Influence of long climatic aging on microstructure of surface of organic glass in semi-arid and subtropical climate
UDC
620.1:53.093:53.096
DOI
10.18577/2307-6046-2022-0-3-15-26
Article PDF (Russian)
(1.97 MB)
How to cite
Kurshev E.V., Lonskii S.L., Mekalina I.V. Influence of long climatic aging on microstructure of surface of organic glass in semi-arid and subtropical climate // Proceedings of VIAM. 2022. No. 3. DOI: 10.18577/2307-6046-2022-0-3-15-26. URL: https://www.viam-works.ru/en/journal/2022/3/2
Keywords
polymethyl methacrylate glazing AO-120, microstructural researches, microphase structure, climatic zones, atmospheric factors, aviation engineering, glazing details
Abstract
Products from organic glasses are widely used in aviation engineering for different types of glazing which work in difficult operational conditions, for example, are exposed to influence of low and high temperatures, moisture, ultra-violet radiation, etc. These factors can influence operational reliability of organic glass. Now application of the oriented polymethyl methacrylate AO-120 organic glass is most widespread in designs of aviation glazing. In the real work results of research of microstructure of surfaces of the AO-120 or-ganic glass which has undergone long influence of atmospheric factors in different climatic zones of the USA (Arizona and Florida) are provided.
Reference list
- Gudimov M.M., Perov B.V. Organic glass. Moscow: Khimiya, 1981, 215 p.
- Gudimov M.M. Silver cracks on organic glass. Moscow: TsIPKK AP, 1997, 260 p.
- Aviation materials: reference book: in 13 vols. Ed. E.N. Kablov. Moscow: VIAM, 2002, vol. 8, pp. 29–51.
- Sentyurin E.G., Kuklina L.S., Trigub T.S., Pashkova T.V. Influence of weather resistance on the operational reliability of plexiglass. Aviatsionnaya promyshlennost, 1984, no. 5, pp. 56–58.
- Gudimov M.M., Sentyurin E.G., Trigub T.S. Silver resistance of organic glass aircraft glazing during its production and operation. Aviatsionnaya promyshlennost, 1995, no. 9–10. pp. 55–60.
- Kirillov V.N., Kavun N.S., Rakitina V.P. et al. Study of the influence of heat and moisture impact on the properties of epoxy fiberglass. Plasticheskiye massy, 2008, no. 9, pp. 14–18.
- Startsev O.V., Prokopenko K.O., Litvinov A.A., Krotov A.S., Anikhovskaya V.I., Dement’eva L.A. Investigation of thermal moisture aging of aviation fiberglass. Vse materialy. Entsiklopedicheskiy spravochnik, 2010, no. 1, pp. 21–25.
- Deev I.S., Kurshev E.V., Lonskii S.L., Zhelezina G.F. Influence of long-term climatic aging on the microstructure of the surface of epoxy organic plastics and the nature of its destruction under bending conditions. Voprosy materialovedeniya, 2016, no. 3 (87). pp. 104–114.
- Laptev A.B., Nikolaev E.V., Kurshev E.V., Goryashnik Yu.S. Features of biodegradation of thermoplastics based on polyesters in different climatic zones. Trudy VIAM, 2019, no. 7 (79), paper no. 10. Available at: http://www.viam-works.ru (accessed: Octobetr14, 2021). DOI: 10.18577/2307-6046-2019-0-7-84-91.
- Laptev A.B., Barbotko S.L., Nikolaev E.V. The main research areas of the persistence properties of materials under the influence of climatic and operational factors. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 547–561. DOI: 10.18577/2071-9140-2017-0-S-547-561.
- Lutsenko A.N., Kurs M.G., Laptev A.B. Justification of the timing of full-scale climatic tests of metallic materials in the atmosphere of the Black Sea coast. Analytical review. Voprosy materialovedeniya, 2016, no. 3, pp. 126–137.
- Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58.
- Mekalina I.V., Aizatulina M.K., Sentjurin E.G., Popov A.A. Features of influence of atmospheric factors on aviation organic glass. Trudy VIAM, 2018, no. 11 (71), paper no. 04. Available at: http://www.viam-works.ru (accessed: May 04, 2021). DOI: 10.18577/2307-6046-2018-0-11-28-34.
- Deev I.S., Kuklin E.A. Features of the formation of the microphase structure of polymethyl methacrylate organic glasses and its changes under aging conditions. Materialovedenie, 2014, no. 4. S. 43–50.
- Deev I.S., Kobets L.P. Structure formation in filled thermosetting polymers. Kolloidnyy zhurnal, 1999, vol. 61, no. 5, pp. 650–660.
- Novikov V.U., Kozitsky D.V., Deev I.S., Ivanova V.S., Kobets L.P. Multifractal analysis of the structure of polymethyl methacrylate studied by scanning electron microscopy. Plasticheskiye massy, 2001, no. 1. S. 7–9.
- Deev I.S., Kobets L.P. Microstructure of epoxy matrices. Mekhanika kompozitnykh materialov, 1986, no. 1, pp. 3–8.
- Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
- Kablov E.N. Materials and chemical technologies for aviation equipment. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, рр. 520–530.
- Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Reports of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Renby B., Rabek Y. Photodestruction, photooxidation, photostabilization of polymers. Moscow: Mir, 1978, 676 p.
- Sentyurin E.G., Gudimov M.M., Rudnev V.P. et al. Aging of organic glass. Aviatsionnaya promyshlennost, 1993, no. 5–6. pp. 50–53.