SiGe structure investigation using methods of X-ray diffraction and transmission electron microscopy

Zaysev D.V., Medvedev P.N., Lukinа E.A.
Zaysev D.V., Medvedev P.N., Lukinа E.A. SiGe structure investigation using methods of X-ray diffraction and transmission electron microscopy // Proceedings of VIAM. 2022. No. 5. DOI: 10.18577/2307-6046-2022-0-5-112-122. URL: https://www.viam-works.ru/en/journal/2022/5/10
Keywords
x-ray diffraction, transmission electron microscopy, crystal lattice, twins, stacking faults, SiGe solid solution, memristors
Abstract

The structure of the SiGe material used to create memristive structures has been studied by x-ray diffractometry and transmission electron microscopy. The phase composition of the material has been determined. Revealed the inhomogeneity of the SiGe solid solution. The lattice periods, the degree of lattice microstrain, and the volume fractions of the solid solution phases are calculated. Using transmission electron microscopy, the following have been investigated: grain structure, distribution of phases and defects in the volume of grains. The defects of the crystal lattice have been investigated, and the character of the inhomogeneity of the SiGe solid solution has been refined using local x-ray microanalysis.

Reference list
  1. Bennett G.L., Lombardo J.J., Hemler R.J. et al. Mission of Daring: The General-Purpose Heat Source Radioisotope Thermoelectric Generator. 4th International Energy Conversion Engineering Conference and Exhibit (IECEC), 2006, pp. 26–29. DOI: 10.2514/6.2006-4096.
  2. Joshi G., Lee H., Lan Y. et al. Enhanced Thermoelectric Figure-of-Merit in Nanostructured p-Type Silicon Germanium Bulk Alloys. Nano Letters, 2008, vol. 8, is. 12, pp. 4670–4674. DOI: 10.1021/nl8026795.
  3. Wang X.W., Lee H., Lan Y.C. et al. Enhanced Thermoelectric Figure of Merit in Nanostructured n-Type Silicon Germanium Bulk Alloy. Applied Physics Letters, 2008, vol. 93, is. 19, pp. 3121. DOI: 10.1063/1.3027060.
  4. Harame D.L., Meyerson B.S. The early history of IBM's SiGe mixed signal technology. IEEE Transactions on Electron Devices, 2001, vol. 48, no. 11, pp. 2555–2567. DOI: 10.1109/16.960383.
  5. Chevalier P., Gianesello F., Pallotta A. et al. PD-SOI CMOS and SiGe BiCMOS Technologies for 5G and 6G communications. 2020 IEEE International Electron Devices Meeting (IEDM), 2020, pp. 34.4.1–34.4.4. DOI: 10.1109/IEDM13553.2020.9371954.
  6. Hofmann A., Jirovec D., Borovkov M. et al. Assessing the potential of Ge/SiGe quantum dots as hosts for singlet-triplet qubits. Available at: https://arxiv.org/pdf/1910.05841.pdf (accessed: January 24, 2022). DOI: 10.48550/arXiv.1910.05841.
  7. Martin S., Vivekananda P.A., Markus B. et al. Investigating microwave loss of SiGe using superconducting transmon qubits. Applied Physics Letters, 2021, vol. 118, is. 12, pp. 4001. DOI: 10.1063/5.0038087.
  8. Ventra M.D., Pershin Y.V. Memcomputing: a computing paradigm to store and process information on the same physical platform. Nature Physics, 2013, vol. 9, pp. 200–202. DOI: 10.48550/arXiv.1304.1675.
  9. Choi S., Tan S.H., Li Z. et al. SiGe epitaxial memory for neuromorphic computing with reproducible high performance based on engineered dislocations. Nature Materials, 2018, vol. 17, pp. 335–340. DOI: 10.1038/s41563-017-0001-5.
  10. Keonhee K., Dae K., Yeonjoo J. et al. Ion Beam-Assisted Solid Phase Epitaxy of SiGe and its Application for Analog Memristors. Journal of Alloys and Compounds, 2021, vol. 884, pp. 161086. DOI: 10.1016/j.jallcom.2021.161086.
  11. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α + β-titanium alloy based on a system of Ti–Al–Sn–Zr–Si–β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  12. Aleksandrov D.A., Muboyadzhyan S.A., Lutsenko A.N., Zhuravleva P.L. Hardening of the surface of titanium alloys by ion implantation method and ionic modification. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 33–39. DOI: 10.18577/2071-9140-2018-0-2-33-39.
  13. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, pp. 24.
  14. Kablov E.N., Lukina E.A., Zavodov A.V., Efimochkin I.Yu. The formation of structure in ultrafine WC–Cо carbide material in the presence of inhibitory additives. Trudy VIAM, 2020, no. 4–5 (88), paper no. 10. Available at: http://www.viam-works.ru (accessed: January 24, 2021). DOI: 10.18577/2307-6046-2020-0-45-89-99.
  15. Benarieb I., Ber L.B., Antipov K.V., Sbitneva S.V. Trends in development of wrought alloys of Al–Mg–Si–(Cu) system. Part 1 (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 14–22. DOI: 10.18577/2071-9140-2019-0-3-14-22.
  16. Treninkov I.A., Zavodov A.V., Petrushin N.V. Research of crystal structure and microstructure of the ZhS32-VI nickel-base superalloy synthesized by selective laser fusion method, after high-temperature mechanical tests. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 57–65. DOI: 10.18577/2071-9140-2019-0-1-57-65.