Methods of mechanical and electrical discharge machining of polymer composite materials (review)

Dyshenko V.S., Donetskiy K.I., Minibaev M.I., Ablyaz T.R., Shlykov E.S., Shiryaev V.V.
Dyshenko V.S., Donetskiy K.I., Minibaev M.I., Ablyaz T.R., Shlykov E.S., Shiryaev V.V. Methods of mechanical and electrical discharge machining of polymer composite materials (review) // Proceedings of VIAM. 2022. No. 3. DOI: 10.18577/2307-6046-2022-0-3-102-120. URL: https://www.viam-works.ru/en/journal/2022/3/10
Keywords
polymer composite materials, electrical discharge machining processing technology, milling of composites, abrasive water jet cutting, cutting, abrasive, delamination
Abstract

Polymer composite materials (PCM) are increasingly being used in various industries. At the same time, knowledge of PCM processing is needed in order not to negate these advantages. An overview of traditional PCM processing methods is presented: cutting with abrasive wheels with and without cooling, milling on a numerically controlled machine, as well as such unconventional methods as: abrasive water jet cutting (AWG) and electrical discharge machining (EDM). Technological features, comparison of cutting modes are described and technological techniques are disclosed.

Reference list
  1. Kablov E.N. Marketing of materials science, aircraft building and industry: present and future. Direktor po marketingu i sbuty, 2017, no. 5–6. pp. 40–44.
  2. Kablov E.N. Materials and chemical technologies for Aircraft Engineering. Herald of the Russian Academy of Sciences, 2012, vol. 82, no. 3, pp. 158–167.
  3. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
  4. Kablov E.N., Sagomonova V.A., Sorokin A.E., Tselikin V.V., Gulyaev A.I. Study of the structure and properties of a polymer composite material with an integrated vibration-absorbing layer. Vse materialy. Encyklopedicheskiy spravochnik, 2020, no. 3, pp. 2–9.
  5. Kablov E.N., Valueva M.I., Zelenina I.V., Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: December 1, 2021). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  6. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  7. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 1. Automated Tape Laying (ATL). Aviation materials and technologies, 2021, no. 2 (63), paper no. 06. Available at: http://www.journal.viam.ru (accessed: October 5, 2021). DOI: 10.18577/2713-0193-2021-0-2-51-61.
  8. Sidorina A.I. Multiaxial carbon fabrics in the products of aviation technology (review). Aviation materials and technologies, 2021, no. 3 (64), paper no. 10. Available at: http://www.journal.viam.ru (accessed: October 11, 2021). DOI: 10.18577/2713-0193-2021-0-3-105-106.
  9. Bolshakov V.A., Solodilov V.I., Korokhin R.A., Kondrashov S.V., Merkulova Yu.I., Dyachkova T.P. Research of crack resistance of polymeric composite materials fabricated by infusion using various concentrates on the basis of modified CNT. Trudy VIAM, 2017, no. 7 (55), paper no. 9. Available at: http://www.viam-works.ru (accessed: December 1, 2021). DOI: 10.18577/2307-6046-2017-0-7-9-9.
  10. Kerber M.L., Vinogradov V.M., Golovkin G.S. et al. Polymer composite materials: structure, properties, technology: textbook. St. Petersburg: Professiya, 2008, 560 p.
  11. Bataev A.A., Bataev V.A. Composite materials: structure, production, application: textbook. Novosibirsk: NGTU, 2002, 384 p.
  12. Vashukov Yu.A. Technology of rocket and aerospace structures from composite materials:a multimedia educational module. Electronic, text and graph. dates (3766 KB, printed version 185 pages). Samara, 2012. CD-R.
  13. Stepanov A.A., Shemelov Yu.Yu. Cutting organoplastic with circles of diamonds and electrocorundum. Sverkhtverdye materily, 1980, no. 3, pp. 37–41.
  14. Tokarev D.I., Matygulina E.V. Machining of plastics: textbook. Perm: Publishing House Perm Nat. Research Polytech. University, 2019, 71 p.
  15. Vorobey V.V. Technology for the production of structures from composite materials. Moscow: MAI publishing house, 1996, 178 p.
  16. Tikhomirov R.A., Nikolaev V.I. Mechanical processing of plastics. Leningrad: Mashinostroenie, 1975, 208 p.
  17. Piece B.P. Machining of plastics: handbook. Moscow: Mashinostroenie, 1987, 152 p.
  18. Yaroslavtsev V.M. Machining of polymer composite materials: textbook. Moscow: Publ. house of MSTU im. N.E. Bauman, 2012, pp. 32–58.
  19. Minibaev M.I., Raskutin A.E, Goncharov V.A. Peculiarities of technology production specimens of PCM on CNC machines (review). Trudy VIAM, 2019, no. 1 (73), paper no. 11. Available at: http://www.viam-works.ru (accessed: October 11, 2021). DOI: 10.18577/2307-6046-2019-0-1-105-114.
  20. Sheikh-Ahmad J.Y. Machining of Polymer Composites. Springer Science Business Media, 2009, 307 p.
  21. Zeng J., Kim T.J. Development of an abrasive water jet kerf cutting model for brittle materials // Jet Cutting Technology. Fluid Mechanics and Its Applications. Dordrecht: Springer, 1992, vol. 13. pp. 483–501. DOI: 10.1007/978-94-011-2678-6_33.
  22. Dyshenko V.S., Raskutin A.E., Donetskskii K.I., Karavaev R.Yu. Hydroabrasive cutting of carbon plastic based on woven preforms. Tekhnologii i kachestvo, 2018, no. 2 (40), pp. 32–36.
  23. Ablyaz T.R., Shlykov E.S., Muratov K.R. Improving the Efficiency of Electrical Discharge
  24. Machining of Special-Purpose Products with Composite Electrode Tools. Materials, 2021, vol. 14, is. 20, art. 6105. DOI: 10.3390/ma14206105.
  25. Ablyaz T.R., Shlykov E.S., Muratov K.R., Sidhu S.S. Analysis of Wire-Cut Electro Discharge Machining of Polymer Composite Materials. Micromachines, 2021. vol. 12, is. 5, art. 571. DOI: 10.3390/mi12050571.
  26. Hsissou R., Benhiba F., Echihi S. et al. New epoxy polymer composites as a potential anticorrosive coatings for carbon steel in 3.5 % NaCl solution: Experimental and computational approa-ches. Chemical Data Collections, 2021, vol. 31, art. 100619. DOI: 10.1016/j.cdc.2020.100619.
  27. Hsissou R., Bekhta A., Dagdag O. et al. Rheological properties of composite polymers and hybrid nanocomposites. Heliyon, 2020, vol. 6, is. 6, art. e04187. DOI: 10.1016/j.heliyon.2020.e04187.
  28. Thomason J. A review of the analysis and characterization of polymeric glass fibresizings. Polymer Testing, 2020, vol. 85, art. 106421. DOI: 10.1016/j.polymertesting.2020.106421.
  29. Gunyayeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.