Modeling and prediction of overheating temperatures of PVC profile samples

Panin S.V.
Panin S.V. Modeling and prediction of overheating temperatures of PVC profile samples // Proceedings of VIAM. 2022. No. 3. DOI: 10.18577/2307-6046-2022-0-3-135-144. URL: https://www.viam-works.ru/en/journal/2022/3/12
Keywords
full-scale climatic tests, structurally similar samples, PVC-profile, surface heating, surface overheating, modeling, forecasting
Abstract

The main purpose of this work was to simulate the temperatures of maximum heating of PVC-profile samples in the climatic conditions of the city of Gelendzhik and their modeling in other climatic conditions (the city of Moscow). The work evaluates the maximum heating temperatures of the surface of PVC-profile samples having a complex spatial shape, evaluates various approaches to its modeling and forecasting in other climatic conditions. The possible influence of the shape of the samples on the processes of their heat exchange with the environment is noted.

Reference list
  1. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  2. Kablov E.N., Startsev V.O., Inozemtsev A.A. The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  3. Startsev O.V., Medvedev I.M., Kurs M.G. Hardness as the indicator of corrosion of aluminum alloys in sea conditions. Aviacionnye materialy i tehnologii, 2012, no. 3, pp. 16–19.
  4. Abramova M.G., Lutsenko A.N., Varchenko E.A. Concerning the aspects of validation of climate resistance of airborne materials at all life cycle stages (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 86–94. DOI: 10.18577/2071-9140-2020-0-1-86-94.
  5. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of aviation composite materials. I. Mechanisms of aging. Deformatsiya i razrusheniye materialov, 2010, no. 11, pp. 19–26.
  6. Startsev V.O., Medvedev I.M., Startsev O.V. Рrognostication of surface temperature of epoxy coatings on aluminum alloy subjected to long exposure in natural climate conditions. Trudy VIAM, 2016, no. 10, paper no. 12. Available at: http://www.viam-works.ru (accessed: November 26, 2021). DOI: 10.18577/2307-6046-2016-0-10-12-12.
  7. Guedes Soares C., Garbatov Y., Zayed A., Wang G. Influence of environmental factors on corrosion of ship structures in marine atmosphere. Corrosion Science, 2009, vol. 51, no. 9, pp. 2014–2026.
  8. Grossman P.R. Investigation of atmospheric exposure factors that determine time of wetness of outdoor structures. ASTM International, 1978, pp. 5–16.
  9. Gardiner C.P., Melchers R.E. Enclosed atmospheric corrosion in ship spaces. British Corrosion Journal, 2003, vol. 6, no. 4, pp. 272–276.
  10. Al-Rawahi N.Z., Zurigat Y.H., Al-Azri N.A. Prediction of hourly solar radiation on horizontal and inclined surfaces for Muscat/Oman. The Journal of Engineering Research, 2011, vol. 8, no. 2, pp. 19–31.
  11. Bijl P. Modelling of sample surface temperature in an outdoor weathering test. Polymer Testing, 2011, vol. 30, no. 5, pp. 485–492.
  12. Burch D.M., Martin J.W. Predicting the Temperature and Relative Humidity of Polymer Coatings in the Field. Service Life Prediction of Organic Coatings ACS Symposium Series. American Chemical Society, 1999, pp. 85–107.
  13. Burch D., Martin J., Van Landingham M. Computer analysis of a polymer coating exposed to field weather conditions. Journal of Coatings Technology, 2002, vol. 74, no. 924, pp. 75–86.
  14. Pickett J.E., Sargent J.R. Sample temperatures during outdoor and laboratory weathering exposures. Polymer Degradation and Stability, 2009, vol. 94, no. 2, pp. 189–195.
  15. Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples’ temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577 / 2071-9140-2020-0-4-47-58.