Influence of mode of local laser annealing on the domain structure in microwires PrDyFeCoB
Dvoretskaya E.V., Koplak O.V., Korolev D.V., Valeev R.A., Sidorov V.L., Piskorsky V.P., Morgunov R.B. Influence of mode of local laser annealing on the domain structure in microwires PrDyFeCoB // Proceedings of VIAM. 2022. No. 5. DOI: 10.18577/2307-6046-2022-0-5-64-73. URL: https://www.viam-works.ru/en/journal/2022/5/6
Keywords
permanent magnets, micromagnets, magnetically modulated structures, laser irradiation, amorphous magnets, magnetic microwires
Abstract
. With the help of continuous IR laser exposure, periodic magnetically modulated structures were created from amorphous microwires. Local laser annealing leads to the formation of regions of nanocrystalline phases 2-14-1, 1-4-1, 2-1 alternating with amorphous regions, thereby creating a pattern on the sample surface with a given magnetization distribution. In amorphous samples without laser irradiation, chaotic domains are observed, disappearing after two hours of annealing at 900 °C. In the samples profiled by a «fast» laser, local annealing leads to further transformation of phases only in the very center of the laser «notches», which is expressed in a change in the slope of the profile line near the domain boundary.
Reference list
- Korolev D.V., Piskorskii V.P., Valeev R.A., Bakradze M.M., Dvoretskaya E.V., Koplak O.V., Morgunov R.B. Rare-earth RE–TM–B micromag-nets engineering (review). Aviation materials and technology, 2021, no. 1 (62), paper no. 05. Available at: http://www.journal.viam.ru (accessed: November 15, 2021). DOI: 10.18577/2713-0193-2021-0-1-44-60.
- Walther A., Marcoux C., Desloges B. et al. Micro-patterning of NdFeB and SmCo magnet films for integration into micro-electro-mechanical-systems. Journal of Magnetism and Magnetic Materials, 2008, vol. 321, pp. 590–594.
- Ning H., Zhang Y., Zhu H. et al. Geometry Design, Principles and Assembly of Micromotors. Journal of Micromachines, 2018, vol. 9, no. 75, pp. 35.
- Peng H.-X., Qin F., Phan M.-H. Ferromagnetic microwire composites. From Sensors to Microwire applications. Springer, 2016. 245 p.
- Morgunov R.B., Koplak O.V., Talantsev A.D., Korolev D.V., Piskorskij V.P., Valeev R.A. The phenomenology of the magnetic hysteresis loops in multilayer microwires α-Fe/DyPrFeCoB. Trudy VIAM, 2019, no. 7 (79), paper no. 08. Available at: http://www.viam-works.ru (accessed: November 15, 2021). DOI: 10.18577/2307-6046-2019-0-7-67-75.
- Koplak O.V., Kunitsyna E.I., Valeev R.A., Korolev D.V., Piskorskii V.P., Morgunov R.B. Ferromagnetic microwires α-Fe/(PrDy)(FeCo)B for micromanipulators and polymer composites. Trudy VIAM, 2019, no. 11 (83), paper no. 07. Available at: http://www.viam-works.ru (accessed: November 15, 2021). DOI: 10.18577/2307-6046-2019-0-11-60-67.
- Croat J.J., Chraplyvy A.R., Herbst J.F. Crystallization of amorphous Pr0.27Co0.73: Magnetic properties and laser induced coercivity. Journal of Applied Physics Letters, 1980, vol. 37, pp. 962–964.
- Ünal A.A., Parabas A., Arora A. et al. Laser-driven formation of transient local ferromagnetism in FeRh thin films. Ultramicroscopy, 2017, vol. 183, pp. 104–108.
- Molian R., Molian P. Pulsed laser deposition and annealing of Dy–Fe–B thin films on melt-spun Nd–Fe–B ribbons for improved magnetic performance. Journal of Magnetism and Magnetic materials, 2009, vol. 321, pp. 241–246.
- Guo B. Chinese Materials Conference, Effect of processing method on the microstructure of Nd4.5Fe77B18.5 magnetic alloy. Procedia Engineering, 2011, vol. 27, pp. 671–679.
- Guo-hau Tu, Aitounian Z., Ryan D.H., Strom-Olsen J.O. Crystallization and texturing in rapidly quenched Nd2Fe14B1 and Nd15Fe77B8. Journal of Applied Physics, 1988, vol. 63, no. 8, pp. 3330–3332.
- Harada T., Fujita M., Kuji T. Laser annealing of an amorphous Nd–Fe–B alloy. Nuclear Instruments and Methods in Physics Research B, 1997, vol. 12, no. 1, pp. 383–386.
- Takashima H., Ueda K., Itoh M. Red photoluminescence in praseodymium-doped titanate perovskite films epitaxially grown by pulsed laser deposition. Journal of Applied Physics Letters, 2006, vol. 89, аrt. 261915.
- Chu K., Jin Z.Q., Chakka V.M., Liu J.P. Rapid magnetic hardening by rapid thermal annealing in NdFeB-based nanocomposites. Journal of Physics D: Applied Physics, 2005, vol. 38, pp. 4009–4014.
- Koplak O.V., Sidorov V.L., Dvoretskaya E.V., Shashkov I.V., Valeev R.A., Korolev D.V., Morgunov R.B. Radial domains in Dy–Pr–FeCo–B microwires. Fizika tverdogo tela, 2021, vol. 63, no. 2, pp. 242–247.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Materials of a new generation and digital technologies for their processing. Bulletin of the Russian Academy of Sciences, 2020, vol. 90, no. 4, pp. 331–334.
- Kablov E.N. Russia Needs New Generation Materials. Redkiye zemli, 2014, no. 3, pp. 8–13.
- Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples’ temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577 / 2071-9140-2020-0-4-47-58.
- Kabanov Yu., Zhukov A., Zhukova V., Gonzalez G. Magnetic domain structure of wires studied by using the magneto-optical indicator film method. Applied Physics Letters, 2005, vol. 87, art. 142507.
- Nikitenko V.I., Gornakov V.S., Dedukh L.M. et al. Magnetooptical indicator film (MOIF) microscopy of granular and layer structures (abstract). Journal of Applied Physics, 1996, vol. 79, pp. 6073.
- Yue M., Liu R.M., Liu W.Q. et al. Ternary DyFeB Nanoparticles and Nanoflakes With High Coercivity and Magnetic Anisotropy. IEEE Transactions on Nanotechnology, 2012, vol. 11, pp. 651–654.
- Yang J., Han J., Tian H. et al. Structural and Magnetic Properties of Nanocomposite Nd–Fe–B Prepared by Rapid Thermal Processing. Engineering, 2020, vol. 6, no. 2, pp. 132–140.
- Ozawa S., Saito T., Motegi T. Effects of cooling rate on microstructures and magnetic properties of Nd–Fe–B alloys. Journal of Alloys and Compounds, 2004, vol. 363, pp. 263–270.
- Wang C., Yan M., Zhang W.Y. Effects of Nb and Zr additions on crystallization behavior, microstructure and magnetic properties of melt-spun (Nd, Pr)2Fe14B/α-Fe alloys. Journal of Magnetism and Magnetic Materials, 2006, vol. 306, pp. 195–198.
- Liu Z.W., Davies H.A. The practical limits for enhancing magnetic property combinations for bulk nanocrystalline NdFeB alloys through Pr, Co and Dy substitutions. Journal of Magnetism and Magnetic Materials, 2007, vol. 313, pp. 337–341.