Influence of the ratio of the anodic and cathodic impulse active times on the properties of the plasma electrolitic coating on the ML5 alloy

Kozlov I.A., Zavarzin S.V., Fomina M.A., Kurshev E.V., Lavrov N.S.
Kozlov I.A., Zavarzin S.V., Fomina M.A., Kurshev E.V., Lavrov N.S. Influence of the ratio of the anodic and cathodic impulse active times on the properties of the plasma electrolitic coating on the ML5 alloy // Proceedings of VIAM. 2022. No. 4. DOI: 10.18577/2307-6046-2022-0-4-84-95. URL: https://www.viam-works.ru/en/journal/2022/4/9
Keywords
magnesium alloy, oxidation, plasma electrolytic oxidation, corrosion, protective coatings, microarc oxidation
Abstract

Considers the question of the influence on the structure of the PEO coating of the time ratio of exposure to the polarizing voltage in the anodic and cathodic half-periods during the oxidation process in a silicate-phosphate electrolyte. A linear dependence of the time of cathodic polarization and the thickness of the coating formed on a cast magnesium alloy in a silicate-phosphate electrolyte has been revealed. When using anodic pulses of short duration, the coating has numerous defects in the form of pores, which negatively affects the protective properties.

Reference list
  1. Kablov E.N. The role of fundamental research in the creation of new generation materials. Report XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  2. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  3. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260). pp. 3–16.
  4. Mostyaev I.V., Akinina M.V. Features and development trends in the field of heat treatment of magnesium alloys (review). Trudy VIAM, 2018, no. 7 (67), paper no. 5. Available at: http://www.viam-works.ru (accessed: December 9, 2021). DOI: 10.18577/2307-6046-2018-0-7-41-48.
  5. Mukhina I.Yu., Uridiya Z.P., Trofimov N.V. Сorrosion-resistant casting magnesium alloys. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 15–23. DOI: 10.18577/2071-9140-2017-0-2-15-23.
  6. Liu L.J., Schlesinger M. Corrosion of magnesium and its alloys. Corrosion Science, 2009, vol. 51, no. 8, pp. 1733–1737. DOI: 10.1016/j.corsci.2009.04.025.
  7. Song G., Atrens A., John D.S. et al. The anodic dissolution of magnesium in chloride and sulphate solutions. Corrosion Science, 1997, vol. 39, no. 10–11, pp. 1981–2004. DOI: 10.1016/S0010-938X(97)00090-5.
  8. Hornberger H., Virtanen S., Boccaccini A.R. Biomedical coatings on magnesium alloys – A review. Acta Biomaterialia, 2012, vol. 8, no. 7, pp. 2442–2455. DOI: 10.1016/j.actbio.2012.04.012.
  9. Kozlov I.A., Vinogradov S.S., Uridiya Z.P., Duyunova V.A., Manchenko V.A. Effekt predvaritelnogo travleniya splava ML5 pered plazmennym elektroliticheskim oksidirovaniyem [Effect of preliminary etching of alloy ML5 before plasma electrolytic oxidation]. Trudy VIAM, 2018, no. 9 (69), paper no. 04. Available at: http://www.viam-works.ru (accessed: December 9, 2021). DOI: 10.18577/2307-6046-2018-0-9-32-42.
  10. Blawert C., Dietzel W., Ghali E., Song G. Anodizing treatments for magnesium alloys and their effect on corrosion resistance in various environments. Advanced Engineering Materials, 2006, vol. 8, no. 6, pp. 511–533. DOI: 10.1002/adem.200500257.
  11. Wang L.I., Chen L.I., Yan Z., Fu W. Optical emission spectroscopy studies of discharge mechanism and plasma characteristics during plasma electrolytic oxidation of magnesium in different electrolytes. Surface and Coatings Technology, 2010, vol. 205, no. 6, pp. 1651–1658. DOI: 10.1016/j.surfcoat.2010.10.022.
  12. Erokhin A.L., Nie X., Leyland A. et al. Plasma electrolysis for surface engineering. Surface and Coatings Technology, vol. 122, no. 2–3, pp. 73–93. DOI: 10.1016/S0257-8972(99)00441-7.
  13. Kuhn A. Plasma anodizing of magnesium alloys. Metal Finishing, 2003, vol. 101, no. 9, pp. 44–50. DOI: 10.1016/S0026-0576(03)90261-3.
  14. Kozlov I.A., Vinogradov S.S., Tarasova K.G., Kulyushina N.V., Manchenko V.A. Plasma electrolytic oxidation of magnesium alloys (review). Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 23–36. DOI: 10.18577/2071-9140-2019-0-1-23-36.
  15. Barati Darband G.H., Aliofkhazraei M., Hamghalam P., Valizade N. Plasma electrolytic oxidation of magnesium and its alloys: Mechanism, properties and applications. Journal of Magnesium and Alloys, 2017, vol. 5, no. 1, pp. 74–132. DOI: 10.1016/j.jma.2017.02.004.
  16. Lu X., Mohedano M., Blawert C. et al. Plasma electrolytic oxidation coatings with particle additions – A review. Surface and Coatings Technology, 2016, vol. 307, pp. 1165–1182. DOI: 10.1016/j.surfcoat.2016.08.055.
  17. Oh Y.-J., Mun J.-I., Kim J.-H. Effects of alloying elements on microstructure and protective properties of Al2O3 coatings formed on aluminum alloy substrates by plasma electrolysis. Surface and Coatings Technology, 2009, vol. 204, no. 1–2, pp. 141–148. DOI: 10.1016/j.surfcoat.2009.07.002.
  18. Rudnev V.S., Adigamova M.V., Lukiyanchuk I.V. et al. Oxide coatings with ferromagnetic characteristics on Al, Ti, Zr and Nb. Surface and Coatings Technology, 2020, vol. 381, art. 125180. DOI: 10.1016/j. surfcoat.2019.125180.
  19. Gnedenkov S.V., Sinebryukhov S.L., Mashtalyar D.V. et al. Electrochemical and hydrophobic properties of composite PEO coatings formed using TFE telomeric solution. Vestnik Dalnevostochnogo otdeleniya Rossiyskoy akademii nauk, 2015, no. 4, pp. 20–27.
  20. Song G.-L., Xu Z. The surface, microstructure and corrosion of magnesium alloy AZ31 sheet. Electrochimica Acta, 2010, vol. 55, no. 13, pp. 4148–4161. DOI: 10.1016/j.electacta.2010.02.068.
  21. Virtanen S. Biodegradable Mg and Mg alloys: Corrosion and biocompatibility. Materials Science & Engineering B: Solid-State Materials for Advanced Technology, 2011, vol. 176, pp. 1600–1608. DOI: 10.1016/j.mseb.2011.05.028.
  22. Kannan M.B. Electrochemical deposition of calcium phosphates on magnesium and its alloys for improved biodegradation performance: A review. Surface and Coatings Technology, 2016, vol. 301, pp. 36–41. DOI: 10.1016/j.surfcoat.2015.12.044.
  23. DeGarmo E.P., Black J.T., Kohser R.A. Materials and processes in engineering. Available at: https://www.worldcat.org/title/degarmos-materials-andprocesses-in-engineering/oclc/76935847 (accessed: December 30, 2021).
  24. Kockar H., Meydan T. The rotation and clamping effect on the magnetic properties of iron films deposited onto a rotating substrate. Physica B: Condensed Matters, 2002, vol. 321, no. 1–4, pp. 124–128. DOI: 10.1016/S0921-4526(02)00836-0.
  25. Karpuz A., Kockar H., Alper M. The effect of different chemical compositions caused by the variation of deposition potential on properties of Ni–Co films. Applied Surface Science, 2011, vol. 257, no. 8, pp. 3632–3635. DOI: 10.1016/j.apsusc.2010.11.092.
  26. Kockar H., Bayirli M., Alper M. A new example of the diffusion-limited aggregation: Ni–Cu film patterns. Applied Surface Science, 2010, vol. 256, no. 9, pp. 2995–2999. DOI: 10.1016/j.apsusc.2009.11.063.
  27. DeLong H.K. Electroplating on Magnesium. Transactions of The Institute of Metal Finishing, 1952, vol. 29, no. 1, pp. 201–226. DOI: 10.1080/00202967.1952.11869600.
  28. Chen X.B., Yang H.Y., Abbott T.B. et al. Magnesium: Engineering the Surface. JOM, 2012, vol. 64, no. 6, pp. 650–656. DOI: 10.1007/s11837-012-0331-3.
  29. Wu X., Su P., Jiang Z., Meng S. Influences of current density on tribological characteristics of ceramic coatings on ZK60 Mg alloy by plasma electrolytic oxidation. ACS Applied Materials & Interfaces, 2010, vol. 2, no. 3, pp. 808–812. DOI: 10.1021/am900802x.
  30. Ono S., Moronuki S., Mori Y. et al. Effect of Electrolyte Concentration on the Structure and Corrosion Resistance of Anodic Films Formed on Magnesium through Plasma Electrolytic Oxidation. Electrochimica Acta, 2017, vol. 240, pp. 415–423. DOI: 10.1016/j.electacta.2017.04.110.
  31. Shi Z., Song G., Atrens A. Influence of anodising current on the corrosion resistance of anodised AZ91D magnesium alloy. Corrosion Science, 2006, vol. 48, no. 8, pp. 1939–1959. DOI: 10.1016/j.corsci.2005.08.004.
  32. Asoh H., Matsuoka S., Sayama H., Ono S. Anodizing under sparking of AZ31B magnesium alloy in Na3PO4 solution. Journal of the Japan Institute of Light Metals, 2010, vol. 60, pp. 608–614.
  33. Kozlov I.A., Vinogradov S.S., Naprienko S.A. Structure and properties of a PEO coating formed on an ML5 alloy in an electrolyte containing silicates and phosphates. Korroziya: materialy, zashchita, 2017, no. 8, pp. 35–41.
  34. Kozlov I.A., Vinogradov S.S., Kulyushina N.V., Kutyrev A.E., Pastukhov A.S. Influence of the polarizing current amplitude ratio on the protective properties of the PEO coating formed on the ML5 alloy. Korroziya: materialy, zashchita, 2016, no. 11, pp. 40–48.