About ways of structure modification of a knitted fillers for polymeric composite materials (review)

Ponomarenko L.A.
Ponomarenko L.A. About ways of structure modification of a knitted fillers for polymeric composite materials (review) // Proceedings of VIAM. 2022. No. 3. DOI: 10.18577/2307-6046-2022-0-3-54-63. URL: https://www.viam-works.ru/en/journal/2022/3/6
Keywords
weft-knitted, flat-knitted jersey, polymer composite materials, tuck and float loops, rib, mechanical properties
Abstract

Methods of modifying the structure of knitted fillers for the manufacture of polymer composite materials (PCM) are considered. The specific features of the use of tuck and float loops are described, the issues of the influence of additionally introduced threads of various compositions in the structure of knitwear on the mechanical properties of filler and PCM are considered. Special attention is paid to the rib type of interlacing of knitted fabrics, which, with a low density of filler, contributes to increasing the strength of the PCM.

Reference list
  1. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  2. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  3. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  4. Kablov E.N., Kulagina G.S., Zhelezina G.F., Lonskii S.L., Kurshev E.V. Microstructure research of the unidirectional organoplastic based on Rusar-NT aramid fibers and epoxy-polysulfone binder. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 19–26. DOI: 10.18577/2071-9140-2020-0-4-19-26.
  5. Kurnosov A.O., Vavilova M.I., Melnikov D.A. Manufacturing technologies of glass fillers and study of effects of finishing material on physical and mechanical properties of fiberglass plastics. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 64–70. DOI: 10.18577/2071-9140-2018-0-1-64-70.
  6. Belinis P.G., Donetskiy K.I., Lukyanenko Yu.V., Rogozhnikov V.N., Mayer Yu., Bystrikova D.V. Volume reinforcing solid-woven preforms for manufacturing of polymer composite materials (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 18–26. DOI: 10.18577/2071-9140-2019-0-4-18-26.
  7. Li C., Zhang R., Jia J. et al. The low-velocity impact and post-impact properties of ultra-high-molecular-weight polyethylene fiber weft plain knitted structural composites. Journal of engineered fibers and fabrics, 2019, vol. 14, pp. 1–10. DOI: 10.1177/1558925019832254.
  8. Balea L., Dusserre G., Bernhart G. Mechanical behaviour of plain-knit reinforced injected composites: effect of inlay yarns and fiber type. Composites. Part B, 2014, no. 56, pp. 20–29. DOI: 10.1016/j/compositesb.2013.07.028.
  9. Faridul Hasan K.M., Péter György Horváth, Tibor Alpár. Potential fabric-reinforced composites: a comprehensive review. Journal of Materials Science. Review, 2021, vol. 56 (1), pp. 1–7. DOI: 10.1007/s10853-021-06177-6.
  10. Dusserre G., Balea L., Bernhart G. Elastic properties prediction of a knitted composite with inlaid yarns subjected to stretching: A coupled semi-analytical model. Composites. Part A: Applied science and manufacturing, 2014, no. 64, pp. 185–193. DOI: 10.1016/j.compositesa.2014.05.007.
  11. Bogomolov I.P., Kozlov I.A., Birulya M.A. Review of modern technologies for the manufacture of volume-reinforcing preforms for promising composite materials. Tekhniko-tekhnologicheskie problemy servisa, 2017, no. 1 (39), pp. 22‒27.
  12. Truevtsev A.V., Tsobkallo E.S., Moskalyuk O.A. Quasi-continuous reinforcement of the composite with knitwear. Tekhnologiya legkoy promyshlennosti, 2016, no. 1, pp. 64–67.
  13. Zilio L., Dias M., Santos T. et al. Characterization and statistical analysis of the mechanical behavior of knitted structures used to reinforce composites: yarn compositions and float stitches. Journal of materials research and technology, 2020, no. 9 (4), p. 8323–8336. DOI: 10.1016/j.jmrt.2020.05.089.
  14. Nermin M. Aly. A review on utilization of textile composites in transportation towards sustainability. 17th World textile conference AUTEX 2017, 2017, no. 254, pp. 1–7. DOI: 10.1088/1757-899X/254/4/042002.
  15. Hu H., Zhang M., Fangueiro R., De Araujo M. Mechanical properties of composite materials made of 3D stitched woven-knitted preforms. Journal of composite materials, 2010, vol. 44, no. 14, pp. 1753–1767. DOI: 10.1177/0021998309359211.
  16. Bhosale N., Jadhav B. Weft Knitted Fabrics. 2017. Available at: http://texnote.blogspot.com/2017/01/weft-knitted-fabrics.html (accessed: October 05, 2021).
  17. Molossov K.A. Development of knitted webs for reinforcement of composite materials: thesis abstract, Cand. Sc. (Techn.). St. Petersburg, 2013, 17 p.
  18. Ishmael N., Fernando A. Textile tehnologies for the manufacture of three-dimensional textile preforms. Research Journal of Textile and Apparel, 2017, vol. 21, no. 4, pp. 342–362. DOI: 10.1108/RJTA-06-2017-0034.
  19. Bezsmertna V., Mazna O., Kohanyiy V. et al. Multifunctional polymer-based composite materials with weft-knitted carbon fibrous fillers. MATEC Web of Conferences EASN 2019, 2019, no. 304, art. 01012. DOI: 10.1051/matecconf/201930401012.
  20. Xue D., Hu H. Mechanical properties of biaxial weft-knitted flax composites. Materials and design, 2012, no. 46, p. 264–269. DOI: 10.1016/j.matdes.2012.10.019.
  21. Dalidovich A.S. Fundamentals of the theory of knitting. Moscow: Legkaya industriya, 1970. 432 p.
  22. Aisyah H.A., Paridah M.T., Sapuan S.M. et al. A comprehensive review on advanced sustainable woven natural fiber polymer composites. Polymers, 2021, vol. 13, no. 471, pp. 15–45. DOI: 10.3390/polym13030471.
  23. Liu D., Christe D., Shakibajahromi B. et al. On the role of material architecture in the mechanical behavior of knitted textiles. International Journal of Solids and Structures, 2017, no. 109, pp. 101–111. DOI: 10.1016/j.ijsolstr.2017.01.011.
  24. Tohidi Sh.D., Rocha A.M., Dencheva N.V., Denchev Z. Microstructutal-mechanical properties relationship in single polymer laminate composites based on polyamide 6. Composites. Part B, 2018, no. 153, pp. 315–324. DOI: 10.1016/j.compositesb.2018.08.106.
  25. Ravandi M., Ahlquist S., Banu M. Numerical modeling of mechanical behavior of weft-knitted carbon fiber composites. 8th European conference for aeronautics and space science (EUCASS), 2019, pp. 1–8. DOI: 10.13009/EUCASS2019-811.
  26. Haijun D., Jialu L., Ying S. et al. Electrothermal and interlaminar shear properties of weft knitted biaxial fabric/epoxy resin electrically heated composites. Acta Materiae Compositae Sinica, 2020, vol. 37, no. 8, pp. 1997–2004. DOI: 10.13801/j.cnki.fhclxb.20191129.001.
  27. Truevtsev A.V., Tsobkallo E.S., Moskalyuk O.A. Polymer composite materials with knitted filler. Modern trends in the development of chemistry and technology of polymer materials: reports IV Intern. scientific conf. St. Petersburg, 2018, pp. 57–59.
  28. Bazanova E.A., Truevtsev A.V. On the possibility of using knitwear as a filler for composites. Young scientists – the development of the national technological initiative (POISK), 2020, no. 1, pp. 21–23.
  29. Truevtsev A.V., Tsobkallo E.S., Moskalyuk O.A. Structure and properties of composites with sunken-loop knit fabric filler. Fibre Chemistry, 2018, vol. 50, no. 4, pp. 325–331. DOI: 10.1007/s10692-019-09984-5.
  30. Gunes K.S., Ince M.E., Icoglu H.I. Compressibility of weft knitted reinforcement fabrics from glass yarn. IOP Conference Series: Materials Science and Engineering, 2018, no. 460, pp. 1–6. DOI: 10.1088/1757 899X/460/1/012029.