An approach to the construction of a mathematical model of the passage of a heat front through a sample of a heat-shielding material under conditions of an unsteady heat flow

Butakov V.V., Shavnev A.A., Lugovoy A.A., Varrik N.M., Babashov V.G.
Butakov V.V., Shavnev A.A., Lugovoy A.A., Varrik N.M., Babashov V.G. An approach to the construction of a mathematical model of the passage of a heat front through a sample of a heat-shielding material under conditions of an unsteady heat flow // Proceedings of VIAM. 2022. No. 6. DOI: 10.18577/2307-6046-2022-0-6-127-137. URL: https://www.viam-works.ru/en/journal/2022/6/11
Keywords
heat-shielding material, thermal conductivity coefficient, heat flux, highly porous material, mathematical model
Abstract

In this work, the principal possibility of quantifying the heat transfer coefficient of the material using a stand was tested, as well as the selection of experimental parameters to increase the reliability of the assessment of the thermal conductivity coefficient of the layered material. It is possible to use one part of the data array within one test to estimate the heat transfer coefficient of the material on its hot side, and when processing another part of the experimental data, to use the heat transfer coefficient to estimate the heat absorbed by the sample. The proposed estimation method is much simpler in terms of hardware compared to the classical calorimetric method.

Reference list
  1. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  2. Soboyejo W.O., Obayemi J.D., Annan E. et al. Review of High Temperature Ceramics for Aerospace Applications. Advanced Materials Research, 2016, vol. 1132, pp. 385–407.
  3. Kablov E.N., Zhestkov B.E., Grashchenkov D.V., Sorokin O.Yu., Lebedeva Yu.E., Vaga-nova M.L. Investigation of the oxidation resistance of a high-temperature coating on SiC-material under the influence of a high-enthalpy flow. Teplofizika vysokikh temperatur, 2017, vol. 55, no. 6, pp. 704–711.
  4. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  5. Armor for "Buran". Materials and technologies of VIAM for the ISS "Energiya–Buran". Ed. E.N. Kablov. Moscow: Nauka i zhizn, 2013, 128 p.
  6. Glass D.E. Thermal Protection Systems and Hot Structures for Hypersonic Vehicles. Aerospace Materials and Applications. American Institute of Aeronautics and Astronautics Inc., 2018, pp. 531–578. DOI: 10.2514/5.9781624104893.0531.0578.
  7. Zamula G.N., Ivanov S.N. Determination of the effective thermal conductivity and emissivity of multilayer and reinforced structures. Uchenye zapiski TsAGI, 1970, vol. 1, no. 1, pp. 116–123.
  8. Zuev A.V., Zarichnyak Yu.P., Barinov D.Ya. Measurement of thermophysical properties rigid fiber insulation. Trudy VIAM, 2021, no. 2 (96), paper no. 10. Available at: http://www.viam-works.ru (accessed: March 02, 2022). DOI: 10.18577/2307-6046-2021-0-2-88-98.
  9. Zuev A.V., Zarichnyak Yu.P., Barinov D.Ya., Krasnov L.L. Measurement of thermophysical properties of flexible thermal insulation. Aviation materials and technology, 2021. no. 1 (62), paper no. 11. Available at: http://www.journal.viam.ru (accessed: March 02, 2022). DOI: 10.18577/2713-0193-2021-0-1-119-126.
  10. Prosuntsov P.V., Mayorova I.A., Zuev A.V. Using combined heat transfer models to analyze the temperature state of thermal protection elements of reusable spacecraft. Teplovye protsessy v tehniki, 2014, vol. 6, no. 7, pp. 317–323.
  11. Wang X., Tang Y. The Heat Transfer Model and Performance Analyses of Fibre-Enhanced Phase Change Material. Conference: Digital Manufacturing and Automation (ICDMA) International Conference. Changoha, 2010. DOI: 10.1109/ICDMA.2010.419.
  12. Zarubin V.S., Zarubin S.V., Kuvyrkin G.N. Mathematical modeling of heat transfer in a unidirectional fibrous composite. Nauka i obrazovanie, 2014, no. 1, pp. 270–281. Available at: http://technomag.bmstu.ru/doc/657262.html (accessed: March 02, 2022). DOI: 10.7463/0114.0657262.
  13. Lugovoy A.A., Babashov V.G., Karpov Yu.V. The thermal diffusivity of the gradientthermal insulation material. Trudy VIAM, 2014, no. 2, paper no. 02. Available at: http://viam-works.ru (accessed: March 02, 2022). DOI: 10.18577/2307-6046-2014-0-2-2-2.
  14. Stand for the qualitative assessment of heat-insulating materials: pat. 156904 Rus. Federation. No. 2014138916; filed 25.09.14; publ. 20.11.15.
  15. Butakov V.V., Lugovoy A.A., Varrik N.M., Babashov V.G. Assessment of thermal conductivity of a layered highly porous thermal insulation material. Aviation materials and technology, 2022. Accepted to publication.