Methods of investigation of the processes of corrosion-mechanical destruction and hydrogenation of metals (review)

Part 3. Corrosion cracking of aluminum alloys
Laptev A.B., Zakirova L.I., Zagorskikh O.A., Pavlov M.R.
Laptev A.B., Zakirova L.I., Zagorskikh O.A., Pavlov M.R. Methods of investigation of the processes of corrosion-mechanical destruction and hydrogenation of metals (review). Part 3. Corrosion cracking of aluminum alloys // Proceedings of VIAM. 2022. No. 6. DOI: 10.18577/2307-6046-2022-0-6-138-149. URL: https://www.viam-works.ru/en/journal/2022/6/12
Keywords
corrosion-mechanical destruction, hydrogen sulfide cracking, metal hydrogenation, hydrogen brittleness, slow stretching, crack development, corrosive environment
Abstract

Based on reviews of the corrosion-mechanical destruction of metals (in parts 1 and 2), the impact of the corrosive environment and mechanical loads on aluminum alloys is considered. The main theories and practical results of determining changes in the mechanical characteristics of aluminum alloys are presented. The values of the tensile velocity must correspond to the investigated metal-medium system and ensure that the mechanism of destruction of the tested material in the experiment on samples corresponds to the mechanism of destruction of real structures under operating conditions.

Reference list
  1. Kablov E.N., Evgenov A.G., Mazalov I.S., Shurtakov S.V., Zaitsev D.V., Prager S.M. The structure and properties of the selective laser laser rafting method EP648 and VH159 after simulation annealing. Materialovedenie, 2020, no. 6, pp. 3–10.
  2. Kablov E.N. The present and future of additive technologies. Metally Evrazii, 2017, no. 1, pp. 2–6.
  3. Kablov E.N., Erofeev V.T., Dergunova A.V., Deraeva E.V., Svetlov D.A. Influence of environmental factors on the processes of biodegradation of vinylester composites. Journal of Physics: Conference Series, 2020, pp. 012029. DOI: 10.1088/1742-6596/1687/1/012029.
  4. Laptev A.B., Nikolaev E.V., Kurshev E.V., Goryashnik Yu.S. Features of biodegradation of thermoplastics based on polyesters in different climatic zones. Trudy VIAM, 2019, no. 7 (79), paper no. 10. Available at: http://www.viam-works.ru (accessed: November 2, 2021). DOI: 10.18577/2307-6046-2019-0-7-84-91.
  5. Getsov L.B., Laptev A.B., Puzanov A.I. et al. The strength of the powder material for the GTD discs in the conditions of aggressive action of the mixture of chlorides and sodium sulfates. Aviatsionnaya tekhnika, 2019, no. 12, pp. 14–25.
  6. Erasov V.S., Oreshko E.I. Reasons for dependence of mechanical characteristics of material fracture resistanceon sample sizes. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 56–64. DOI: 10.18577/2071-9140-2018-0-3-56-64.
  7. Erasov V.S., Oreshko E.I., Lutsenko A.N. Formation of new surfaces in a firm body at stages of elastic and plastic deformations, the beginning and destruction development. Trudy VIAM, 2018, no. 2, paper no. 12. Available at: http://www.viam-works.ru (accessed: November 2, 2021). DOI: 10.18577/2307-6046-2018-0-2-12-12.
  8. Sinyavsky V.S., Valkov V.D., Budov G.M. Corrosion and protection of aluminum alloys. Moscow: Metallurgiya, 1979, 224 p.
  9. Takase Т., Setoguchi K., Wakahara T. Effect of Surface Roughness on Fatigue Strength of 0,25 % С Annealed Steel and Policarbonate. Transactions of the Japan Society of Mechanical Engineering A, 1998, vol. 64, no. 622, pp. 1463–1467.
  10. Alcantar-Modragón N., García-García V., Reyes-Calderón F. et al. Study of cracking susceptibility in similar and dissimilar welds between carbon steel and austenitic stainless steel through finger test and FE numerical model. International Journal of Advanced Manufacturing Technology. 2021, vol. 116, no. 7–8, pp. 2661–2686.
  11. Laptev A., Kurs M., Lonskaya N. et al. Investigation of Corrosion Damage of Hydration Aluminium Alloys at Full-Scale Accelerated Tests. International Journal of Engineering and Technology, 2018, vol. 7, no. 4, pp. 5061–5066.
  12. Rajasekaran R., Lakshminarayanan A.K. Probing the stress corrosion cracking resistance of laser beam welded AISI 316LN austenitic stainless steel. Proceedings of the Institution of Mechanical Engineers. Part C: Journal of Mechanical Engineering Science, 2021, vol. 235, no. 17, pp. 3299–3317.
  13. Semenychev V.V. Corrosion resistance of alloy D16ch.-T sheets in marine subtropics. Trudy VIAM, 2014, no. 7, paper no. 11. Available at: http://www.viam-works.ru (accessed: November 2, 2021). DOI: 10.18577/2307-6046-2014-7-11-11.
  14. Kablov E.N., Startsev V.O., Inozemtsev A.A. The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  15. Laptev A.B., Zakirova L.I. Zagorskikh O.A., Pavlov M.R. Methods of investigation of the processes of corrosion-mechanical destruction and hydrogenation of metals (review). Part 1. Investigation of corrosion-mechanical destruction of steels. Trudy VIAM, 2022, no. 4 (110), paper no. 12. Available at: http://www.viam-works.ru (accessed: November 2, 2021). DOI: 10.18577/2307-6046-2022-0-4-118-130.
  16. Borisova T.M., Castro R.A. The dielectric properties of MDP – structures based on aluminum oxide. Materials of the XII Intern. Conf. "Dielectrics-2011". St. Petersburg: Herzen Rus. State Pedagogical University, 2011, vol. 1, pp. 356–359.
  17. Panin V.E. Fundamentals of physical mesomechanics. Fizicheskaya mezomekhanika, 1998, no. 1, pp. 5–22.
  18. Grinevich A.V., Lutsenko A.N., Karimova S.A. Durability of products and corrosion fatigue of structural materials. Voprosy materialovedeniya, 2013, no. 1 (73), pp. 220–229.
  19. Chen X., Karasz E., Badwe N., Sieradzk K. Dynamic fracture and dealloying induced stress-corrosion cracking. Corrosion Science, 2021, vol. 187. Art. 109503.