orlov M.R., Grigorenko V.B., Morozova L.V., Naprienko S.A. Research of operational damages of bearings by methods of optical microscopy, scanning electron microscopy and Х-ray microanalysis. Trudy VIAM, 2016, no. 1 (37), paper no. 9. Available at: http://viam-works.ru (accessed: January 19, 2022). DOI: 10.18577/2307-6046-2016-0-1-62-79.
  7. Kotov S.A., Muzafarova S.-V.R., Sevalnev G.S. The influence of technological factors on the operational resistance of bearings from steel EI347-Sh. Metallovedenie i termicheskaya obrabotka metallov, 2020, no. 12, pp. 43–47.
  8. Yakusheva N.A. High-strength constructional steels for landing gears of perspective products of aircraft equipment. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 3–9. DOI: 10.18577/2071-9140-2020-0-2-3-9.
  9. Porishevsky A.I. Rolling bearings. Moscow: Mechanical Engineering, 1968, 632 p.
  10. Zaitsev A.M., Korostashevsky R.V. Operation of aviation rolling bearings. Moscow: Transport, 1968, 224 p.
  11. Conter L.Ya. Steel for heat-resistant bearings (review). Moscow: NIIavtoprom, 1978, 78 p.
  12. Gromov V.I., Voznesenskaya N.M., Pokrovskaya N.G., Tonysheva O.A. High-strength constructional and corrosion-resistant steels developed by VIAM for aviation engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 159–174. DOI: 10.18577/2071-9140-2017-0-S-159-174.
  13. Korobova E.N., Sevalnev G.S., Gromov V.I., Leonov A.V. Steels for the manufacture of roller bearings for special purposes (review). Trudy VIAM, 2021, no. 11 (105), paper no. 01. Available at: http://www.viam-works.ru (accessed: February 05, 2022). DOI: 10.18577/2307-6046-2021-0-11-3-11.
  14. Korneev A.A. Calculation of the heating time of the bearing. Modern innovations in science and technology: Proceedings of 4th Int. Scientific and Practical Conf. Kursk: Universitetskaya kniga, 2014, pp. 265–267.
  15. Korneev A.A. The choice of hardening temperature became EI347-Sh. Prospective development of science, technology and technology: Materials of 3rd Int. Scientific and Practical Conf. Kursk: Universitetskaya kniga, 2013, pp. 157–158.
  16. Morozova L.V. The damage to rolling bearings during the operation of aviation gas turbine engines. The role of fundamental research in the implementation of strategic directions for the development of materials and technologies for their processing for the period until 2030. Moscow: VIAM, 2019, pp. 175–189.
  17. Geller Yu.A. Instrumental steel. Moscow: Metallurgy, 1983, 525 p.
  18. Sevalnev G.S., Sevalneva T.G., Kolmakov A.G., Dulnev K.V., Krylov S.A. Study of the tribo-technical characteristics of corrosion-resistant steels with different mechanisms of volumetric hardening. Trudy VIAM, 2021, no. 10 (104), paper no. 01. Available at: http://www.viam-works.ru (accessed: February 07, 2022). DOI: 10.18577/2307-6046-2021-0-10-3-11.
  19. Spector A.G., Zelbet B.M., Kiseleva S.A. The structure and properties of bearing steels. Moscow: Metallurgiya, 1980, 264 p.
  20. Rausin Ya.R. Thermal processing of chromium steel (for bearings and tools). Moscow: Mashgiz, 1963, 384 p.
  21. The Materials Project. Available at: https://materialsproject.org (accessed: February 10, 2022).