Research of operating properties of RTV silicone sealants at elevated temperatures (up to +400 °C) and ways of their increase

Ilyukhina M.A., Timonin V.V.
Ilyukhina M.A., Timonin V.V. Research of operating properties of RTV silicone sealants at elevated temperatures (up to +400 °C) and ways of their increase // Proceedings of VIAM. 2022. No. 3. DOI: 10.18577/2307-6046-2022-0-3-44-53. URL: https://www.viam-works.ru/en/journal/2022/3/5
Keywords
silicone sealants, thermal ageing, thermogravimetric analysis
Abstract

On the basis of a number of research works results on heat ageing of silicone sealants VIKSINT were received. Test results after heat ageing of plates of sealants and samples of the sealants brought on metal are presented. Temperature dependences of properties of sealants on speed and duration of thermal ageing are shown. Resources of work of sealants are defined at various temperatures. Ways of increase of operating properties of silicone sealants are considered.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Chemistry in aviation materials science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, noo. 1, pp. 3–4.
  3. Kolobkov A.S. Polymer composite materials for various aircraft structures (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 05. Available at: http://www.viam-works.ru (accessed: November 2, 2021). DOI: 10.18577/2307-6046-2020-0-67-38-44.
  4. Minasyan R.M. Silicone one-component adhesive-sealants. Vse materialy. Entsiklopedicheskiy spravochnik, 2010, no. 10, pp. 31–34.
  5. Sharova I.A., Petrova A.P. Review of world adhesive and sealant conference (WAC-2012, France. Trudy VIAM, 2013, no. 8, paper no. 06. Available at: http://www.viam-works.ru (accessed: November 2, 2021).
  6. Kablov E.N. VIAM: materials of new generation for PD-14. Krylya Rodiny. 2019, no. 7–8, pp. 54–58.
  7. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  8. Chigorina E.A., Arutyunyantc A.A., Bestaev M.V., Chigorina T.M., Abaev V.T. Organosiloksanovye glues-sealants with the increased physicomechanical properties. Klei. Germetiki. Tekhnologii, 2018, no. 1, pp. 24–27.
  9. Gosh D., Khastgir D. Degradation and stability of polymeric high-voltage insulators and prediction of their service life through environmental and accelerated aging processes. ACS Omega, 2018, no. 3, pp. 11317–11330.
  10. Savenkova A.V. Sealants with increased heat and frost resistance. Klei. Germetiki. Tekhnologii, 2008, no. 3, pp. 13–15.
  11. Startsev V.O. Methods for studying the aging of polymer binders. Klei. Germetiki. Tekhnologii, 2020, no. 9, pp. 16–26.
  12. Eliseev O.A., Glazov P.A., Ilyukhina M.A. Study of the kinetics of thermal decomposition of vulcanizates of low molecular weight organosilicon rubbers. Klei. Germetiki. Tekhnologii, 2015, no. 6, pp. 18–21.
  13. Shitov R.O., Kitaeva N.S., Shiryakina Yu.M., Kurshev E.V. Research of influence of modifiers of varied nature on the thermo-oxidative stability of a model silicone binder. Trudy VIAM, 2020, no. 6–7 (89), paper no. 03. Available at: http://www.viam-works.ru (accessed: February 10, 2021). DOI: 10.18577/2307-6046-2020-0-67-19-28.
  14. Lukina N.F., Petrova A.P., Kotova E.V. Heat-resistent adhesives used in aviation and space technique. Trudy VIAM, 2014, no. 3, paper no. 06. Available at: http://www.viam-works.ru (accessed: November 2, 2021). DOI: 10.18577/2307-6046-2014-0-3-6-6.
  15. Kireev V.V., Dyachenko B.I., Rybalko V.P. Structure and thermo-oxidative transformations of polymethylsesquioxanes. Vysokomolekulyarnyye soyedineniya. Ser.: A, 2008, vol. 50, no. 4, p. 614.
  16. Bonding in mechanical engineering: reference book: in 2 vols. Ed. G.V. Malyshev. Moscow: Nauka i tekhnologii, 2005, vol. 1, pp. 87–97.
  17. Khananashvili L.M., Andrianov K.A. Technology of organoelement monomers and polymers. Moscow: Khimiya, 1983, p. 416.
  18. Neelova O.V., Gazzaeva R.A. Curing system for polyorganosiloxane compositions. Klei. Germetiki. Tekhnologii, 2016, no. 9, pp. 2–8.
  19. Hamdani S., Longuet C., Perrin D., Lopez-cuesta J.-M. Flame retardancy of silicone-based materials: Review. Polymer Fegradation and Stability, 2009, vol. 94, no. 4, pp. 465–495. DOI: 10.1016/j.polymerdegradstab.2008.11.019.
  20. Kim Y., Joeng H., Lee K.W. Mechanical and Thermal Properties of Environmentally Benign Silicone Foam Filled with Wollastonite. Elastomers and Composites, 2020, vol. 55, no. 4, pp. 300–305.
  21. Wong J.F., Chan J.X., Hassan A., Mohamad Z. Thermal and flammability properties of wollastonite-filled thermoplastic composites: a review. Journal of Materials Science, 2021, vol. 56, no. 2, pp. 1–40.
  22. Liao Y., Weng Y., Wang J. Silicone rubber composites with high breakdown strength and dielectric loss based on polydopamine coated mica. Polymers, 2019, vol. 11, no. 12. DOI: 10.3390/polym11122030.
  23. Wang J., Ji C., Yan Y., Zhao D. Mechanical and ceramifiable properties of silicone rubber filled with different inorganic fillers. Polymer Degradation and Stability, 2015, no. 121, pp. 149–156.
  24. Zubareva A.N., Utkin A.V., Mochalova V.M., Efremov V.P. Experimental study of spall strength of silicon rubber with microspheres under shock-wave action. Journal of Physics Conference Series, 2020, no. 1556, art. 012026. Available at: http://www.iopscience.iop.org (accessed: November 2, 2021). DOI: 10.1088/1742-6596/1556/012026.
  25. Montazeri Sh., Ranjbar Z., Osati M. Preparation and characterization of a thermal barrier heat-resistant silicone coating. Progress in Color, Colorants and Coatings, 2020, vol. 15, pp. 65–73.
  26. Zhang J., Jiang G., Tianhao H. et al. Synthesis and performance of polyurethane/silicon oxide nano-composite coatings. Science and Engineering of Composite Materials, 2019, vol. 26, is. 1, pp. 301–307.
  27. Ivakhnenko Yu.A., Baruzdin B.V., Varrik N.M., Maksimov V.G. High-temperature fibrous sealing materials. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 272–289. DOI: 10.18577/2071-9140-2017-0-S-272-289.