Development of the isothermal deformation on air technology of production turbocharger disks using computer modeling

Kapitanenko D.V., Moiseev N.V., Bazhenov A.R., Gladkov Yu.A.
Kapitanenko D.V., Moiseev N.V., Bazhenov A.R., Gladkov Yu.A. Development of the isothermal deformation on air technology of production turbocharger disks using computer modeling // Proceedings of VIAM. 2022. No. 4. DOI: 10.18577/2307-6046-2022-0-4-13-21. URL: https://www.viam-works.ru/en/journal/2022/4/2
Keywords
heat-resistant nickel alloys, isothermal deformation, computer modeling, die tooling, turbine disks, turbocharger
Abstract

Describes the results of the work performed on the development of technology for the manufacturing of forgings of disk made of heat-resistant nickel alloys by isothermal deformation on air using computer modeling in the QForm software package. The stress-strain state of die tooling was calculated and the technology for producing disk forgings for welded shafts of the TK32 compressor was developed. Information on the of introduction of the developed technology into serial production are presented.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. History of aviation materials science. VIAM – 75 years of search, creativity, discoveries. Moscow: Nauka, 2007, 343 p.
  3. Kablov E.N., Antipov V.V., Sviridov A.V., Gribkov М.S. Features of electron beam welding of heat-resistant alloys EI698-VD and EP718-ID with steel 45. Trudy VIAM, 2020, no. 9 (91), paper no. 01. Available at: http://www.viam-works.ru (accessed: July 9, 2021). DOI: 10.18577/2307-6046-2020-0-9-3-14.
  4. Lomberg B.S., Shestakova A.A., Bakradze M.M., Karachevtsev F.N. The investigation of the stability of γ-phase with size below 100 nm in Ni-base superalloy VZh175-ID. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 3–10. DOI: 10.18577/2071-9140-2018-0-4-3-10.
  5. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577 / 2071-9140-2019-0-2-3-11.
  6. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. The application of new wrought nickel alloys for advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.
  7. Volkov A.M., Vostrikov A.V., Bakradze M.M. Development principles and alloying features of p/m Ni-base superalloys for jet-engine disks application. Trudy VIAM, 2016, no. 8, paper no. 2. Available at: http://www.viam-works.ru (accessed: July 1, 2021). DOI: 10.18577/2307-6046-2016-0-8-2-2.
  8. Ponomarenko D.A., Moiseev N.V., Skugorev A.V. Efficient technology for manufacturing GTE disks from heat-resistant nickel alloys. Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem, 2013, no. 10, pp. 13–17.
  9. Polukhin P.I., Gun G.Ya., Galkin A.M. Resistance to plastic deformation of metals and alloys. Moscow: Metallurgiya, 1983, 488 p.
  10. Gladkov Yu.A., Mordvintsev P.S. Modeling of technological processes of stamping in solving problems of aircraft and engine building. Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem, 2012, no. 5, pp. 8–47.
  11. Shpagin A.S., Kucheryaev V.V., Bubnov M.V. Computer simulation of thermomechanical processing of heat-resistant nickel alloys VZh175 and EP742. Trudy VIAM, 2019, No. 8 (80), paper no. 04. Available at: http://www.viam-works.ru (accessed: July 01, 2021). DOI: 10.18577/2307-6046-2019-0-8-27-35.
  12. Bakradze M.M., Skugorev A.V., Kucheryayev V.V., Bubnov M.V. Computer modeling of technological metal forming processes as effective instrument for development of new technologies. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 175–185. DOI: 10.18577/2071-9140-2017-0-S-175-185.
  13. Stebunov S.A., Bocharov Yu.A. Certification of aviation forgings based on process modeling in the QForm program. Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem, 2011, no. 6, pp. 33–35.
  14. Stebunov S.A., Biba N.V. QForm – a program designed for technologists. Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem, 2004, no. 9, pp. 38–43.
  15. Vlasov A.V., Stebunov S.A., Evsyukov S.A. Finite element modeling of technological processes of forging and forging. Moscow: Bauman MSTU, 2019, 383 p.
  16. Alimov A., Zabelyan D., Burlakov I., Korotkov I., Gladkov Y. Simulation of Deformation Behavior and Microstructure Evolution during Hot Forging of TC11 Titanium Alloy. Defect and Diffusion Forum, 2018, vol. 385, pp. 449–454. DOI: 10.4028/www.scientific.net/DDF.385.449.