Rubber-based sealants (review)

Pravada E.S., Vakhrusheva Ja.A., Gerasimov D.M., Chaykun A.М.
Pravada E.S., Vakhrusheva Ja.A., Gerasimov D.M., Chaykun A.М. Rubber-based sealants (review) // Proceedings of VIAM. 2022. No. 12. DOI: 10.18577/2307-6046-2022-0-12-14-26. URL: https://www.viam-works.ru/en/journal/2022/12/2
Keywords
sealants, special purpose rubbers, polymer combination, adhesion, sealing of critical products, elastomeric sealing materials
Abstract

The review is devoted to rubbers used in the production of sealing materials (sealants). According to literary sources and experimental works, the dependences of the properties of sealing materials on the structure of rubbers are analyzed, general requirements for sealants used in critical products are identified. The assessment of rubbers used in sealing materials for aviation purposes and their main technical characteristics is given. The prospects of using combined polymers (rubbers) in the production of sealants for critical products have been revealed.

Reference list
  1. Smyslova R.A., Kotlyarova S.V. Reference manual for sealing materials based on rubbers. Moscow: Chemistry, 1976, 72 p.
  2. Zaikin A.E., Sofina S.Yu., Stoyanov O.V. Polymer tapes with an adhesive layer for anticorrosive insulation of pipelines. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2010, no. 6, pp. 98–112.
  3. Performed adhesive compositions: pat. 617614 US, no. 4581092; filed 05.06.84; publ. 08.04.86.
  4. Minibaeva L.A., Murtazina L.I., Galimzyanova R.Yu., Khakimullin Yu.N. Influence of the nature and content of calcium carbonate on the deformation-strength properties of non-cured sealants based on nitrile rubber. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2013, no. 9, pp. 105–107.
  5. Kablov E.N. The sixth technological order. Nauka i zhizn, 2010, no. 4, pp. 2–7.
  6. Shitov R.O., Kitaeva N.S., Shiryakina Yu.M., Kurshev E.V. Research of influence of modifiers of varied nature on the thermo-oxidative stability of a model silicone binder. Trudy VIAM, 2020, no. 6–7 (89), paper no. 03. Available at: http://www.viam-works.ru (accessed: July 08, 2022). DOI: 10.18577/2307-6046-2020-0-67-19-28.
  7. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  8. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. XX Mendeleev Congress on General and Applied Chemistry: abstracts. reports. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
  9. History of aviation materials science. VIAM – 80 years: years and people. Ed. E.N. Kablov. Moscow: VIAM, 2012, pp. 346–348.
  10. Kablov E.N. Aerospace materials science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
  11. Kablov E.N. Chemistry in aviation materials science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 3–4.
  12. Kablov E.N. Materials for aerospace engineering. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
  13. What is the future to be made of? Materials of a new generation, technologies for their creation and processing – the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  14. Kurshev E.V., Lonskii S.L., Mekalina I.V. Influence of long climatic aging on microstructure of surface of organic glass in semi-arid and subtropical climate. Trudy VIAM, 2018, no. 3 (109), paper no. 02. Available at: http://www.viam-works.ru (accessed: July 08, 2022). DOI: 10.18577/2307-6046-2022-0-3-15-26.
  15. Silaeva A.A., Kuznetsova V.A., Zheleznyak V.G., Kurshev E.V. Research of adhesion and adhesive durability of functional paint coatings for protection of polimer composite surface. Trudy VIAM, 2021, no. 9 (103), paper no. 06. Available at: http://www.viam-works.ru (accessed: July 08, 2022). DOI: 10.18577/2307-6046-2021-0-9-59-66.
  16. A large guide rubberman: in 2 parts. Eds. S.V. Reznichenko, Yu.L. Morozov. Moscow: Tekhinform, 2012, part 2: Rubbers and rubber products, 648 p.
  17. Lisanevich M.S., Galimzyanova R.Yu., Rusakova S.N. Curing type hot melt sealants based on butyl rubber and ethylene-vinyl acetate copolymer. Klei. Germetiki. Tekhnologii, 2018, no. 4, pp. 9–12.
  18. Rusanova S.N. Modification of ethylene copolymers with polar comonomers by saturated alkoxysilanes: thesis, Dr. Sc. (Chem.). Kazan, 2017, 219 p.
  19. Ignatov A.V. Modern achievements in the field of adhesives and sealants. Klei. Germetiki. Tekhnologii, 2015, no. 11, pp. 35–39.
  20. Griadunova Yu.E., Nikulin S.S., Belykh A.G., Posanchukov D.P. Increasing the performance of sealing compositions by electric fields. Klei. Germetiki. Tekhnologii, 2018, no. 4, pp. 35–39.
  21. Kardashov D.A. Adhesives and sealants. Moscow: Chemistry, 1978, 200 p.
  22. Eremenko V.N. Physical chemistry of condensed phases, superhard materials and their interfaces. Kyiv: Naukova dumka, 1975, 231 p.
  23. Imamutdinov I.V., Galimzyanova R.Yu., Khakimullin Yu.N. Sealants based on elastomers. Vestnik tekhnologicheskogo universiteta, 2015, vol. 18, no. 6, pp. 69–74.
  24. Agayants I.M. Five centuries of rubber and rubber. Moscow: Modern-A, 2002, 432 p.
  25. Garmonov I.V. Synthetic rubber. Leningrad: Chemistry, 1976, 752 p.
  26. Bryk Ya.A., Smirnov D.N. Research of frost resistance of aeronautical sealants. Trudy VIAM, 2018, no. 1 (61), paper no. 09. Available at: http://www.viam-works.ru (accessed: July 8, 2022). DOI: 10.18577/2307-6046-2018-0-1-9-9.
  27. A large guide rubberman: in 2 parts. Eds. S.V. Reznichenko, Yu.L. Morozov. Moscow: Tekhinform, 2012, part 1: Rubbers and ingredients, 744 p.
  28. Irzhak V.I. Topological structure of polymers. Kazan: Publishing House of KNRTU, 2013, 520 p.
  29. Irzhak V.I. Polymer architecture. Moscow: Nauka, 2012, 367 p.
  30. Kuleznev V.N., Shershnev V.A. Chemistry and physics of polymers. St. Petersburg: Lan, 2014, 368 p.
  31. Todmor Z., Gogos K. Theoretical foundations of polymer processing. Moscow: Chemistry, 1984, 632 p.
  32. Perfil'eva S.A., Shashok Zh.S., Uss E.P. and other Confectionary stickiness of filled rubber mixtures with petroleum resins. Klei. Germetiki. Tekhnologii, 2020, no. 3, pp. 21–26. DOI: 10.31044/1813-7008-2020-0-3-21-26.
  33. Voyutsky S.S. Autohesion and adhesion of polymers. Moscow: Rostekhizdat, 1960, 244 p.
  34. Vasenin R.M. Adhesion of polymers. Moscow: Publishing House of the Academy of Sciences of the USSR, 1963, pp. 17–22.
  35. Chalykh A.E. Diffusion in polymer systems. Moscow: Chemistry, 1987, 311 p.
  36. Stroilov S.V., Lyusova L.R., Glagolev V.A. Adhesive compositions with permanent tack based on nitrile rubber. Vestnik MITHT, 2009, vol. 4, no. 2, pp. 24–27.
  37. Bryk Ya.A., Eliseev O.A., Smirnov D.N. Corrosion protection of magnesium alloys polysulphide sealants. Trudy VIAM, 2017, no. 10 (58), paper no. 10. Available at: http://www.viam-works.ru (accessed: July 08, 2020). DOI: 10.18577/2307-6046-2017-0-10-10-10.
  38. Zakharov V.P., Ganiev G.M., Tereshchenko K.A., Utilin N.V. Perspective technological solutions for the production of low molecular weight butyl rubber used as the basis of sealants. Klei. Germetiki. Tekhnologii, 2016, no. 12, pp. 11–15.
  39. Technology of rubber: compounding and testing. Ed. J.S. Dick. St. Petersburg: Nauchnye osnovy i tekhnologii, 2010, 620 p.
  40. Vagin S.Yu., Vasin V.P., Zdorikova G.A., Rudakova T.A. Flame-retardant vibration damping material. Pozharovzryvobezopasnost, 2010, vol. 19, no. 10, pp. 13–17.
  41. Slobodkina K.N., Rudakov A.A., Makarov T.V., Wolfson S.I. Oil and petrol resistant sealing compositions based on nitrile rubber and thiokol. Klei. Germetiki. Tekhnologii, 2015, no. 5, pp. 12–14.
  42. Kornev A.E., Bukanov A.M., Sheverdyaev O.N. Technology of elastomeric materials: a textbook for universities. Moscow: NPPA "Istek", 2009, 504 p.
  43. Murtazina L.I., Gariffulin A.R., Nikultsev I.A. et al. Effect of calcium carbonate on the properties of non-curing sealants based on ethylene propylene diene rubber and thermoplastics. Klei. Germetiki. Tekhnologii, 2015, no. 1, pp. 21–26.
  44. Murtazina L.I., Garifullin A.R., Nikultsev I.A. et al. Non-curing sealants of high filling based on ethylene propylene diene rubber. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2013, no. 24, pp. 71–73.
  45. Ososhnik I.A., Shutilin Yu.F., Karmanova O.V. Manufacture of rubber technical products. Voronezh: Voronezh State Technol. Acad., 2007, 972 p.
  46. Fedyukin D.P., Makhles F.A. Technical and technological properties of rubbers. Moscow: Chemistry, 1985, 240 p.
  47. Tager A.A. Physico-chemistry of polymers. Moscow: Scientific world, 2007, 576 p.
  48. Meyer K.H. Propriétés de polymères en solution XVI. Interprétation statistique des propriétés thermodynamiques de systèmes binaires liquides. Helvetica Chimica Acta, 1940, vol. 23, no. 1, pp. 1063–1070. DOI: 10.1002/hlca.194002301130.
  49. Baramboim N.K. Mechanochemistry of macromolecular compounds. Moscow: Chemistry, 1971, 364 p.
  50. Shvarts A.G., Ginzburg B.N. Combination of rubbers with plastics and synthetic resins. Moscow: Chemistry, 1972, 224 p.
  51. Bogdanov V.V., Torner R.V., Krasovsky V.N., Reger E.O. Mixing polymers. Leningrad: Chemistry, 1979, 192 p.
  52. Gelfman M.I., Kovalevich O.V., Yustratov V.P. Colloidal chemistry. St. Petersburg: Lan, 2010, 336 p.
  53. Bohn K. Die Einfriertemperatur des Polyäthylens. Kolloid-Zeitschrift und Zeitschrift für Polymere, 1964, no. 1, pp. 10–15.
  54. Berlin A.A., Wolfson S.A., Oshmyan V.G., Enikolopov N.S. Principles of creation of composite polymeric materials. Moscow: Chemistry, 1990, 240 p.
  55. Perry E. Block polymers of styrene and acrylonitrile. Journal of Applied Polymer Science, 1964, vol. 8, no. 6, pp. 2605–2618. DOI: 10.1002/APP.1964.070080609.
  56. Slonimsky G.L., Reztsova E.V. On the mutual solubility of polymers. V. Mechano-chemical combination. Vysokomolekulyarnye soedineniya, 1959, vol. 1, no. 4, pp. 534–538.
  57. Novitskaya S.P., Nudelman Z.N., Dontsov A.A. Fluoroelastomers. Moscow: Chemistry, 1988, 240 p.
  58. Laptev A.B., Nikolayev E.V., Kolpachkov E.D. Thermodynamic characteristics of aging of polymeric composite materials under conditions of real exploitation. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 80–88. DOI: 10.18577/2071-9140-2018-0-3-80-88.
  59. Khorova E.A., Myshlyavtsev A.V., Strizhak E.A., Tretyakova N.A. Examination of hydrogenated butadiene-nitrile rubbers by methods of differential scanning calorimetry and dynamic mechanical analysis. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 11–16. DOI: 10.18577/2071-9140-2019-0-1-11-16.
  60. Kovrizhkina N.A., Kuznetsova V.A., Silaeva A.A., Marchenko S.A. Ways to improve the properties of paint coatings by adding different fillers (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 41–48. DOI: 10.18577/2071-9140-2019-0-4-41-48.
  61. Kuznetsova V.А. Influence of the elastomeric modifier on mechanical and viscoelastic properties of epoxy and rubber compositions for erosion resistant coatings. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 56–62. DOI: 10.18577/2071-9140-2020-0-2-56-62.