Application of carbon fiber plastics in constructions of pilotless devices (review)
Mishkin S.I. Application of carbon fiber plastics in constructions of pilotless devices (review) // Proceedings of VIAM. 2022. No. 5. DOI: 10.18577/2307-6046-2022-0-5-87-95. URL: https://www.viam-works.ru/en/journal/2022/5/8
Keywords
polymeric composite material, construction, carbon fiber plastic, pilotless device, tail plumage, wings, propeller blade, rigidity, prepreg, molten technology, vacuum infusion
Abstract
The overview on application of carbon fiber plastics in different constructions of pilotless devices is carried out. The main requirements to constructions, such as rigidity, durability, shock resistance, cost, etc. are provided. The analysis of scientific publications on advantages of application of carbon fiber plastics is provided in tail plumage, wings, the body and blades of pilotless devices screws. Are given the recommendation about application developed in Research Center Kurchatovsky institut – VIAM of carbon fiber plastics in constructive parts of pilotless devices.
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
- Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
- Kablov E.N. Marketing of materials science, aircraft building and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5–6, pp. 40–44.
- Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Abstracts of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
- Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
- Senyushkin N.S., Yamaliev R.R., Yalchibaeva L.R. The use of composite materials in the construction of UAVs. Molodoy uchenyy, 2011, vol. 1, no. 4 (27), pp. 59–61. Available at: https://moluch.ru/archive/27/2963/ (accessed: February 07, 2022).
- Kuprikova E.Yu., Aseeva T.P., Razina G.M., Stepanov N.V. Technological aspects of manufacturing a truss rib from composite materials for the wing of an unmanned aerial vehicle using a truss and a rubber element. Konstruktsii iz kompozitsionnykh materialov, 2016, no. 1, pp. 30–33.
- Pavlov M.S., Karavatsky A.K., Kostyushin K.V. et al. Optimal design of the body of an unmanned aerial vehicle. Vestnik Tomskogo gosudarstvennogo universiteta, 2021, no. 73, pp. 71–80.
- Lazorin A.E., Degtyarev A.A., Polikarpov A.A. Numerical study of the strength characteristics of the V-shaped tail of an unmanned aerial vehicle based on composite materials. Vestnik Kontserna VKO «Almaz-Antey», 2020, no. 3, pp. 54–61. DOI: 10.38013/2542-0542-2020-3-54-61.
- Kakhanchik-Pilinoga E., Svistunova A., Luzan M., Bakaev A. Application of promising composite materials in unmanned aerial systems. Nauka i innovatsii, 2017, no. 6 (172), pp. 34–38.
- Kolobkov A.S. Polymer composite materials for various aircraft structures (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 05. Available at: http://www.viam-works.ru (accessed: December 16, 2021). DOI: 10.18577/2307-6046-2020-0-67-38-44.
- Nagornov A.Yu. Flutter of an unmanned aerial vehicle made of composite materials with two-beam plumage. Trudy MAI, 2020, no. 113. Available at: http://www.trudymai.ru (accessed: December 16, 2021). DOI: 10.34759/trd-2020-113-19.
- Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM. Aviacionnye materialyi tekhnologii, 2011, no. 2, pp. 38–42.
- Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021. no. 1 (62), paper no. 03. Available at: https://journal.viam.ru (accessed: February 19, 2021). DOI: 10.18577/2713-0193-2021-0-1-22-23.
- Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Influence of fillers on properties of adhesive prepregs and PCM on their basis. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 51–55. DOI: 10.18577/2071-9140-2017-0-4-51-55.
- Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
- Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.