Laser modification of rare earth magnetic alloys (review)

Morgunov R.B., Korolev D.V., Valeev R.A., Piskorsky V.P.
Morgunov R.B., Korolev D.V., Valeev R.A., Piskorsky V.P. Laser modification of rare earth magnetic alloys (review) // Proceedings of VIAM. 2022. No. 3. DOI: 10.18577/2307-6046-2022-0-3-75-90. URL: https://www.viam-works.ru/en/journal/2022/3/8
Keywords
magnetic materials, permanent magnets, laser processing, selective laser sintering, magnetic properties, micromagnets
Abstract

Аnalyzes the physico-chemical processes in the laser processing of magnetic materials. It is shown that not only the duration of the laser pulse and its power (the main parameters usually taken into account when laser modification of the microstructure of the material), but also the wavelength, polarization of light can affect the result of laser processing. The local temperature caused by laser irradiation depends both on the size of the irradiated object, its chemical composition, heat capacity and thermal conductivity of the material, and on the rate of energy exchange between thermal reservoirs associated with the atomic, electron and spin subsystems of the magnet.

Reference list
  1. Korolev D.V., Piskorskii V.P., Valeev R.A., Bak-radze M.M., Dvoretskaya E.V., Koplak O.V., Morgunov R.B. Rare-earth RE–TM–B micromagnets engineering (review). Aviation materials and technology, 2021, no. 1 (62). paper no. 05. Available at: http://www.journal.viam.ru (accessed: October 11, 2021). DOI: 10.18577/2713-0193-2021-0-1-44-60.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  4. Kablov E.N. Russia Needs New Generation Materials. Redkiye zemli, 2014, no. 3, pp. 8–13.
  5. Bäuerle D. Laser Processing and Chemistry. 4th ed. Berlin, Heidelberg: Springer-Verlag, 2011, p. 12. DOI: 10.1007/978-3-642-17613-5_1.
  6. Palneedi H., Park J. H., Maurya D. et al. Laser Irradiation of Metal Oxide Films and Nanostructure Applications and Advances. Advanced Materials Review, 2018, pp. 1–38.
  7. Yap C.Y., Chua C.K., Dong Z.L. et al. Review of selective laser melting Materials and applications. Applied Physics Reviews – Focused Review, 2015, vol. 2, pp. 1–21.
  8. Sridharan N., Cakmak E., List F.A. et al. Rationalization of solidification mechanism of Nd–Fe–B magnets during laser directed-energy deposition. Journal of Material Science, 2018, vol. 53, pp. 8619–8626.
  9. Huber C., Sepehri-Amin H., Goertler M. et al. Сoercivity enhancement of selective laser sintered NdFeB magnets by grain boundary infiltration. Acta Materialia, 2019, vol. 172, рр. 66–77.
  10. Perigo E.A., Jacimovic J., García Ferré F., Scherf L.M. Additive Manufacturing of Magnetic Materials. Additive Manufacturing, 2019, vol. 30, рр. 1–48.
  11. Chaudhary V., Mantri S.A., Ramanujan R.V., Banerjee R. Additive Manufacturing of Magnetic Materials. Progress in Materials Science, 2020, vol. 114, рр. 1–81.
  12. Bittner F., Thielsch J., Drossel1 W. Laser powder bed fusion of Nd–Fe–B permanent magnets. Progress in Additive Manufacturing, 2020, vol. 5, no. 3, pp. 1–9. DOI: 10.1007/s40964-020-00117-7.
  13. Volegov A.S., Andreev S.V., Selezneva N.V. et al. Additive manufacturing of heavy rare earth free high-coercivity. Acta Materialia, 2020, vol. 188, рр. 733–739.
  14. Hopkinson D., Cockburn A., O’Neill W. Fiber laser processing of amorphous rare earth NeFeB magnetic materials. Conference: ICALEO® 2011: 30th International Congress on Laser Materials Processing, Laser Microprocessing and Nanomanufacturing, 2011, pp. 1233. DOI: 10.2351/1.5062208.
  15. Korolev D.V., Piskorsky V.P., Valeev R.A., Koplak O.V., Morgunov R.B. Local crystallization under the action of a single laser pulse in amorphous PrDyFeCoB microwires. Fizika tverdogo tela, 2021, vol. 63, no. 8, pp. 1105–1114.
  16. Xu Y., Wang R., Ma S. et al. Theoretical analysis and simulation of pulsed laser heating at interface. Journal of Applied Physics, 2018, vol. 123, pp. 025301. DOI: 10.1063/1.5008963.
  17. Croat J., Chraply A.R., Herbst J.F. Crystallization of amorphous Pr0.27Co0.73: Magnetic properties and laser induced coercivity. Applied Physics Letters, 1980, vol. 37, pp. 962. DOI: 10.1063/1.91777.
  18. Molian R., Molian P. Pulsed laser deposition and annealing of Dy–Fe–B thin films on melt-spun Nd–Fe–B ribbons for improved magnetic performance. Journal of Magnetism and Magnetic Materials, 2009, vol. 321, vol. 4, pp. 241–246. DOI: 10.1016/j.jmmm.
  19. Morgunov R.B., Koplak O.V., Talantsev A.D., Korolev D.V., Piskorskij V.P., Valeev R.A. The phenomenology of the magnetic hysteresis loops in multilayer microwires α-Fe/DyPrFeCoB. Trudy VIAM, 2019, no. 7 (79), paper no. 08. Available at: http://www.viam-works.ru (accessed: October 11, 2021). DOI: 10.18577/2307-6046-2019-0-7-67-75.
  20. Koplak O.V., Kunitsyna E.I., Valeev R.A., Korolev D.V., Piskorskii V.P., Morgunov R.B. Ferromagnetic microwires α-Fe/(PrDy)(FeCo)B for micromanipulators and polymer composites. Trudy VIAM, 2019, no. 11 (83), paper no. 7. Available at: http://www.viam-works.ru (accessed: October 11, 2021). DOI: 10.18577/2307-6046-2019-0-11-60-67.
  21. Korolev D.V., Stolyankov Yu.V., Piskorsky V.P., Valeev R.A., Bahmetiev M.V., Dvorez-kaya E.V., Koplak O.V., Morgunov R.B. Magnetic properties and magnetic strip domains in micro stripes PrDyFeCoB. Aviation materials and technologies, 2021, no. 3 (64), paper no. 08. Available at: http://www.journal.viam.ru (accessed: October 11, 2021). ). DOI: 10.18577/2713-0193-2021-0-3-86-93.
  22. Gerrits Th., Van den Berg M.H.A., Hohlfeld J. et al. Ultrafast precessional magnetization reversal by picosecond magnetic field pulse shaping. Nature, 2002, vol. 418, pp. 509–512.
  23. Mangin S., Gottwald M., Lambert C.-H. et al. Engineered materials for all-optical helicity-dependent magnetic switching. Nature Materials, 2014, vol. 13, no. 3, pp. 286–292. DOI: 10.1038/nmat3864.
  24. Xu Y., Hehn M., Zhao W. et al. From single to multiple pulse all-optical switching in GdFeCo thin films. Physics Review B, 2019, vol. 100, pp. 064424.
  25. Ovcharenko S.V., Yakushenkova P.O., Ilyina N.A., Brekhova K.A., Semenova E.M., Vus Ankhua, Mishina E.D. Ultrafast switching of the magnetic state of a medium by a single femtosecond laser pulse in DyFeCo films. Fizika metallov i metallovedenie, 2019, vol. 120, no. 9, pp. 899–904.
  26. Kalashnikova A.M., Kozub V.I. Exchange scattering as the driving force for ultrafast all-optical and bias-controlled reversal in ferrimagnetic metallic structures. Physics Review B, 2016, vol. 93, pp. 054424.
  27. Shelukhin L.A., Pertsev N.A., Scherbakov A.V. et al. Laser-Induced Magnetization Precession in Individual Magnetoelastic Domains of a Multiferroic Co40Fe40B20/BaTiO3 Composite. Physical Review Applied, 2020, vol. 14, pp. 034061.
  28. Ellis O.A.M., Fullerton E.E., Chantrell R.W. All-optical switching in granular ferromagnets caused by magnetic circular dichroism. Scientific Reports, 2016, vol. 6, p. 30522.
  29. Davies C.S., Janssen T., Mentink J.H. et al. Pathways for Single-Shot All-Optical Switching of Magnetization in Ferrimagnets. Physical Review Applied, 2002, vol. 13, p. 024064.
  30. Wang C., Liu Y. Ultrafast optical manipulation of magnetic order in ferromagnetic materials. Nano Convergence, 2020, vol. 7, p. 35. DOI: 10.1186/s40580-020-00246-3.
  31. Chu K., Jin Z .Q., Chakka V.M., Liu J.P. Rapid magnetic hardening by rapid thermal annealing in NdFeB-based nanocomposites. Journal of Physics D: Applied Physics, 2005, vol. 38, no. 22, pp. 4009–4014.
  32. Kolb T., Huber F., Akbulut B. et al. Laser Beam Melting of NdFeB for the production of rare-earth magnets. 6th International Electric Drives Production Conference (EDPC), 2016, pp. 34–40. DOI: 10.1109/EDPC.2016.7851311.