90-year practice of anticorrosive protection

Antipov V.V., Duyunova V.A., Oglodkov M.S., Fomina M.A., Frantsuzova T.P., Kozlov I.A.
Antipov V.V., Duyunova V.A., Oglodkov M.S., Fomina M.A., Frantsuzova T.P., Kozlov I.A. 90-year practice of anticorrosive protection // Proceedings of VIAM. 2022. No. 6. DOI: 10.18577/2307-6046-2022-0-6-108-126. URL: https://www.viam-works.ru/en/journal/2022/6/10
Keywords
aviation equipment, aircraft, corrosion, protective coatings, anti-corrosion protection, structural materials
Abstract

Results of practical researches of corrosion resistance of the metal materials used in designs of domestic aviation engineering, for the long-term period are stated. In work the chronology of researches and development of anticorrosive protection is observed. Problem questions regarding climatic and biological firmness of materials are stated. Standard corrosion destructions of metal materials because of corrosion cracking, application of technical liquids and fuels, and also contact of diverse materials are given. Technological decisions on the anticorrosive protection, its developments accepted at different stages which are actual and now are provided.

Reference list
  1. Antipov V.V., Kurs M.G., Girsh R.I., Serebrennikova N.Yu. Climatic field tests of SIAL type metal-polymer composition materials in marine climate. Aviaсionnye materialy i tehnologii, 2019, no. 4 (57), pp. 56–64. DOI: 10.18577/2071-9140-2019-0-4-56-64.
  2. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  3. Kablov E.N. The role of fundamental research in the creation of new generation materials. Abstracts of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vol. St. Petersburg, 2019, vol. 4, pp. 24.
  4. Suchalkin E.A. Aviation of the Russian Navy – 100 years. Vozdushno-kosmicheskiye sily. Teoriya i praktika, 2017, no.1 (1), pp. 372–382.
  5. Gaidarev R.V., Obertyaeva I.A. The legendary aircraft of the Great Patriotic War – Il-2. Molodezhnyy innovatsionnyy vestnik, 2020, no. 53, pp. 20–22.
  6. Mukhin M.Yu. From the history of the military-industrial complex of the prewar and war years: organization of work in the field of jet aircraft construction in the USSR in the 1930s – mid-1940s. Trudy Instituta rossiyskoy istorii RAN, 2017, no. 14, pp. 72–96.
  7. Dugin G.S., Manuilov S.A. Aircraft icing. Conditions for the occurrence and types of icing. Problemy bezopasnosti poletov, 2021, no. 1, pp. 27–40.
  8. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. Features of technology and polymer composite materials for the manufacture of wings of advanced aircraft (review). Trudy VIAM, 2022, no. 1 (107), paper no. 07. Available at: http://www.viam-works.ru (accessed: May 15, 2022). DOI: 10.18577/2307-6046-2022-0-1-66-75.
  9. Kutyrev A.E., Chesnokov D.V., Antipov V.V., Vdovin A.I. A study of the use of combined anodic dissolution of aluminum alloys with not high sensibility to IGC evidence from alloy of Al–Li–Cu system with the purpose of predicting loss of mechanical properties at atmospheric corrosion. Trudy VIAM, 2021, no. 2 (96), paper no. 12. Available at: http://www.viam-works.ru (accessed: May 15, 2022). DOI: 10.18577/2307-6046-2021-0-2-109-118.
  10. Antipov V.V., Medvedev I.M., Kutyrev A.E., Zhitnyuk S.V. The investigation of electro-chemical properties of non-sealed oxide coatings on 1163, V-1461, V96С3pch aluminum alloys during accelerated testing. Trudy VIAM, 2019, no. 6 (78), paper no. 06. Available at: http://www.viam-works.ru (accessed: May 15, 2022). DOI: 10.18577/2307-6046-2019-0-6-51-64.
  11. Butushin S.V., Semin A.V. Processing and analysis of data on the operating conditions of the loading of Tu-154 aircraft. Sbornik nauchnykh trudov GosNII GA, 2010, no. 311, pp. 91–97.
  12. Lebedeva I.A., Kharlamov V.A. Features of flight operation of the stabilizer control system in the combined mode of operation on the Tu-154M aircraft. Nauchnyy vestnik MGTU GA, 2006, no. 103, pp. 75–81.
  13. Yurin S.P., Gromov M.S., Uvaev S.F., Lisin O.V. Assessment of the state and adequacy of the resource of the fleet of AI-24 engines for An-24 and An-26 aircraft. Nauchnyy vestnik GosNII GA, 2020, no. 31, pp. 20–29.
  14. Arep'ev K.A., Povarov O.Yu., Popov D.P., Dubinsky V.S. Generalization of the results of the work on the study of the units of the steering control system and the wing mechanization control system of the An-124-100 aircraft. Nauchnyy vestnik GosNII GA, 2019, no. 29, pp. 22–35.
  15. Karnaukh G.E., Arustamova I.S. An-124 is the pinnacle of O.K. Antonova. X International. sci.-pract. conf. young scientists dedicated to 59th anniversary of Yu.A. Gagarin into space (April 8–9, 2020): Sat. scientific articles. Krasnodar: Publishing House - South, 2020, pp. 143–146.
  16. Povarov O.Yu., Arepiev K.A., Popov D.P. Corrosion state of An-28 aircraft. Nauchnyy vestnik GosNII GA, 2021, no. 35, pp. 39–49.
  17. Zhukov A.V. Analysis of some aviation events related to the operation of the An-2 and Yak-18 aircraft. Nauchnyy vestnik UI GA, 2017, no. 9, pp. 28–37.
  18. Gromov M.S., Nizev V.Ya., Kostenko A.V., Smirnov A.V., Stepanov V.N. Influence of a package of repair pads on the stress state of a passenger aircraft wing panel. Nauchnyy vestnik GosNII GA, no. 36, pp. 110–117.
  19. Arepev K.A., Kovalevsky S.A., Simonov T.N. Review of operating conditions for the An-24 aircraft fleet in the Russian Federation in 2017–2018. Nauchnyy vestnik GosNII GA, 2019, no. 28, pp. 40–49.
  20. Maslennikova G.E., Arep'ev K.A., Tazhetdinov R.R., Nikonov V.V., Spryskov V.B. Investigation of the reasons for the change in the characteristics of the climb of the Il-96-300 aircraft. Izvestiya vysshikh uchebnykh zavedeniy. Aviatsionnaya tekhnika, 2019, no. 1, pp. 140–144.
  21. Kulikov V.V., Sharova I.A., Petrova A.P. Repair of honeycomb metal structures in Il aircraft. Remont. Vosstanovleniye. Modernizatsiya, 2016, no. 12, pp. 15–18.
  22. Maslennikova G.E., Kruglyakova O.V. Aircraft Il-76TD-90VD – new life of the old airframe. Nauchnyy vestnik GosNII GA, 2014, no. 4 (315), pp. 22–28.
  23. Demchenko O.F. 80 years of OKB named after A.S. Yakovleva. Polet. Obshcherossiyskiy nauchno-tekhnicheskiy zhurnal, 2007, no. 5, pp. 11–17.
  24. Pavlov N.V. Mi-2 helicopter – US flying laboratory. Aviatsionnyye sistemy, 2016, no. 8, pp. 53–55.
  25. Urnyshev D.S., Nikushkin N.V. Analysis of corrosion damage of the power structure of the airframe of Mi-8T type helicopters. Aktualnyye problemy aviatsii i kosmonavtiki, 2010, no. 6, pp. 242–243.
  26. Anikhovskaya L.I., Kolobova Z.N., Uglova G.N. Materials for the repair of blades of Mi-8 and Mi-24 helicopters under operating conditions. Klei. Germetiki. Tekhnologii, 2005, no. 12, pp. 32–33.
  27. Osipov D.N., Shapkin V.S. Measurement of the rate of development of fatigue cracks in stringers made of material 01420 of the Mi-26T helicopter. Nauchnyy vestnik MGTU GA, 2010, no. 153, pp. 77–82.
  28. Dmitrieva Yu.A. Nikolay Ilyich Kamov and his helicopters. Aktualnyye problemy aviatsii i kosmonavtiki, 2018, no. 4 (14), pp. 553–554.
  29. Aleksandrov N. Sukhoi interceptor. 50 years in service. Dvigatel, 2008, no. 5(59), pp. 26–31.
  30. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviaсionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  31. Karimova S.A., Pavlovskaya T.G., Chesnokov D.V., Semenova L.V. Corrosive activity of CFRPs and protection of metal load-bearing structures in contact with CFRP. Rossiyskiy khimicheskiy zhurnal, vol. 54, no. 1, pp. 110–116.
  32. Lutsenko A.N., Slavin A.V., Erasov V.S., Khvatskiy K.K. Strength tests and researches of aviation materials. Aviaсionnye materialy i tehnologii, 2017, no. S, pp. 527–546.
  33. Kablov E.N. Marketing of Materials Science, Aircraft Engineering and Industry: Present and Future. Direktor po marketingu i sbytu. 2017, no. 5–6, pp. 40–44.