Antifriction materials based on polymer fibers

Kulagina G.S., Kan A.Ch., Zhelezina G.F., Levakova N.M.
Kulagina G.S., Kan A.Ch., Zhelezina G.F., Levakova N.M. Antifriction materials based on polymer fibers // Proceedings of VIAM. 2022. No. 11. DOI: 10.18577/2307-6046-2022-0-11-48-59. URL: https://www.viam-works.ru/en/journal/2022/11/5
Keywords
ant-friction organoplastic, antifriction fabric, self-lubricating material, polytetrafluoroethylene fiber, friction coefficient
Abstract

The paper considers self-lubricating antifriction materials reinforced with fabric based on organic fibers. Experimental fabrics of various composition and textile structure were designed and manufactured. Fabrics contain fibers of PTFE and other organic polymers. Samples of fabrics and antifriction organoplastics based on them have been studied, their physical-mechanical and tribological properties have been determined. It is shown that organoplastics based on experimental tissues can be considered as self-lubricating antifriction materials.

Reference list
  1. Modern engineering materials. Non-metallic materials: reference book. Ed. I.V. Gorynin, A.S. Oryshchenko. St. Petersburg: Professional, 2012, 916 p.
  2. Pogosyan A.K. Friction and wear of filled polymeric materials. Moscow: Nauka, 1977, 138 p.
  3. Myshkin N.K., Petrokovets M.I. Tribology. Principles and applications. Gomel: IMMS NASB, 2002, 310 p.
  4. Semenov A.P., Savinsky Yu.E. Metallic fluoroplastic bearings. Moscow: Mashinostroenie, 1967, 354 p.
  5. Mashkov Yu.K., Ovchar Z.N., Baibaratskaya M.Yu., Mamaev O.A. Polymer composite materials in tribotechnics. Moscow: Nedra-Businesscenter, 2004, 262 p.
  6. Voronkov B.D. Dry friction bearings. Leningrad: Mashinostroenie, 1979, 224 p.
  7. Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermo-plastic polymer composite materials based on polyether-etherketones of various manufacturers. Trudy VIAM, 2022, no. 1 (107), paper no. 04. Available at: http://www.viam-works.ru (accessed: September 01, 2022). DOI: 10.18577/2713-0193-2022-0-1-41-50.
  8. Mikhailin Yu.A. Heat-resistant polymers and polymeric materials. St. Petersburg: Professiya, 2012, 624 p.
  9. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  10. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://journal.viam.ru (accessed: September 05, 2022). DOI: 10.18577/2713-0193-2021-0-1-22-23.
  11. Craig W.D., Remorenko R.P. Initial wear of PTFE lined bearings. Lubrication Engineering, 1966, vol. 22, no. 5, pp. 181–186.
  12. Anti-friction fabric: pat. 590383 USSR, no. 2319403/28-12; filed 15.12.75; publ. 30.01.78.
  13. Kuzharov A.S., Ryadchenko V.G., Grechko V.O. Study of tribotechnical properties of various textile structures based on fibrous polytetrafluoroethylene. Trenie i iznos, 1986, vol. 7, no. 5, pp. 945–950.
  14. Kuzharov A.S., Ryadchenko V.G. Composite antifriction coatings based on polytetrafluoroethylene fibers. Wearlessness: Interuniver. collection of scientific papers. Rostov-on-Don: RISHM, 1992, is. 2, pp. 140–147.
  15. Ampep X-l an improved bearing material. Industrial lubrication and Tribology, 1975, vol. 97, no. 2, pp. 54–56.
  16. Antifriction organoplastic prepreg and product made from it: pat. 2404202 Rus. Federation, no. 2009111566/05; filed 31.03.09; publ. 20.11.10.
  17. Kablov E.N. Materials for aerospace engineering. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
  18. Kablov E.N. Materials and chemical technologies for aviation equipment. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, pp. 520–530.
  19. Kablov E.N. Aerospace materials science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
  20. Solomentseva A.V., Fadeeva V.M., Zhelezina G.F. Antifriction organoplastics for heavy loaded sliding friction units of aircraft structures. Aviacionnye materialy i tehnologii, 2016, no. 2, pp. 30–34. DOI: 10.18577/2071-9140-2016-0-2-30-34.
  21. Kan A.Ch., Kulagina G.S., Ayupov T.R., Zhelezina G.F. The influence of environmental factors on the characteristics of antifriction organoplasty Orgalon AF-1M. Trudy VIAM, 2018, no. 3 (109), paper no. 09. Available at: http://www.viam-works.ru (accessed: October 06, 2022). DOI: 10.18577/2307-6046-2022-0-3-91-101.
  22. Kulagina G.S., Zhelezina G.F., Levakova N.M. Antifriction organoplastics for high-loaded friction knots. Trudy VIAM, 2019, no. 2 (74), paper no. 09. Available at: http://www.viam-works.ru (accessed: September 05, 2022). DOI: 10.18577/2307-6046-2019-0-2-89-96.
  23. Gulyaev A.I., Medvedev P.N., Sbitneva S.V., Petrov A.A. Experimental research of «fiber–matrix» adhesion strength in carbon fiber epoxy/polysulphone composite. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 80–86. DOI: 10.18577/2071-9140-2019-0-4-80-86.