Use of metal powder compositions to remove defects of parts from VAS-1 alloy by cold gas-dynamic spraying method

Kozlov I.A., Fomina M.A., Dyomin S.A., Benarieb I., Khmeleva K.M.
Kozlov I.A., Fomina M.A., Dyomin S.A., Benarieb I., Khmeleva K.M. Use of metal powder compositions to remove defects of parts from VAS-1 alloy by cold gas-dynamic spraying method // Proceedings of VIAM. 2022. No. 12. DOI: 10.18577/2307-6046-2022-0-12-96-106. URL: https://www.viam-works.ru/en/journal/2022/12/9
Keywords
repair, CGN-coatings, additive technologies, aluminum coatings, Dimet-405, gas-dynamic spraying
Abstract

During the operation of aircraft parts, internal stresses may occur, leading to the appearance of cracks, as well as the formation of defects due to impact loads, which can lead to the destruction of the part and structure. The method of cold gas-dynamic spraying (CGS) of metals makes it possible not only to apply various protective and functional coatings, but also, when using plastic materials, to effectively eliminate defects in parts and assemblies for various purposes.

Reference list
  1. Kablov E.N. Additive technologies – the dominant of the national technological initiative. Intellekt i tekhnologii, 2015, no. 2 (11), pp. 52–55.
  2. Ryabov D.K., Antipov V.V., Korolev V.A., Medvedev P.N. Effect of technological factors on structure and properties of Al–Si alloy obtained by selective laser melting. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 44–51. DOI: 10.18577/2071-9140-2016-0-S1-44-51.
  3. Ryabov D.K., Morozova L.V., Korolev V.A., Ivanova A.O. Alternation of mechanical features of alloy AK9ch manufactured by selective laser melting. Trudy VIAM, 2016, no. 9, paper no. 02. Available at: http://www.viam-works.ru (accessed: August 08, 2022). DOI: 10.18577/2307-6046-2016-0-9-2-2.
  4. Sercombe T., Schaffer G. Rapid manufacturing of aluminum components. Science, 2003, vol. 301 (5637), pp. 1225–1227.
  5. Bremen S., Meiners W., Diatlov A. Selective Laser Melting. Laser Technic Journal, 2012, vol. 9 (2), pp. 33–38.
  6. Kablov E.N. What is the future to be made of? Materials of a new generation, technologies for their creation and processing – the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  7. Ivanova A.O., Ryabov D.K., Antipov V.V., Pahomkin S.I. Application of Thermo-Calc software for determination of parameters of heat treatment 1913 alloy and temperatures of gas atomization for aluminium alloys. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 52–59. DOI: 10.18577/2071-9140-2016-0-S1-52-59.
  8. Akopyan T.K., Zolotorevsky V.S., Khvan A.V. Calculation of phase diagrams of Al–Cu–Zn–Mg and Al–Cu–Zn–Mg–Fe–Si systems. Tsvetnaya metallurgiya, 2013, no. 3, pp. 44–51.
  9. Ivanova A.O., Vahromov R.O., Grigor'ev M.V., Senatorova O.G. Effect of small additive of silver on structure and properties of Al–Cu–Mg alloys. Trudy VIAM, 2014, no. 10, paper no. 01. Available at: http://www.viam-works.ru (accessed: August 08, 2022). DOI: 10.18577/2307-6046-2014-0-10-1-1.
  10. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  11. Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  12. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  13. Kablov E.N., Kutyrev A.E., Vdovin A.I., Kozlov I.A., Afanasyev-Khodykin A.N. The research of possibility of galvanic corrosion in brazed connections used in aviation engine construction. Aviation materials and technologies, 2021, no. 4 (65), paper no. 01. Available at: http://www.journal.viam.ru (accessed: May 12, 2022). DOI: 10.18577/2713-0193-2021-0-4-3-13.
  14. Aleksandrov D.A., Muboyadzhyan S.A., Lutsenko A.N., Zhuravleva P.L. Hardening of the surface of titanium alloys by ion implantation method and ionic modification. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 33–39. DOI: 10.18577/2071-9140-2018-0-2-33-39.
  15. Plokhikh A.I., Safonov M.D., Kolesnikov A.G., Karpukhin S.D. Mechanism of interlaminar stress relaxation in multilayer steel materials. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 26–32. DOI: 10.18577/2071-9140-2018-0-2-26-32.
  16. Kurs M.G., Nikolayev E.V., Abramov D.V. Full-scale and accelerated tests of metallic and nonmetallic materials: key factors and specialized stands. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 66–73. DOI: 10.18577/2071-9140-2019-0-1-66-73.
  17. Kozlov I.A., Leshchev K.A., Nikiforov A.A., Demin S.A. Cold spray coatings (review). Trudy VIAM, 2020, no. 8 (90), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 08, 2022). DOI: 10.18577/2307-6046-2020-0-8-77-93.
  18. Kosarev V.F., Alkhimov A.P. Technology, equipment, tools. Obrabotka metallov, 2003, no. 3, pp. 28–30.
  19. Alkhimov A.P., Gulidov A.I., Kosarev V.F., Nesterovich N.I. Peculiarities of deformation of microparticles upon impact with a solid barrier. Prikladnaya mekhanika i tekhnicheskaya fizika, 2000, vol. 41, no. 1, pp. 204–209.
  20. Alkhimov A.P., Klinkov S.V., Kosarev V.F., Fomin V.M. Cold gas-dynamic spraying. Theory and practice. Moscow: Fizmatlit, 2010, pp. 25–27.